Sub-zero treatments of AISI D2 steel: Part I. Microstructure and hardness

被引:186
作者
Das, Debdulal [2 ]
Dutta, Apurba Kishore [3 ]
Ray, Kalyan Kumar [1 ]
机构
[1] Indian Inst Technol, Dept Met & Mat Engn, Kharagpur 721302, W Bengal, India
[2] Bengal Engn & Sci Univ, Dept Met & Mat Engn, Sibpur 711103, Howrah, India
[3] Bengal Engn & Sci Univ, Dept Mech Engn, Sibpur 711103, Howrah, India
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2010年 / 527卷 / 09期
关键词
Sub-zero treatment; Retained austenite; Decomposition of martensite; Carbide precipitation; Hardness; Die steel; DEEP-CRYOGENIC TREATMENT; WEAR-RESISTANCE; CARBIDE PRECIPITATION; MECHANICAL-PROPERTIES; TOOL STEEL; HEAT-TREATMENT; BEHAVIOR; LIFE; TEMPERATURE; MORPHOLOGY;
D O I
10.1016/j.msea.2009.10.070
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Microstructure, hardness and wear behavior of AISI D2 steel subjected to varied sub-zero treatments have been examined with reference to conventional heat treatment. Part I of this work presents the variations of microstructure and hardness, whereas part 11 deals with the wear behavior. The sub-zero treatments studied are cold treatment, shallow cryogenic treatment and deep cryogenic treatment. The developed microstructures have been characterized by XRD, optical microscopy and SEM examinations coupled with EDX and image analyses. Macrohardness and microhardness of the specimens have been evaluated by Vickers indentation technique. The obtained results infer that (i) retained austenite content is reduced by cold treatment, but is almost completely eliminated by both shallow and deep cryogenic treatments, (ii) the sub-zero treatments modify the precipitation behavior of secondary carbides; lower the temperature of sub-zero treatment higher is the degree of modification, (iii) the deep cryogenic treatment refines the secondary carbides, increases their amount and population density, and leads to more uniform distribution, and (iv) bulk hardness increases marginally but apparent hardness of the matrix improves considerably by deep cryogenic treatment. (C) 2009 Elsevier B.V. All rights reserved.
引用
收藏
页码:2182 / 2193
页数:12
相关论文
共 79 条
  • [1] Effects of cryogenic treatment on wear behavior of D6 tool steel
    Akhbarizadeh, A.
    Shafyei, A.
    Golozar, M. A.
    [J]. MATERIALS & DESIGN, 2009, 30 (08) : 3259 - 3264
  • [2] ALEXANDRU I, 1990, MEM ETUD SCI REV MET, V87, P383
  • [3] [Anonymous], 2008, C62 ASTM
  • [4] BABU PS, 2005, IE I J MM, V86, P64
  • [5] Fatigue scatter reduction through deep cryogenic treatment on the 18NiCrMo5 carburized steel
    Baldissera, Paolo
    [J]. MATERIALS & DESIGN, 2009, 30 (09) : 3636 - 3642
  • [6] Effects of deep cryogenic treatment on static mechanical properties of 18NiCrMo5 carburized steel
    Baldissera, Paolo
    Delprete, Cristiana
    [J]. MATERIALS & DESIGN, 2009, 30 (05) : 1435 - 1440
  • [7] BARRON RF, 1982, CRYOGENICS, V22, P409, DOI 10.1016/0011-2275(82)90085-6
  • [8] BARRON RF, 1973, PROGR REFRIGERATION, V1, P529
  • [9] Effect of cryogenic treatment on distribution of residual stress in case carburized En 353 steel
    Bensely, A.
    Venkatesh, S.
    Lal, D. Mohan
    Nagarajan, G.
    Rajadurai, A.
    Junik, Krzysztof
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2008, 479 (1-2): : 229 - 235
  • [10] Effect of cryogenic treatment on tensile behavior of case carburized steel-815M17
    Bensely, A.
    Senthilkumar, D.
    Lal, D. Mohan
    Nagarajan, G.
    Rajadurai, A.
    [J]. MATERIALS CHARACTERIZATION, 2007, 58 (05) : 485 - 491