Superplastic behavior and cavitation in high-strain-rate superplastic Si3N4p/Al-Mg-Si composites

被引:15
|
作者
Iwasaki, H [1 ]
Mori, T
Mabuchi, M
Higashi, K
机构
[1] Himeji Inst Technol, Coll Engn, Dept Mat Sci & Engn, Hyogo 6712201, Japan
[2] Natl Ind Res Inst Nagoya, Nagoya, Aichi 4620057, Japan
[3] Univ Osaka Prefecture, Coll Engn, Dept Met & Mat Sci, Osaka 5998531, Japan
来源
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE | 1998年 / 29卷 / 02期
关键词
D O I
10.1007/s11661-998-0148-4
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
High-strain-rate superplastic behavior has been investigated for Si3N4p/Al-Mg-Si (6061) composites with a V-f = 20 and 30 pct, respectively, where V-f is the volume fraction of reinforcements. A maximum elongation was attained at a temperature close to the onset temperature for melting for both composites, The maximum elongation for the 30 vol pct composite was larger than that for the 20 vol pct composite. Development of cavities transverse to the tensile direction is responsible for the lower maximum elongation of the 20 vol pct composite. However, development of the transverse cavities was limited to the optimum superplastic temperature for the 30 vol pct composite. The differential scanning calorimetry (DSC) investigation showed that a sharp endothermic peak appeared for the 30 vol pct composite, indicating that sufficient partial melting occurs. It is, therefore, likely that the stress concentrations are sufficiently relaxed by a liquid phase and that the development of transverse cavities is limited for the 30 vol pct composite.
引用
收藏
页码:677 / 683
页数:7
相关论文
共 50 条
  • [1] Superplastic behavior and cavitation in high-strain-rate superplastic Si3N4p/Al-Mg-Si composites
    Hajime Iwasaki
    Takasuke Mori
    Mamoru Mabuchi
    Kenji Higashi
    Metallurgical and Materials Transactions A, 1998, 29 : 677 - 683
  • [2] Superplastic behavior and cavitation in high-strain-rate superplastic Si3N4p/Al-Mg-Si composites
    Iwasaki, H.
    Mori, T.
    Mabuchi, M.
    Higashi, K.
    Metallurgical and Materials Transactions A: Physical Metallurgy and Materials Science, 1998, 29 A (02): : 677 - 683
  • [3] Evaluation of cavity growth in a high-strain-rate superplastic Si3N4p/Al-Mg-Si composite
    Iwasaki, H
    Mori, T
    Mabuchi, M
    Higashi, K
    THERMEC '97 - INTERNATIONAL CONFERENCE ON THERMOMECHANICAL PROCESSING OF STEELS AND OTHER MATERIALS, VOLS I-II, 1997, : 1991 - 1997
  • [4] Observation of cavitation formation in a superplastic Si3N4p/Al-Mg-Si composite at high strain rates
    Iwasaki, H
    Ohtani, T
    Mori, T
    Mabuchi, M
    Higashi, K
    Tanimura, S
    MATERIALS SCIENCE RESEARCH INTERNATIONAL, 1995, 1 (01): : 31 - 36
  • [5] PROCESSING OF HIGH-STRAIN-RATE SUPERPLASTIC SI3N4W/AL-MG-SI
    MABUCHI, M
    HIGASHI, K
    JOURNAL OF MATERIALS RESEARCH, 1995, 10 (10) : 2494 - 2502
  • [6] The role of liquid phase in cavitation and fracture in high-strain-rate superplastic Si3N4p/Al alloy composite
    Iwasaki, H
    Mabuchi, M
    Higashi, K
    TOWARDS INNOVATION IN SUPERPLASTICITY II, 1999, 304-3 : 645 - 650
  • [7] Mechanisms of cavity shrinkage by static annealing in a high strain rate superplastic Si3N4p/Al-Mg-Si composite
    Iwasaki, H
    Mori, T
    Mabuchi, M
    Higashi, K
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1998, 242 (1-2): : 32 - 38
  • [8] The role of liquid phase in cavitation in a Si3N4p/Al-Mg-Si composite exhibiting high-strain-rate superplasticity
    Iwasaki, H
    Mabuchi, M
    Higashi, K
    ACTA MATERIALIA, 1997, 45 (07) : 2759 - 2764
  • [9] An investigation of shear deformation in a semi-solid state of a high strain rate superplastic Si3N4p/Al-Mg-Si composite
    Mabuchi, M
    Iwasaki, H
    Higashi, K
    ACTA MATERIALIA, 1998, 46 (15) : 5335 - 5343
  • [10] Cavitation and fracture in high strain rate superplastic Al alloy/Si3N4(p) composites
    Iwasaki, H.
    Mabuchi, M.
    Higashi, K.
    Materials Science and Technology, 12 (06):