Cavitation Erosion Resistance and Wear Mechanism Model of Flame-Sprayed Al2O3-40%TiO2/NiMoAl Cermet Coatings

被引:37
作者
Szala, Miroslaw [1 ]
Hejwowski, Tadeusz [1 ]
机构
[1] Lublin Univ Technol, Dept Mat Engn, Fac Mech Engn, Nadbystrzycka 36D, PL-20618 Lublin, Poland
关键词
cermet coating; aluminia-titania; thermal spraying; flame spraying; cavitation erosion; microstructure; wear model; THERMAL BARRIER COATINGS; TRIBOLOGICAL BEHAVIOR; TIO2; SUPERALLOYS;
D O I
10.3390/coatings8070254
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
This manuscript deals with the cavitation erosion resistance of flame-sprayed Al2O3-40%TiO2/NiMoAl cermet coatings (low-velocity oxy-fuel (LVOF)), a new functional application of cermet coatings. The aim of the study was to investigate the cavitation erosion mechanism and determine the effect of feedstock powder ratio (Al2O3-TiO2/NiMoAl) of LVOF-sprayed cermet coatings on their cavitation erosion resistance. As-sprayed coatings were investigated for roughness, porosity, hardness, and Young's modulus. Microstructural characteristics of the cross section and the surface of as-sprayed coatings were examined by light optical microscopy (LOM), scanning electron microscopy (SEM) with energy-dispersive X-ray spectroscopy (EDS) and X-ray diffraction (XRD) methods. Coating cavitation tests were conducted in accordance with the ASTM G32 standard using an alternative stationary specimen testing method with usage of reference samples made from steel, copper, and aluminum alloys. Cavitation erosion resistance was measured by weight and volume loss, and normalised cavitation erosion resistance was calculated. Surface eroded due to cavitation was examined in successive time intervals by LOM and SEM-EDS. On the basis of coating properties and cavitation investigations, a phenomenological model of the cavitation erosion of Al2O3-40%TiO2/NiMoAl cermet coatings was elaborated. General relationships between their properties, microstructure, and cavitation wear resistance were established. The Al2O3-40%TiO2/NiMoAl composite coating containing 80% ceramic powder has a higher cavitation erosion resistance than the reference aluminium alloy.
引用
收藏
页数:19
相关论文
共 31 条
[21]   Oxidation resistance of low-velocity oxy fuel-sprayed Al2O3-13TiO2 coating on nickel-based superalloys at 800 °C [J].
Mishra, N. K. ;
Mishra, S. B. ;
Kumar, R. .
SURFACE & COATINGS TECHNOLOGY, 2014, 260 :23-27
[22]  
Morks M., 2008, J MANUF PROCESS, V10, P1, DOI [10.1016/j.jmapro.2008.10.001, DOI 10.1016/J.JMAPRO.2008.10.001]
[23]   Slurry and cavitation erosion resistance of thermal spray coatings [J].
Santa, J. F. ;
Espitia, L. A. ;
Blanco, J. A. ;
Romo, S. A. ;
Toro, A. .
WEAR, 2009, 267 (1-4) :160-167
[24]   The dependency of microstructure and properties of nanostructured coatings on plasma spray conditions [J].
Shaw, LL ;
Goberman, D ;
Ren, RM ;
Gell, M ;
Jiang, S ;
Wang, Y ;
Xiao, TD ;
Strutt, PR .
SURFACE & COATINGS TECHNOLOGY, 2000, 130 (01) :1-8
[25]   International Cavitation Erosion Test and quantitative assessment of material resistance to cavitation [J].
Steller, J .
WEAR, 1999, 233 :51-64
[26]   Application of computer image analysis software for determining incubation period of cavitation erosion - preliminary results [J].
Szala, Miroslaw .
II INTERNATIONAL CONFERENCE OF COMPUTATIONAL METHODS IN ENGINEERING SCIENCE (CMES'17), 2017, 15
[27]   Thermally sprayed coatings resistant to erosion and corrosion for power plant boilers - A review [J].
Szymanski, Krzysztof ;
Hernas, Adam ;
Moskal, Grzegorz ;
Myalska, Hanna .
SURFACE & COATINGS TECHNOLOGY, 2015, 268 :153-164
[28]   Cavitation erosion of aluminas [J].
Tomlinson, W ;
Kalitsounakis, N ;
Vekinis, G .
CERAMICS INTERNATIONAL, 1999, 25 (04) :331-338
[29]  
Tucker R.C., 2013, ASM HDB A, V5
[30]  
Yao Y., 2016, J MAT SCI CHEM ENG, V04, P8, DOI DOI 10.4236/MSCE.2016.47002