Study and methods of analysis of mechanically alloyed Cu-Mo powders

被引:44
|
作者
Aguilar, C.
Ordonez, S.
Marin, J.
Castro, F.
Martinez, V.
机构
[1] Univ Santiago Chile, USACH, Dept Ingn Met, Santiago 3363, Chile
[2] CCHEN, Comis Chilena Energia Nucl, Santiago, Chile
[3] CEIT, Ctr Estudios & Invest Tecn Guipuzcoa, San Sebastian 20018, Spain
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2007年 / 464卷 / 1-2期
关键词
mechanical alloying; nanohardness; Cu-Mo; DSC; TEM;
D O I
10.1016/j.msea.2007.02.017
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The microstructural evolution during mechanical alloying of Cu and Mo was studied. The aim of this work is to study the effect of the milling time on the formation of the solid solution of molybdenum in copper, employing variable amounts of Mo (I and 8 at.%). The milling was performed under an inert argon atmosphere in a SPEX 80001) mill. Milling times of 4, 8, 25, 50, 75 and 100 h were used keeping a constant ball to powder ratio of 10-1. The effects of milling parameters such as milling time and composition on the synthesis and structure of Cu-Mo powders were investigated using XRD, nanohardness, differential scanning calorimetry (DSC) and TEM. The results show that the grain size and particle size of powders decrease with increasing milling time. Grain size in samples with 8 at.% Mo approached a minimum value of 20 nm after 50 h, and in samples with 1 at.% Mo, 30 nm after 75 h of milling. Nanohardness shows a maximum about 4 GPa for the alloy with 8 at.% of Mo and 100 h of milling. The measured crystallite size by TEM is in good agreement with the value calculated by XRD. Thermal analyses (DSC) showed the temperature intervals where the dynamic recrystallization would take place. According to these results this phenomenon would happen near 350 degrees C. (c) 2007 Elsevier B.V. All rights reserved.
引用
收藏
页码:288 / 294
页数:7
相关论文
共 50 条
  • [41] RESEARCHES REGARDING THE PROPERTIES OF SINTERED ELECTRICAL CONTACTS OBTAINED FROM MECHANICALLY ALLOYED W-Cu POWDERS
    Predescu, Constantin
    Nicolicescu, Claudiu
    Gavrila, Mann
    ADVANCED MATERIALS AND STRUCTURES IV, 2012, 188 : 395 - +
  • [42] Consolidation of mechanically alloyed Mg49Y15Cu36 powders by vacuum hot pressing
    Lee, P. Y.
    Lo, C.
    Jang, J. S. C.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2007, 434 : 354 - 357
  • [43] The influence of the condensation rate on the structure of Cu-Mo pseudoalloys
    Riaboshtan, V.
    Zubkov, A.
    Zhadko, M.
    Zozulya, E.
    Zubarev, E.
    LOW TEMPERATURE PHYSICS, 2024, 50 (01) : 44 - 47
  • [44] Structural and magnetic relaxations of mechanically alloyed Fe-Mo
    Jiraskova, Y.
    Bursik, J.
    Turek, I.
    Cizek, J.
    Prochazka, I.
    JOURNAL OF PHYSICS D-APPLIED PHYSICS, 2014, 47 (43)
  • [45] Nanostructure, Composition, and Magnetic Behavior of Mechanically Alloyed Fe–Mo
    Y. Jirásková
    J. Buršík
    I. Turek
    Journal of Superconductivity and Novel Magnetism, 2013, 26 : 1717 - 1721
  • [46] Magnetic properties of mechanically alloyed Co-Cu
    Modder, IW
    Schoonderwaldt, E
    Zhou, GF
    Bakker, H
    PHYSICA B, 1998, 245 (04): : 363 - 375
  • [47] Mechanically induced crystalline-glassy phase transformations of mechanically alloyed Ta55Zr10Al10Ni10Cu15 multicomponent alloy powders
    El-Eskandarany, MS
    Zhang, W
    Inoue, A
    JOURNAL OF ALLOYS AND COMPOUNDS, 2003, 350 (1-2) : 222 - 231
  • [48] A review of soft magnetic properties of mechanically alloyed amorphous and nanocrystalline powders
    Yakin, Alican
    Simsek, Tuncay
    Avar, Baris
    Simsek, Telem
    Chattopadhyay, Arun K.
    EMERGENT MATERIALS, 2023, 6 (02) : 453 - 481
  • [49] Mechanically Alloyed Magnesium Based Nanostructured Alloy Powders for Biomedical Applications
    Morcos, P.
    ElKhodary, K. I.
    Salem, H. G.
    MAGNESIUM TECHNOLOGY 2017, 2017, : 35 - 41
  • [50] STRUCTURE AND MAGNETIC-PROPERTIES OF MECHANICALLY ALLOYED IRON NITRIDE POWDERS
    LEE, PY
    CHEN, TR
    CHIN, TS
    JOURNAL OF ALLOYS AND COMPOUNDS, 1995, 222 : 179 - 183