Hot Corrosion Behavior of Monel 400 and AISI 304 Dissimilar Weldments Exposed in the Molten Salt Environment Containing Na2SO4+60% V2O5 at 600 °C

被引:10
作者
Ramkumar, K. Devendranath [1 ]
Arivazhagan, N. [1 ]
Narayanan, S. [1 ]
Mishra, Debidutta [1 ]
机构
[1] VIT Univ, Sch Mech & Bldg Sci, Vellore 632014, Tamil Nadu, India
来源
MATERIALS RESEARCH-IBERO-AMERICAN JOURNAL OF MATERIALS | 2014年 / 17卷 / 05期
关键词
Monel; 400; AISI 304 stainless steel; filler metals; mechanical properties; hot corrosion; MICROSTRUCTURE; OXIDATION; CHROMIUM; ALLOYS; NICKEL;
D O I
10.1590/1516-1439.274314
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
This research work investigates the use of pulsed current for joining two dissimilar metals Monel 400 and AISI 304 using Pulsed Current Gas Tungsten Arc welding using three different filler metals such as ER309L, ERNiCu-7 and ERNiCrFe-3. Microstructure observations showed the presence of Partially Melted Zone (PMZ) at the heat affected zone (HAZ) of all the weldments. The formation of secondary phases was witnessed at the HAZ of Monel 400 on using ERNiCu-7 filler. Tensile studies corroborated that the bimetallic combinations employing ERNiCu-7 offer better tensile properties as compared to ER309L and ERNiCrFe-3 weldments. Parent metal Monel 400 exhibited better corrosion resistance as compared to other zones of the weldments when exposed in the synthetic molten salt environment containing Na-2 SO4 - 60% V2O5 environment at 600 degrees C. A detailed structure -property relationship was made using the combined techniques of optical microscopy and SEM. Also the hot corrosion products were revealed using the thermogravimetric plots, XRD and SEM/EDAX analysis.
引用
收藏
页码:1273 / 1284
页数:12
相关论文
共 21 条
  • [1] El Din AMS, 2000, DESALINATION, V130, P89
  • [2] Gitanjaly, 2003, THESIS
  • [3] EFFECT OF ARC OSCILLATIONS ON THE TEMPERATURE DISTRIBUTION AND MICROSTRUCTURE IN GTA TANTALUM WELDS
    GRILL, A
    [J]. METALLURGICAL TRANSACTIONS B-PROCESS METALLURGY, 1981, 12 (04): : 667 - 674
  • [4] Development of a chromium-free consumable for austenitic stainless steels - Part 1: Monel (alloy 400) filler metal
    Kim, YH
    Frankel, GS
    Lippold, JC
    Guaytima, G
    [J]. CORROSION, 2006, 62 (01) : 44 - 53
  • [5] OXIDATION AND HOT CORROSION IN NA2SO4-10-PERCENT-V2O5 OF NI-17CR-6AL-0.5Y AND NI-16CR-5.7AL-0.47Y-5SI MCRALY ALLOYS AT 700-DEGREES-C
    LAMBERT, P
    CHAMPAGNE, B
    ARSENEAULT, B
    [J]. CANADIAN METALLURGICAL QUARTERLY, 1991, 30 (02) : 125 - 130
  • [6] A corrosion study of nickel-copper and nickel-copper-palladium welding filler metals
    Liang, D.
    Sowards, J. W.
    Frankel, G. S.
    Alexandrov, B. T.
    Lippold, J. C.
    [J]. MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 2010, 61 (11): : 909 - 919
  • [7] A study on hot corrosion behaviour of Ni-5Al coatings on Ni- and Fe-based superalloys in an aggressive environment at 900 °C
    Mahesh, R. A.
    Jayaganthan, R.
    Prakash, S.
    [J]. JOURNAL OF ALLOYS AND COMPOUNDS, 2008, 460 (1-2) : 220 - 231
  • [8] OATES WR, 1998, WELDING HDB MAT APPL, P59
  • [9] THE HOT CORROSION OF IN-657 SUPERALLOY IN NA2SO4-V2O5 MELT EUTECTIC
    OTERO, E
    PARDO, A
    HERNAEZ, J
    PEREZ, FJ
    [J]. CORROSION SCIENCE, 1991, 32 (07) : 677 - 683
  • [10] MASS-TRANSPORT OF CHROMIUM AND NICKEL IN MONEL-400
    PAUL, AR
    NAIK, MC
    KAIMAL, KNG
    [J]. JOURNAL OF NUCLEAR MATERIALS, 1975, 58 (02) : 205 - 210