Effect of microstructural parameters and Al alloying on creep behavior, threshold stress and activation volumes of molybdenum disilicides

被引:13
作者
Mitra, R
Sadananda, K
Feng, CR
机构
[1] USN, Res Lab, Div Mat Sci & Technol, Washington, DC 20375 USA
[2] Indian Inst Technol, Dept Met & Mat Engn, Kharagpur 721302, W Bengal, India
关键词
molybdenum silicides; composites; ternary alloy systems; creep; grain boundaries; structure;
D O I
10.1016/j.intermet.2004.02.033
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Creep behavior of several molybdenum disilicides, with varying grain sizes, silica content, SiC reinforcement, or Al additions has been studied at 1200 degreesC, and compared with the deformation behavior at constant strain rates. The effect of grain size on creep rate supercedes all other factors. A high silica content is less deleterious at coarser grain sizes in the dislocation creep range. In addition, 20 vol% SiC reinforcement of MoSi2 can enhance creep strength, if grain size remains coarse. Furthermore, Al addition has been found to be beneficial up to a critical concentration, which helps in the removal of silica at grain boundaries, while retaining the tetragonal structure of MoSi2. threshold stress for creep can arise due to the build up of internal stresses at second phase particles or dislocation networks. These stresses inhibit further movement of dislocations. The activation volume was found to vary between 27b(3) and 2b(3) with applied stress, where b is the Burgers vector. This implies that the rate controlling creep mechanism can be overcoming glide type of barrier (say, Peierls stress) at low stresses, and dislocation climb at higher stresses. (C) 2004 Published by Elsevier Ltd.
引用
收藏
页码:827 / 836
页数:10
相关论文
共 33 条
[1]  
Campbell J. P., 1995, High-Temperature Ordered Intermetallic Alloys VI. Symposium, P893
[2]   THERMALLY ACTIVATED DEFORMATION OF METALS [J].
CONRAD, H .
JOM-JOURNAL OF METALS, 1964, 16 (07) :582-&
[3]  
DIETER GE, 1986, MECH METALLURGY, P179
[4]  
FRANKWICZ PS, 1993, MAT RES S C, V288, P159
[5]  
FRNECH JD, 1995, CERAM ENG SCI P, V16, P129
[6]  
GHOSH AK, 1992, MATER RES SOC SYMP P, V273, P259, DOI 10.1557/PROC-273-259
[7]   Dislocation processes during the deformation of MoSi2 single crystals in a soft orientation [J].
Guder, S ;
Bartsch, M ;
Yamaguchi, M ;
Messerschmidt, U .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1999, 261 (1-2) :139-146
[8]  
GUZEI LS, 1990, TERNARY ALLOYS COMPR, V7, P226
[9]   Effects of carbon additions on MoSi2 microstructure and properties [J].
Idasetima, JS ;
Petrovic, JJ .
PHILOSOPHICAL MAGAZINE A-PHYSICS OF CONDENSED MATTER STRUCTURE DEFECTS AND MECHANICAL PROPERTIES, 1997, 76 (02) :271-287
[10]   Creep deformation of single crystals of binary and some ternary MoSi2 with the C11b structure [J].
Inui, H ;
Ishikawa, K ;
Yamaguchi, M .
INTERMETALLICS, 2000, 8 (9-11) :1159-1168