Electrophoretic deposition (EPD) was used to form ZnO deposits. ZnO with an average particle size of 40 nm was dispersed in water with the, addition of an appropriate amount of anionic polyelectrolyte. Uniform and bubble-free ZnO deposits have been obtained via EPD on a zinc anode in an aqueous suspension. The obtained deposits showed good sinterability. (C) 2002 Elsevier Science Ltd. All rights reserved.