Effect of sp2 phase content on hydrophobicity of diamond layers

被引:0
作者
Mosinska, Lidia [1 ]
Popielarski, Pawel [1 ]
Popielarski, Piotr [1 ]
Frankow, Wojciech [1 ]
Banaszak-Piechowska, Agnieszm [1 ]
机构
[1] Univ Kazimierza Wielkiego, Bydgoszcz, Poland
来源
PRZEMYSL CHEMICZNY | 2014年 / 93卷 / 09期
关键词
CHEMICAL-VAPOR-DEPOSITION; CONTACT-ANGLE MEASUREMENT; RAMAN-SPECTROSCOPY; QUALITY; GROWTH; CARBON; FILMS;
D O I
暂无
中图分类号
O6 [化学];
学科分类号
0703 ;
摘要
Diamond layers were deposited on Si substrate by hot-filament chem. vapour deposition from MeOH/H-2 mixt. and studied for crystal structure, hydrophobic properties (contact angle) and crystallite size (0,72-1,04 mu m). The morphol. was confirmed by Raman spectroscopy (content of sp(2) phase).
引用
收藏
页码:1587 / 1590
页数:4
相关论文
共 50 条
  • [1] Quinone electrochemistry for the comparative assessment of sp2 surface content of boron doped diamond electrodes
    Ayres, Zoe J.
    Cobb, Sam J.
    Newton, Mark E.
    Macpherson, Julie V.
    ELECTROCHEMISTRY COMMUNICATIONS, 2016, 72 : 59 - 63
  • [2] Structural defects and sp2 localization in CVD diamond
    Monteiro, Othon R.
    JOURNAL OF MATERIALS SCIENCE, 2019, 54 (03) : 2300 - 2306
  • [3] Detecting sp2 phase on diamond surfaces by atomic force microscopy phase imaging and its effects on surface conductivity
    Kozak, H.
    Kromka, A.
    Ukraintsev, E.
    Houdkova, J.
    Ledinsky, M.
    Vanecek, M.
    Rezek, B.
    DIAMOND AND RELATED MATERIALS, 2009, 18 (5-8) : 722 - 725
  • [4] Doped diamond electrodes on titanium substrates with controlled sp2/sp3 hybridization at different boron levels
    Migliorini, F. L.
    Alegre, M. D.
    Baldan, M. R.
    Lanza, M. R. V.
    Ferreira, N. G.
    THIN SOLID FILMS, 2014, 564 : 97 - 103
  • [5] Influence of the sp2 content on boron doped diamond electrodes applied in the textile dye electrooxidation
    Migliorini, F. L.
    Alegre, M. D.
    Alves, S. A.
    Lanza, M. R. V.
    Baldan, M. R.
    Ferreira, N. G.
    SYNTHESIS AND ELECTROCHEMICAL ENGINEERING (GENERAL) - 224TH ECS MEETING, 2014, 58 (19): : 27 - 33
  • [6] Correlation between tribological properties, sp2/sp3-ratio and H-content of low-wear diamond-like carbon (DLC) layers
    Vogli, E.
    Hoffmann, F.
    Bartis, E.
    Oehrlein, G. S.
    Tillmann, W.
    THERMEC 2011, PTS 1-4, 2012, 706-709 : 2596 - +
  • [7] Laser-patterned boron-doped diamond electrodes with precise control of sp2/sp3 carbon lateral distribution
    Hrabovsky, J.
    Zelensky, M.
    Sladek, J.
    Zukerstein, M.
    Fischer, J.
    Schwarzova-Peckova, K.
    Taylor, A.
    Veis, M.
    Mandal, S.
    Williams, O. A.
    Bulgakova, N. M.
    APPLIED SURFACE SCIENCE, 2023, 639
  • [8] Enhanced electrochemical ozone production via sp2 carbon content optimization in boron doped diamond electrodes using laser micromachining
    Tully, Joshua J.
    Rodriguez, Irina M. Terrero
    Kaewsen, Manisa
    Wood, Georgia F.
    Houghton, Daniel
    Han, Yisong
    Mollart, Timothy P.
    Macpherson, Julie V.
    CARBON, 2024, 228
  • [9] Optimization of Polycrystalline CVD Diamond Seeding with the Use of sp3/sp2 Raman Band Ratio
    Golunski, L.
    Sobaszek, M.
    Gardas, M.
    Gnyba, M.
    Bogdanowicz, R.
    Ficek, M.
    Plotka, P.
    ACTA PHYSICA POLONICA A, 2015, 128 (01) : 136 - 140
  • [10] Impact of chemical vapour deposition plasma inhomogeneity on the spatial variation of sp2 carbon in boron doped diamond electrodes
    Ayres, Zoe J.
    Newland, Jonathan C.
    Newton, Mark E.
    Mandal, Soumen
    Williams, Oliver A.
    Macpherson, Julie V.
    CARBON, 2017, 121 : 434 - 442