Hot Deformation Behavior of a Ni-Based Superalloy with Suppressed Precipitation

被引:10
作者
Lizzi, Franco [1 ,2 ,3 ]
Pradeep, Kashyap [3 ,4 ]
Stanojevic, Aleksandar [5 ]
Sommadossi, Silvana [1 ,2 ]
Poletti, Maria Cecilia [3 ,4 ]
机构
[1] Comahue Natl Univ, Mat Characterizat, RA-8300 Neuquen, Argentina
[2] IITCI CONICET UNCo, RA-8300 Neuquen, Argentina
[3] Christian Doppler Lab Design High Performance All, A-8010 Graz, Austria
[4] Graz Univ Technol, Inst Mat Sci Joining & Forming, A-8010 Graz, Austria
[5] Voestalpine Bohler Aerosp GmbH & Co KG, A-8605 Kapfenberg, Austria
关键词
Inconel(&#174); 718; hot deformation; Gleeble; recrystallization; flow modelling approach; POST-DYNAMIC RECRYSTALLIZATION; INCONEL; 718; ALLOY; CONSTITUTIVE-EQUATIONS; DELTA-PHASE; STRAIN-RATE; EVOLUTION; KINETICS; WORKABILITY; TEMPERATURE; MECHANISMS;
D O I
10.3390/met11040605
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Inconel(R)718 is a well-known nickel-based super-alloy used for high-temperature applications after thermomechanical processes followed by heat treatments. This work describes the evolution of the microstructure and the stresses during hot deformation of a prototype alloy named IN718WP produced by powder metallurgy with similar chemical composition to the matrix of Inconel(R)718. Compression tests were performed by the thermomechanical simulator Gleeble(R)3800 in a temperature range from 900 to 1025 degrees C, and strain rates scaled from 0.001 to 10 s(-1). Flow curves of IN718WP showed similar features to those of Inconel(R)718. The relative stress softening of the IN718WP was comparable to standard alloy Inconel(R)718 for the highest strain rates. Large stress softening at low strain rates may be related to two phenomena: the fast recrystallization rate, and the coarsening of micropores driven by diffusion. Dynamic recrystallization grade and grain size were quantified using metallography. The recrystallization grade increased as the strain rate decreased, although showed less dependency on the temperature. Dynamic recrystallization occurred after the formation of deformation bands at strain rates above 0.1 s(-1) and after the formation of subgrains when deforming at low strain rates. Recrystallized grains had a large number of sigma 3 boundaries, and their percentage increased with strain rate and temperature. The calculated apparent activation energy and strain rate exponent value were similar to those found for Inconel(R)718 when deforming above the solvus temperature.
引用
收藏
页数:18