Effect of chromium on erosion-corrosion properties of ZrO2-Al2O3 particles reinforced Fe-based composites in artificial seawater slurries

被引:16
作者
Li, Cong [1 ,2 ]
Goei, Ronn [2 ]
Li, Yefei [1 ]
Shi, Jing [3 ]
Liu, Fei [4 ]
Li, Bo [1 ]
Gao, Yimin [1 ]
Li, Yuehui [1 ]
Li, Shuzhou [2 ]
Tok, Alfred Iing Yook [2 ]
机构
[1] Xi An Jiao Tong Univ, Sch Mat Sci & Engn, State Key Lab Mech Behav Mat, Xian 710049, Peoples R China
[2] Nanyang Technol Univ, Sch Mat Sci & Engn, Singapore 639798, Singapore
[3] Xian Univ Technol, Sch Mat Sci & Engn, Xian 710048, Peoples R China
[4] Inner Mongolia Univ Technol, Coll Mat Sci & Engn, Hohhot, Peoples R China
基金
中国国家自然科学基金; 中国博士后科学基金;
关键词
ZTA(P)/Fe composites; Cr coating; Interfacial layer; Erosion-corrosion resistance; Artificial seawater; STAINLESS-STEEL; IN-SITU; WEAR-RESISTANCE; SLIDING-WEAR; CAST IRONS; BEHAVIOR; MICROSTRUCTURE; CACO3; PHOSPHORUS; STRENGTH;
D O I
10.1016/j.corsci.2022.110138
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The influence of Cr on the interfacial bonding and erosion-corrosion resistance of ZrO2-Al2O3 particles reinforced high chromium white cast irons based (ZTA(P)/Fe) composites were systematically investigated. The Cr coatings on the surface of ZTA particle (ZTA(P)) ceramics were fabricated by multi-arc ion plating. The results indicated that a uniform and continuous Cr coating was tightly adhered with ZTA ceramic substrate. The thickness and grain size of the Cr coating could be effectively controlled by regulating the deposition parameters. The grain size of Cr coating increased with deposition time. The ZTA(P)/Fe composites assisted without (N1) and with (N2) Cr coating were prepared via infiltration casting. The addition of Cr coating obtained a smooth and tight interface, attributed to the improvement of the wettability between ZTA ceramic and high chromium white cast irons matrix (Cr15). Moreover, the erosion-corrosion resistance property of the Cr coated ZTA(P)/Fe composites (N2) improved up to 44% compared with bare-ZTA(P)/Fe composites (N1) due to their interfacial enhancement action. Meanwhile, the interfacial layer of the N2 composites had a low roughness after erosion-corrosion.
引用
收藏
页数:10
相关论文
共 56 条
[1]   Structural evolution and high-temperature tribological properties of AlCrON coatings deposited by multi-arc ion plating [J].
Ahmad, Farooq ;
Zhang, Lin ;
Zheng, Jun ;
Sidra, Iram ;
Cai, Fei ;
Zhang, Shihong .
CERAMICS INTERNATIONAL, 2020, 46 (15) :24281-24289
[2]   Comparative study of the structure and corrosion behavior of Zr-20%Cr and Zr-20%Ti alloy films deposited by multi-arc ion plating technique [J].
Ali, Farhat ;
Mehmood, Mazhar ;
Qasim, Abdul Mateen ;
Ahmad, Jamil ;
Naeem-ur-Rehman ;
Iqbal, Muhammad ;
Qureshi, Ammad H. .
THIN SOLID FILMS, 2014, 564 :277-283
[3]   Effects of tungsten on erosion-corrosion behavior of high chromium white cast iron [J].
Anijdan, S. H. Mousavi ;
Bahrami, A. ;
Varahram, N. ;
Davami, P. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2007, 454 (623-628) :623-628
[4]   Effect of Cu content on microstructure, mechanical and anti-fouling properties of TiSiN-Cu coating deposited by multi-arc ion plating [J].
Bai, Xuebing ;
Li, Jinlong ;
Zhu, Lihui ;
Wang, Liping .
APPLIED SURFACE SCIENCE, 2018, 427 :444-451
[5]   Characterization of calcareous deposits in artificial seawater by impedance techniques 3 -: Deposit of CaCO3 in the presence of Mg(II) [J].
Barchiche, C ;
Deslouis, C ;
Festy, D ;
Gil, O ;
Refait, P ;
Touzain, S ;
Tribollet, B .
ELECTROCHIMICA ACTA, 2003, 48 (12) :1645-1654
[6]   Effect of annealing temperature on slurry erosion resistance of ferritic X10CrAlSi18 steel [J].
Buszko, M. H. ;
Krella, A. K. ;
Marchewicz, A. ;
Gajowiec, G. .
TRIBOLOGY INTERNATIONAL, 2021, 153
[7]   Processing, microstructure and mechanical properties of Al2O3-Cr nanocomposites [J].
Chmielewski, Marcin ;
Pietrzak, Katarzyna .
JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2007, 27 (2-3) :1273-1279
[8]   The synergistic effects of ocean acidification and organic metabolism on calcium carbonate (CaCO3) dissolution in coral reef sediments [J].
Cyronak, Tyler ;
Eyre, Bradley D. .
MARINE CHEMISTRY, 2016, 183 :1-12
[9]   A superior strength and sliding-wear resistance combination of ductile iron with nanobainitic matrix [J].
Du, Yuzhou ;
Wang, Xiaolong ;
Zhang, Dongya ;
Wang, Xin ;
Ju, Chunpeng ;
Jiang, Bailing .
JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2021, 11 :1175-1183
[10]   Kinetics of phase separation, border of miscibility gap in Fe-Cr and limit of Cr solubility in iron at 832 K [J].
Dubiel, S. M. ;
Zukrowski, J. .
MATERIALS CHARACTERIZATION, 2019, 158