Effect of Cement Types and Superabsorbent Polymers on the Properties of Sustainable Ultra-High-Performance Paste

被引:13
|
作者
Xuan, Mei-Yu [1 ]
Wang, Yi-Sheng [2 ]
Wang, Xiao-Yong [1 ,2 ]
Lee, Han-Seung [3 ]
Kwon, Seung-Jun [4 ]
机构
[1] Kangwon Natl Univ, Dept Architectural Engn, Chuncheon Si 24341, South Korea
[2] Kangwon Natl Univ, Dept Integrated Energy & Infra Syst, Chuncheon Si 24341, South Korea
[3] Hanyang Univ, Dept Architectural Engn, Ansan 15588, South Korea
[4] Hannam Univ, Dept Civil & Environm Engn, Daejeon Si 34430, South Korea
基金
新加坡国家研究基金会;
关键词
superabsorbent polymer; belite-rich Portland cement; sustainable ultra-high-performance paste; internal curing; autogenous shrinkage; PORTLAND LHP CEMENT; AUTOGENOUS SHRINKAGE; FLY-ASH; HYDRATION HEAT; PORE STRUCTURE; LIMESTONE POWDER; PULSE VELOCITY; SILICA FUME; CONCRETE; STRENGTH;
D O I
10.3390/ma14061497
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
This study focuses on the effects of superabsorbent polymers (SAP) and belite-rich Portland cement (BPC) on the compressive strength, autogenous shrinkage (AS), and micro- and macroscopic performance of sustainable, ultra-high-performance paste (SUHPP). Several experimental studies were conducted, including compressive strength, AS, isothermal calorimetry, X-ray diffraction (XRD), thermogravimetric analysis (TGA), attenuated total reflectance (ATR)-Fourier-transform infrared spectroscopy (FTIR), ultra-sonic pulse velocity (UPV), and electrical resistivity. The following conclusions can be made based on the experimental results: (1) a small amount of SAP has a strength promotion effect during the first 3 days, while BPC can significantly improve the strength over the following 28 days. (2) SAP slows down the internal relative humidity reduction and effectively reduces the development of AS. BPC specimens show a lower AS than other specimens. The AS shows a linear relationship with the internal relative humidity. (3) Specimens with SAP possess higher cumulative hydration heat than control specimens. The slow hydration rate in the BPC effectively reduces the exothermic heat. (4) With the increase in SAP, the calcium hydroxide (CH) and combined water content increases, and SAP thus improves the effect on cement hydration. The contents of CH and combined water in BPC specimens are lower than those in the ordinary Portland cement (OPC) specimen. (5) All samples display rapid hydration of the cement in the first 3 days, with a high rate of UPV development. Strength is an exponential function of UPVs. (6) The electrical resistivity is reduced due to the increase in porosity caused by the release of water from SAP. From 3 to 28 days, BPC specimens show a greater increment in electrical resistivity than other specimens.
引用
收藏
页数:20
相关论文
共 50 条
  • [1] Effect of superabsorbent polymers on the properties of cement paste particle under different relative humidities
    Lyu, Jingjing
    Zhang, Jianjian
    Guan, Xinchun
    JOURNAL OF BUILDING ENGINEERING, 2024, 91
  • [2] Influence of superabsorbent polymers on the surrounding cement paste
    Wang, Fazhou
    Yang, Jin
    Hu, Shuguang
    Li, Xinping
    Cheng, Hua
    CEMENT AND CONCRETE RESEARCH, 2016, 81 : 112 - 121
  • [3] Mechanical properties of affordable and sustainable ultra-high-performance concrete
    Tahwia, Ahmed M.
    Elgendy, Gamal M.
    Amin, Mohamed
    CASE STUDIES IN CONSTRUCTION MATERIALS, 2022, 16
  • [4] Developing Sustainable Ultra-High-Performance Concrete
    Kareem, Rahman
    Alsalman, Ali
    Dang, Canh N.
    Marti-Vargas, Jose R.
    Hale, W. Micah
    ACI MATERIALS JOURNAL, 2022, 119 (03) : 127 - 136
  • [5] Effect of industrial wastes on the properties of sustainable ultra-high-performance concrete: Ganite, ceramic, and glass
    Amin, Mohamed
    Zeyad, Abdullah M.
    Agwa, Ibrahim Saad
    Rizk, Mostafa S.
    CONSTRUCTION AND BUILDING MATERIALS, 2024, 428
  • [6] IMPACT PERFORMANCE OF LOW CEMENT ULTRA-HIGH-PERFORMANCE CONCRETE
    Azmee, Norzaireen Mohd
    Nuruddin, Muhd Fadhil
    SUSTAINABLE CITY XII, 2017, 223 : 481 - 488
  • [7] Shrinkage of ultra-high performance concrete with superabsorbent polymers
    Lesovik, V. S.
    Popov, D. Y.
    Fediuk, R. S.
    Sabri, M. M.
    Vavrenyuk, S. V.
    Liseitsev, Yu. L.
    MAGAZINE OF CIVIL ENGINEERING, 2023, 121 (05):
  • [8] Strength and hydration of metakaolin-containing ultra-high-performance paste
    Mo, Zongyun
    Bai, Ligai
    Fu, Xu
    PROCEEDINGS OF THE INSTITUTION OF CIVIL ENGINEERS-CONSTRUCTION MATERIALS, 2020, 176 (03) : 106 - 116
  • [9] Strength and hydration of metakaolin-containing ultra-high-performance paste
    Mo, Zongyun
    Bai, Ligai
    Fu, Xu
    PROCEEDINGS OF THE INSTITUTION OF CIVIL ENGINEERS-CONSTRUCTION MATERIALS, 2023, 176 (03) : 106 - 116
  • [10] Effect of aggregate and fibre types on ultra-high-performance concrete designed for radiation shielding
    Zeyad, Abdullah M.
    Hakeem, Ibrahim Y.
    Amin, Mohamed
    Tayeh, Bassam A.
    Agwa, Ibrahim Saad
    JOURNAL OF BUILDING ENGINEERING, 2022, 58