Impact of defect migration on electrical and dielectric properties in molten salt synthesized CaCu3Ti4O12 and customizing the properties by compositional engineering with Mg doping

被引:21
|
作者
Yadav, Bhoomika [1 ,2 ]
Kar, Kamal K. [1 ,3 ]
Ghorai, Manas K. [4 ]
Kumar, Devendra [5 ]
Yadav, Dharmendra [6 ]
机构
[1] Indian Inst Technol Kanpur, Mat Sci Programme, Adv Nanoengn Mat Lab, Kanpur 208016, India
[2] Chhatrapati Shahu Ji Maharaj Univ, Kanpur 208026, India
[3] Indian Inst Technol Kanpur, Dept Mech Engn, Adv Nanoengn Mat Lab, Kanpur 208016, India
[4] Indian Inst Technol Kanpur, Dept Chem, Kanpur 208016, India
[5] Banaras Hindu Univ, Indian Inst Technol, Dept Ceram Engn, Varanasi 221005, India
[6] Banaras Hindu Univ, Indian Inst Technol, Dept Phys, Varanasi 221005, India
关键词
Dielectric properties; Defect chemistry; Impedance spectroscopy; Compositional engineering; Rietveld refinement; MAGNETIC-PROPERTIES; CRYSTAL-STRUCTURE; AC-CONDUCTION; IMPEDANCE; RESISTIVITY; RELAXATION; CHEMISTRY; CONSTANT; CERAMICS; BEHAVIOR;
D O I
10.1016/j.matchemphys.2022.125893
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
For the CaCu3Ti4O12 (CCTO) synthesized using the molten salt method, sintered at 973-1273 K, the effect of extrinsic and intrinsic point defects on conductivity and dielectric behavior in the temperature range 300-450 K and frequency range 20 Hz-1 MHz was studied. The crystal structure, microstructures, and ionic distribution were studied by XRD, SEM, and EDS. The energy-dispersive X-ray spectroscopy, EDS, revealed qualitatively that CCTO has a minor deficiency of O and Ca and a slight excess of Ti and Cu. To maintain electrical neutrality, this results in the formation of V center dot center dot(O), e(/), h center dot, Ti3+, and Cu1+, etc., as complimentary point defects leading to an increased loss. Dielectric loss (tan delta similar to 6-7 at similar to 300 K/20 Hz) in a low-temperature regime was observed due to extrinsic defects migration with activation energy. E-a sigma dcMott's similar to 0.028 eV through Mott's variable range hopping. For temperatures >= 350 K, long-range conduction occurs due to an avalanche of intrinsic defects accumulated at sample electrode interface having activation energy, E-aArrhenius's similar to 0.177 eV, culminating in loss, tan delta similar to 40 at-450 K/20 Hz). To minimize excessive loss, compositional engineering was done in CCTO by substituting Mg at the Ti site. Judicious choice of Mg doping, having high Schottky defect formation energy (triangle H-f approximate to 7.7 eV) at Ti site (CCTMgO) resulted in almost temperature-independent dielectric constant, epsilon(r) approximate to 10(3) and a significant reduction in the loss at similar to 300-370 K in the frequency range 20 Hz -1 kHz. Phase formation, structural refinements, etc., were further investigated in CCTMgO using the Rietveld refinement technique.
引用
收藏
页数:15
相关论文
共 50 条
  • [31] Dielectric properties of Zr doped CaCu3Ti4O12 synthesized by sol-gel route
    Jesurani, S.
    Kanagesan, S.
    Hashim, M.
    Ismail, I.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2013, 551 : 456 - 462
  • [32] Dielectric Properties of CaCu3Ti4O12 Ceramics
    You, Jinghan
    Gong, Xiaoyang
    Li, Tongwei
    Chen, Qingdong
    Li, Liben
    HIGH-PERFORMANCE CERAMICS VI, 2010, 434-435 : 253 - 255
  • [33] Dielectric Properties of Polytetrafluoroethylene/CaCu3Ti4O12 Composites
    Liang, Fei
    Zhao, Yifei
    Chen, Xizi
    Wan, Qianxing
    Lue, Wenzhong
    JOURNAL OF WUHAN UNIVERSITY OF TECHNOLOGY-MATERIALS SCIENCE EDITION, 2019, 34 (01): : 189 - 194
  • [34] Electrical Conduction and Dielectric Properties of the Rb-doped CaCu3Ti4O12
    Yang, Zhi
    Zhang, Yue
    Lu, Zhihong
    Zhang, Kun
    Xiong, Rui
    Shi, Jing
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2013, 96 (03) : 806 - 811
  • [35] Effects of Ta5+ doping on microstructure evolution, dielectric properties and electrical response in CaCu3Ti4O12 ceramics
    Thongbai, Prasit
    Jumpatam, Jutapol
    Yamwong, Teerapon
    Maensiri, Santi
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2012, 32 (10) : 2423 - 2430
  • [36] Role of Relaxation on the Giant Permittivity and Electrical Properties of CaCu3Ti4O12 Ceramics
    Zhao, Xuetong
    Ren, Lulu
    Liao, Ruijin
    Li, Jianying
    Yang, Lijun
    Wang, Feipeng
    JOURNAL OF ELECTRONIC MATERIALS, 2016, 45 (06) : 3079 - 3086
  • [37] Influence of Zirconium doping on microstructure and dielectric properties of CaCu3Ti4O12 synthesized by the sol-gel method
    Sun, Li
    Wang, Zhenduo
    Hao, Wentao
    Cao, Ensi
    Zhang, Yongjia
    Peng, Hua
    JOURNAL OF ALLOYS AND COMPOUNDS, 2015, 651 : 283 - 289
  • [38] Effects of rare earth ionic doping on microstructures and electrical properties of CaCu3Ti4O12 ceramics
    Xue, Renzhong
    Chen, Zhenping
    Dai, Haiyang
    Liu, Dewei
    Li, Tao
    Zhao, Gaoyang
    MATERIALS RESEARCH BULLETIN, 2015, 66 : 254 - 261
  • [39] Giant dielectric permittivity and non-linear electrical behavior in CaCu3Ti4O12 varistors from the molten-salt synthesized powder
    Huang, Yanmin
    Liu, Laijun
    Shi, Danping
    Wu, Shuangshuang
    Zheng, Shaoying
    Fang, Liang
    Hu, Changzheng
    Elouadi, Brahim
    CERAMICS INTERNATIONAL, 2013, 39 (06) : 6063 - 6068