Mixed silicon-graphite composites as anode material for lithium ion batteries influence of preparation conditions on the properties of the material

被引:183
作者
Dimov, N [1 ]
Kugino, S [1 ]
Yoshio, A [1 ]
机构
[1] Saga Univ, Dept Appl Chem, Saga 8408502, Japan
关键词
silicon; lithium-ion; batteries; anode; composite;
D O I
10.1016/j.jpowsour.2004.05.012
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Mixed silicon-graphite composites were studied as an anode material for LIB. Estimation of the capacity of the composite as a function of silicon mass fraction as well as the lithium mole fraction in the final Li-Si alloy was performed. Based on this estimation, appropriate cycling test was introduced. Possible cycling stability region in terms of Si mass fraction, mole fraction of Li in the Li-Si alloy and average particle size was evaluated. (C) 2004 Published by Elsevier B.V.
引用
收藏
页码:108 / 114
页数:7
相关论文
共 12 条
[1]   Key factors controlling the reversibility of the reaction of lithium with SnO2 and Sn2BPO6 glass [J].
Courtney, IA ;
Dahn, JR .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1997, 144 (09) :2943-2948
[2]   Carbon-coated silicon as anode material for lithium ion batteries: advantages and limitations [J].
Dimov, N ;
Kugino, S ;
Yoshio, M .
ELECTROCHIMICA ACTA, 2003, 48 (11) :1579-1587
[3]   Characterization of carbon-coated silicon - Structural evolution and possible limitations [J].
Dimov, N ;
Fukuda, K ;
Umeno, T ;
Kugino, S ;
Yoshio, M .
JOURNAL OF POWER SOURCES, 2003, 114 (01) :88-95
[4]   Decrepitation Model For Capacity Loss During Cycling of Alloys in Rechargeable Electrochemical Systems [J].
Huggins, R. A. ;
Nix, W. D. .
IONICS, 2000, 6 (1-2) :57-63
[5]   Tin-based amorphous oxide: A high-capacity lithium-ion-storage material [J].
Idota, Y ;
Kubota, T ;
Matsufuji, A ;
Maekawa, Y ;
Miyasaka, T .
SCIENCE, 1997, 276 (5317) :1395-1397
[6]   Amorphous silicon thin-film negative electrode prepared by low pressure chemical vapor deposition for lithium-ion batteries [J].
Jung, HJ ;
Park, M ;
Han, SH ;
Lim, H ;
Joo, SK .
SOLID STATE COMMUNICATIONS, 2003, 125 (7-8) :387-390
[7]  
Kim I, 2000, ELECTROCHEM SOLID ST, V3, P493
[8]   The crystal structural evolution of nano-Si anode caused by lithium insertion and extraction at room temperature [J].
Li, H ;
Huang, XJ ;
Chen, LQ ;
Zhou, GW ;
Zhang, Z ;
Yu, DP ;
Mo, YJ ;
Pei, N .
SOLID STATE IONICS, 2000, 135 (1-4) :181-191
[9]  
Umeno T, 2001, CHEM LETT, P1186
[10]   Sub-microcrystalline Sn and Sn-SnSb powders as lithium storage materials for lithium-ion batteries [J].
Yang, J ;
Wachtler, M ;
Winter, M ;
Besenhard, JO .
ELECTROCHEMICAL AND SOLID STATE LETTERS, 1999, 2 (04) :161-163