A DRIFT spectroscopic study of potassium acetate intercalated mechanochemically activated kaolinite

被引:19
|
作者
Frost, RL
Kristóf, J
Makó, É
Horváth, E
机构
[1] Queensland Univ Technol, Ctr Instrumental & Dev Chem, Brisbane, Qld 4001, Australia
[2] Univ Veszprem, Dept Analyt Chem, H-8201 Veszprem, Hungary
[3] Univ Veszprem, Dept Silicate & Mat Engn, H-8201 Veszprem, Hungary
[4] Univ Veszprem, Dept Environm Engn & Chem Technol, H-8201 Veszprem, Hungary
基金
澳大利亚研究理事会;
关键词
kaolinite; intercalation; mechanochemical activation; XRD; Raman microscopy; DRIFT spectroscopy;
D O I
10.1016/S1386-1425(02)00317-7
中图分类号
O433 [光谱学];
学科分类号
0703 ; 070302 ;
摘要
Kaolinite has been mechanochemically activated by dry grinding for periods of time up to 10 h. The kaolinite was then intercalated with potassium acetate and the changes in the structure followed by DRIFT spectroscopy. Intercalation of the kaolinite with potassium acetate is difficult and only the layers, which remain hydrogen bonded, are intercalated. The mechanochemical activation of the kaolinite may be followed by the loss of intensity of the hydroxyl-stretching vibrations. The intensity of the 3695 and 3619 cm(-1) bands reach a minimum after 10 h of grinding. The observation of a band at 3602 cm(-1) is indicative of the intercalation of the kaolinite with potassium acetate. The degree of intercalation decreases with mechanochemical treatment. The effect of exposure of the intercalated mechanochemically activated kaolinite to moist air results in de-intercalation. The effect of the mechanochemical treatment is loss of layer stacking, which prevents the intercalation of the kaolinite. (C) 2002 Elsevier Science B.V. All rights reserved.
引用
收藏
页码:1183 / 1194
页数:12
相关论文
共 50 条
  • [21] Kaolinite-potassium acetate and halloysite-potasium acetate complexes prepared by mechanochemical, solution and homogenization techniques: a comparative study
    Mako, E.
    Kovacs, A.
    Horvath, E.
    Kristof, J.
    CLAY MINERALS, 2014, 49 (03) : 457 - 471
  • [22] Thermal behavior and decomposition of kaolinite-potassium acetate intercalation composite
    Cheng, Hongfei
    Liu, Qinfu
    Yang, Jing
    Zhang, Qian
    Frost, Ray L.
    THERMOCHIMICA ACTA, 2010, 503 : 16 - 20
  • [23] Birdwood kaolinite: a highly ordered kaolinite that is difficult to intercalate - an XRD, SEM and Raman spectroscopic study
    Frost, RL
    Van Der Gaast, SJ
    Zbik, M
    Kloprogge, JT
    Paroz, GN
    APPLIED CLAY SCIENCE, 2002, 20 (4-5) : 177 - 187
  • [24] Delamination of kaolinite-potassium acetate intercalates by ball-milling
    Cheng, Hongfei
    Liu, Qinfu
    Zhang, Jinshan
    Yang, Jing
    Frost, Ray L.
    JOURNAL OF COLLOID AND INTERFACE SCIENCE, 2010, 348 (02) : 355 - 359
  • [25] Effect of the Preparation Conditions on Potassium Acetate-Intercalated Metakaolinite Composites
    Xu, Tao
    Han, Wei
    Li, Zhen
    Wang, Zaiqin
    PROCEEDINGS OF THE 6TH ASIAN SYMPOSIUM ON POLYMERS IN CONCRETE, 2009, : 162 - 167
  • [26] Drift spectroscopic study of the mechanism of selective shear-flocculation of hematite from kaolinite
    Gong, WQ
    JOURNAL OF WUHAN UNIVERSITY OF TECHNOLOGY-MATERIALS SCIENCE EDITION, 1997, 12 (1-2): : 83 - 93
  • [27] DRIFT SPECTROSCOPIC STUDY OF THE MECHANISM OF SELECTIVE SHEAR-FLOCCULATION OF HEMATITE FROM KAOLINITE
    龚文琪
    Journal of Wuhan University of Technology-Materials Science, 1997, (Z1) : 83 - 93
  • [28] The molecular structure of kaolinite-potassium acetate intercalation complexes: A combined experimental and molecular dynamic simulation study
    Cheng, Hongfei
    Zhang, Shuai
    Liu, Qinfu
    Li, Xiaoguang
    Frost, Ray L.
    APPLIED CLAY SCIENCE, 2015, 116 : 273 - 280
  • [29] Rehydration and phase changes of potassium acetate-intercalated halloysite at 298 K
    Frost, RL
    Kristof, J
    Horvath, E
    Kloprogge, JT
    JOURNAL OF COLLOID AND INTERFACE SCIENCE, 2000, 226 (02) : 318 - 327
  • [30] Calorimetric study of the mechanochemically activated sphalerite
    Xiao, ZL
    Chen, QY
    Yin, ZN
    Zhang, PM
    THERMOCHIMICA ACTA, 2003, 404 (1-2) : 265 - 270