Characteristics of degraded cellulose obtained from steam-exploded wheat straw

被引:580
作者
Sun, XF
Xu, F
Sun, RC [1 ]
Fowler, P
Baird, MS
机构
[1] Univ Wales, BioComposites Ctr, Bangor LL57 2UW, Gwynedd, Wales
[2] Univ Wales, Dept Chem, Bangor LL57 2UW, Gwynedd, Wales
[3] NW Univ Agr & Forest Sci & Technol, Coll Forestry, Yangling 712100, Peoples R China
[4] S China Univ Technol, State Key Lab Pulp & Paper Engn, Guangzhou 510641, Peoples R China
基金
中国国家自然科学基金;
关键词
wheat straw; steam explosion; cellulose; peroxide;
D O I
10.1016/j.carres.2004.10.022
中图分类号
Q5 [生物化学]; Q7 [分子生物学];
学科分类号
071010 ; 081704 ;
摘要
The isolation of cellulose from wheat straw was studied using a two-stage process based on steam explosion pre-treatment followed by alkaline peroxide post-treatment. Straw was steamed at 200degreesC, 15bar for 10 and 33 min, and 220degreesC, 22 bar for 3, 5 and 8 min with a solid to liquid ratio of 2:1 (w/w) and 220degreesC, 22 bar for 5 min with a solid to liquid ratio of 10:1, respectively. The steamed straw was washed with hot water to yield a solution rich in hemicelluloses-derived mono- and oligosaccharides and gave 61.3 %, 60.2 %, 66.2 %, 63.1 %, 60.3 % and 61.3 % of the straw residue, respectively. The washed fibre was delignified and bleached by 2 % H2O2, at 50degreesC for 5 h under pH 11.5, which yielded 34.9 %, 32.6 %, 40.0 %, 36.9 %, 30.9 % and 36.1% (% dry wheat straw) of the cellulose preparation, respectively. The optimum cellulose yield (40.0 %) was obtained when the steam explosion pre-treatment was performed at 220degreesC, 22 bar for 3 min with a solid to liquid ratio of 2:1, in which the cellulose fraction obtained had a viscosity average degree of polymerisation of 587 and contained 14.6 % hemicelluloses and 1.2 % klason lignin. The steam explosion pre-treatment led to a sianificant loss in hemicelluloses and alkaline peroxide post-treatment resulted in substantial dissolution of lignin and an increase in cellulose crystallinity. The six isolated cellulose samples were further characterised by FT-IR and C-13-CP/MAS NMR spectroscopy and thermal analysis. (C) 2004 Elsevier Ltd. All rights reserved.
引用
收藏
页码:97 / 106
页数:10
相关论文
共 28 条
[1]   Effect of chip size on steam explosion pretreatment of softwood [J].
Ballesteros, I ;
Oliva, JM ;
Navarro, AA ;
González, A ;
Carrasco, J ;
Ballesteros, M .
APPLIED BIOCHEMISTRY AND BIOTECHNOLOGY, 2000, 84-6 (1-9) :97-110
[2]   FRACTIONATION AND BIOCONVERSION OF STEAM-EXPLODED WHEAT STRAW [J].
BELTRAME, PL ;
CARNITI, P ;
VISCIGLIO, A ;
FOCHER, B ;
MARZETTI, A .
BIORESOURCE TECHNOLOGY, 1992, 39 (02) :165-171
[3]   A SIMPLE AND RAPID PREPARATION OF ALDITOL ACETATES FOR MONOSACCHARIDE ANALYSIS [J].
BLAKENEY, AB ;
HARRIS, PJ ;
HENRY, RJ ;
STONE, BA .
CARBOHYDRATE RESEARCH, 1983, 113 (02) :291-299
[4]   AQUEOUS THERMOMECHANICAL PRETREATMENT OF ASPEN IN A BATCH REACTOR SYSTEM [J].
CARRASCO, F .
JOURNAL OF WOOD CHEMISTRY AND TECHNOLOGY, 1992, 12 (02) :213-230
[5]   The organosolv fractionation of cork components [J].
Cordeiro, N ;
Neto, CP ;
Rocha, J ;
Belgacem, MN ;
Gandini, A .
HOLZFORSCHUNG, 2002, 56 (02) :135-142
[6]  
Delong E.A., 1981, Canadian Patent, Patent No. [CA1096374, 1096374]
[7]   OBSERVATIONS BY HIGH-RESOLUTION C-13 NUCLEAR MAGNETIC-RESONANCE OF CELLULOSE-I RELATED TO MORPHOLOGY AND CRYSTAL-STRUCTURE [J].
EARL, WL ;
VANDERHART, DL .
MACROMOLECULES, 1981, 14 (03) :570-574
[8]   CELLULOSE MOLECULAR-WEIGHTS DETERMINED BY VISCOMETRY [J].
EVANS, R ;
WALLIS, AFA .
JOURNAL OF APPLIED POLYMER SCIENCE, 1989, 37 (08) :2331-2340
[9]   Characterization of the lignin obtained by alkaline delignification and of the cellulose residue from steam-exploded olive stones [J].
Fernández-Bolaños, J ;
Felizón, B ;
Heredia, A ;
Guillén, R ;
Jiménez, A .
BIORESOURCE TECHNOLOGY, 1999, 68 (02) :121-132
[10]   Comparative study of hemicelluloses released during two-stage treatments with acidic organosolv and alkaline peroxide from Caligonum monogoliacum and Tamarix spp [J].
Geng, ZC ;
Sun, RC ;
Sun, XF ;
Lu, Q .
POLYMER DEGRADATION AND STABILITY, 2003, 80 (02) :315-325