Optimum design of alkali activated slag concretes for the low oxygen/chloride ion permeability and thermal conductivity

被引:57
作者
Balcikanli, Mtizeyyen [1 ]
Ozbay, Erdogan [1 ]
机构
[1] Iskenderun Tech Univ, Dept Civil Engn, Iskenderun, Turkey
关键词
Mechanical properties; Thermal properties; Statistical properties; Geopolymer; ASH-BASED GEOPOLYMER; FLY-ASH; MECHANICAL-PROPERTIES; CEMENT GROUTS; STRENGTH; PARAMETERS; OPTIMIZATION; WORKABILITY; TECHNOLOGY; DURABILITY;
D O I
10.1016/j.compositesb.2016.01.047
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In this research, individual and interactional effect of curing temperature (CT), curing time (Crime), sodium concentration (SC) and silicate modulus (SM) on the compressive strength, chloride ion permeability, oxygen permeability and thermal conductivity of alkali activated slag (AAS) concretes were investigated and the best possible combination of CT, Crime, SC and SM for the maximization of compressive strength while for the minimization of chloride ion permeability, oxygen permeability and thermal conductivity of AAS concretes were determined. An experimental program that contains 21 different combinations of independent parameters (CT, Crime, SC and SM) was conducted by using the central composite design method. Alkali solution-slag ratio was kept constant at 0.53 in all production. The effects of the independent parameters were characterized and analyzed by using statistically significant quadratic regression models on the measured properties (dependent parameters). Optimum values of the independent parameters were determined by solving a multi-objective optimization problem obtained by using the proposed regression models for dependent parameters. The results of test and the analysis indicate that the independent parameters affect the dependent parameters considerably; however, the most effective parameter for the compressive strength, chloride ion permeability, oxygen permeability and thermal conductivity is the sodium concentration. The optimum combination of CT, Crime, SC and SM is 46.8 degrees C, 83 h, 5.5% and 2.0, respectively, for the minimization of chloride ion permeability, oxygen permeability and thermal conductivity and the maximization of compressive strength of AAS concretes. (C) 2016 Elsevier Ltd. All rights reserved.
引用
收藏
页码:243 / 256
页数:14
相关论文
共 54 条
  • [1] Durability of concrete incorporating GGBS activated by water-glass
    Al-Otaibi, Saud
    [J]. CONSTRUCTION AND BUILDING MATERIALS, 2008, 22 (10) : 2059 - 2067
  • [2] Permeability of cracked concrete
    Aldea, CM
    Shah, SP
    Karr, A
    [J]. MATERIALS AND STRUCTURES, 1999, 32 (219) : 370 - 376
  • [3] Alkali activation of a slag at ambient and elevated temperatures
    Altan, Ekin
    Erdogan, Sinan T.
    [J]. CEMENT & CONCRETE COMPOSITES, 2012, 34 (02) : 131 - 139
  • [4] [Anonymous], 1999, MATER STRUCT, V32, P176
  • [5] [Anonymous], 2004, C39 ASTM
  • [6] [Anonymous], 2004, C1202 ASTM
  • [7] [Anonymous], 1999, MATER STRUCT, V32, P174
  • [8] [Anonymous], 2007, DES EXP SOFTW DES EX
  • [9] Lightweight concretes of activated metakaolin-fly ash binders, with blast furnace slag aggregates
    Arellano Aguilar, R.
    Burciaga Diaz, O.
    Escalante Garcia, J. I.
    [J]. CONSTRUCTION AND BUILDING MATERIALS, 2010, 24 (07) : 1166 - 1175
  • [10] Influence of activator on the strength and drying shrinkage of alkali-activated slag mortar
    Atis, Cengiz Duran
    Bilim, Cahit
    Celik, Oezlem
    Karahan, Okan
    [J]. CONSTRUCTION AND BUILDING MATERIALS, 2009, 23 (01) : 548 - 555