Secondary hardening in Co-Ni-Cr super-alloy investigated by Mechanical Spectroscopy

被引:4
作者
Cosimati, Raffaele [1 ]
Mari, Daniele [1 ]
机构
[1] Ecole Polytech Fed Lausanne, Inst Condensed Matter Phys, Stn 3, CH-1015 Lausanne, Switzerland
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2016年 / 662卷
关键词
Metals and alloys; Precipitation; Age hardening; Thermoelectric power; Internal friction; THERMOELECTRIC-POWER; INTERNAL-FRICTION; HEAT-TREATMENT; MP35N ALLOY; MP159; ALLOY; RECRYSTALLIZATION; PRECIPITATION; DEFORMATION; TRANSFORMATION; WORK;
D O I
10.1016/j.msea.2016.03.091
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The effects of thermal treatments on a Co-Ni-Cr super-alloy in the temperature range from 250 degrees C to 900 degrees C, resulting in secondary hardening, have been studied by Mechanical Spectroscopy. The simultaneous evolution of the internal friction spectra and of the dynamic modulus suggests that precipitates are involved in complex mechanisms, which control the dislocation mobility increasing the strength of the material. Precipitation induces pinning of dislocations and depinning is induced by a threshold stress. Such a precipitation process occurs in the temperature range from 400 degrees C to 600 degrees C and it is confirmed by reversible changes on thermoelectric power (TEP) due to the depletion of alloying elements from solid solution and by hardness measurements showing a hardness increase at the same annealing temperature as the maximum in TEP curve. The amplitude-dependent internal friction spectra as well as the interaction between dislocations and precipitates are interpreted by proposing a phenomenological model based on the Granato-Lucke theory. (C) 2016 Elsevier B.V. All rights reserved.
引用
收藏
页码:426 / 431
页数:6
相关论文
共 35 条
  • [1] The secondary hardening phenomenon in strain-hardened MP35N alloy
    Asgari, S
    El-Danaf, E
    Shaji, E
    Kalidindi, SR
    Doherty, RD
    [J]. ACTA MATERIALIA, 1998, 46 (16) : 5795 - 5806
  • [2] Strain hardening regimes and microstructural evolution during large strain compression of low stacking fault energy fcc alloys that form deformation twins
    Asgari, S
    ElDanaf, E
    Kalidindi, SR
    Doherty, RD
    [J]. METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1997, 28 (09): : 1781 - 1795
  • [3] Batist R.D, 1972, Internal friction of structural defects in crystalline solids
  • [4] EFFECTS OF PRECIPITATION ON THE THERMOELECTRIC-POWER OF IRON CARBON ALLOYS
    BENKIRAT, D
    MERLE, P
    BORRELLY, R
    [J]. ACTA METALLURGICA, 1988, 36 (03): : 613 - 620
  • [5] Blanter MS, 2007, SPRINGER SER MATER S, V90, pVII, DOI 10.1007/978-3-540-68758-0
  • [6] Davis J.R., 2000, ASM SPECIALTY HANDBO
  • [7] Feltham P., 1971, J PHYS C SOLID STATE, V32, P187
  • [8] Graham A., 1969, T ASM, V62, P930
  • [9] WORK STRENGTHENING BY A DEFORMATION-INDUCED PHASE TRANSFORMATION IN MP-ALLOYS
    GRAHAM, AH
    YOUNGBLO.JL
    [J]. METALLURGICAL TRANSACTIONS, 1970, 1 (02): : 423 - &
  • [10] Granato A., 1956, DISLOCATIONS MECHANI, P425