Fracture in ceramic-reinforced metal matrix composites based on high-speed steel

被引:38
|
作者
Bolton, JD [1 ]
Gant, AJ [1 ]
机构
[1] Univ Bradford, Dept Mech & Mfg Engn, Bradford BD7 1DP, W Yorkshire, England
关键词
D O I
10.1023/A:1004303609990
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
A series of metal matrix composites based upon M3/2 high-speed steel was produced by a powder metal sintering route. Hard ceramic titanium carbide or niobium carbide additions and a self-lubricant in the form of manganese sulfide, were added as a basis for achieving improved wear resistance and reduced friction. After sintering, the composites were given a full standard high-speed steel heat treatment and subjected to mechanical tests. All three particulate additions had a deleterious effect on three-point bend strength, particularly in the case of MnS addition, mainly due to the ease of initiating cracks at or near to the particulate additions. Bend strengths were further reduced by the simultaneous addition of both MnS and either TiC or NbC especially when a high volume fraction of approximately 25 vol % MnS was added. Single, low volume fraction (less than or equal to 8%) additions, of TiC, NbC, or MnS, had little effect on fracture toughness and K-IC values were comparable to those found in the baseline M3/2 steel. Slight improvements in fracture toughness shown to occur in the 7.74% NbC composites were attributed to energy dissipation caused by the effects of crack branching during crack propagation. Composites with the higher volume fraction additions of MnS and ceramic carbide gave poor fracture toughness by forming MnS/carbide clusters which provided an easy path for crack propagation. (C) 1998 Chapman & Hall.
引用
收藏
页码:939 / 953
页数:15
相关论文
共 50 条
  • [21] Bioactive ceramic-reinforced composites for bone augmentation
    Tanner, K. E.
    JOURNAL OF THE ROYAL SOCIETY INTERFACE, 2010, 7 : S541 - S557
  • [22] Ceramic Preforms with 2D Regular Channels for Fabrication of Metal/Ceramic-Reinforced Composites
    Ighodaro, Osayande L.
    Okoli, Okenwa I.
    Zhang, Mei
    Wang, Ben
    INTERNATIONAL JOURNAL OF APPLIED CERAMIC TECHNOLOGY, 2012, 9 (02) : 421 - 430
  • [23] Ceramic-reinforced HEA matrix composites exhibiting an excellent combination of mechanical properties
    Mehmood, M. Adil
    Shehzad, Khurram
    Mujahid, M.
    Bin Yaqub, Talha
    Godfrey, Andy
    Fernandes, Filipe
    Muhammad, F. Z.
    Yaqoob, Khurram
    SCIENTIFIC REPORTS, 2022, 12 (01):
  • [24] Fracture in Ceramic-Matrix Composites Reinforced with Strongly Bonded Metal Particles
    X. Kong
    Y. Qiao
    Mechanics of Composite Materials, 2005, 41 : 205 - 216
  • [25] Fracture in ceramic-matrix composites reinforced with strongly bonded metal particles
    Kong, X
    Qiao, Y
    MECHANICS OF COMPOSITE MATERIALS, 2005, 41 (03) : 205 - 216
  • [26] Machinability investigations on high-speed drilling of aluminum reinforced with silicon carbide metal matrix composites
    Ch Asad Abbas
    Chuanzhen Huang
    Jun Wang
    Zhen Wang
    Hanlian Liu
    Hongtao Zhu
    The International Journal of Advanced Manufacturing Technology, 2020, 108 : 1601 - 1611
  • [27] Machinability investigations on high-speed drilling of aluminum reinforced with silicon carbide metal matrix composites
    Abbas, Ch Asad
    Huang, Chuanzhen
    Wang, Jun
    Wang, Zhen
    Liu, Hanlian
    Zhu, Hongtao
    INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2020, 108 (5-6): : 1601 - 1611
  • [28] TEM study of the interface in ceramic-reinforced aluminum-based composites
    Kostka, A
    Lelatko, J
    Gigla, M
    Morawiec, H
    Janas, A
    MATERIALS CHEMISTRY AND PHYSICS, 2003, 81 (2-3) : 323 - 325
  • [29] Ceramic-Reinforced -TiAl-Based Composites: Synthesis, Structure, and Properties
    Lazurenko, Daria V.
    Stark, Andreas
    Esikov, Maksim A.
    Paul, Jonathan
    Bataev, Ivan A.
    Kashimbetova, Adelya A.
    Mali, Vyacheslav I.
    Lorenz, Uwe
    Pyczak, Florian
    MATERIALS, 2019, 12 (04)
  • [30] High-speed steels and high-speed-steel based composites
    Oliveira, MM
    INTERNATIONAL JOURNAL OF MATERIALS & PRODUCT TECHNOLOGY, 2000, 15 (3-5): : 231 - 251