In-situ investigations of hydrogen influenced crack initiation and propagation under tensile and low cycle fatigue loadings in RPV steel

被引:22
|
作者
Singh, Rajwinder [1 ]
Singh, Vishal [1 ]
Arora, Aman [1 ]
Mahajan, Dhiraj K. [1 ]
机构
[1] Indian Inst Technol Ropar, Dept Mech Engn, Ropar Mech Mat Lab, Rupnagar 140001, Punjab, India
关键词
SA508 grade 3 class I low alloy steel; Tensile loading; Low cycle fatigue loading; Hydrogen charging; Crack initiation; Crack propagation; PRESSURE-VESSEL STEELS; LOW-ALLOY STEEL; FRACTURE-BEHAVIOR; STRAIN-RATE; MECHANICAL-PROPERTIES; GROWTH-BEHAVIOR; EMBRITTLEMENT; DEFORMATION; TEMPERATURE; PLASTICITY;
D O I
10.1016/j.jnucmat.2019.151912
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Present work aims to unveil the mechanism of hydrogen embrittlement (HE) in SA508 Grade 3 Class I low alloy reactor pressure vessel (RPV) steel. In-situ tensile and low cycle fatigue (LCF) tests are performed on specially designed specimens using tensile/fatigue testing stage under scanning electron microscope (SEM). Electrochemical hydrogen charging resulted in localized void formation at prior austenite grain boundaries (PAGBs) during tensile loading. Alongside the hydrogen induced weakening of PAGBs due to synergetic HELP (hydrogen enhanced localized plasticity) and HEDE (hydrogen enhanced decohesion) mechanisms of HE, fish-eyes formation around Al2O3-SiO2 type inclusions are the primary factors for hydrogen enhanced tensile properties degradation in subject RPV steel. During LCF loading, crack initiation and propagation is facilitated by long rod inter-lath cementite particles distributed along the bainitic ferrite lath boundaries in the un-charged specimen. In case of hydrogen charged specimen, the edge crack formed during LCF loading propagated through the specimen by cleavage. Predominantly plasticity (slip) driven transgranular crack propagation occurred in un-charged specimen. In contrary, hydrogen charging resulted in LCF crack to propagate in mixed intergranular and transgranular manner during early stages of propagation, whereas once the crack length exceeded 5 to 6 grains, cleavage type transgranular crack propagation was observed. (C) 2019 Elsevier B.V. All rights reserved.
引用
收藏
页数:13
相关论文
共 50 条
  • [21] Characteristic Fatigue Crack Growth Behavior of Low Carbon Steel Under Low-pressure Hydrogen Gas Atmosphere
    Ohnishi, Yosuke
    Koyama, Motomichi
    Sasaki, Daisuke
    Noguchi, Hiroshi
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 2015, 101 (11): : 605 - 610
  • [22] An in situ fatigue-CZM for unified crack initiation and propagation in composites under cyclic loading
    Nojavan, S.
    Schesser, D.
    Yang, Q. D.
    COMPOSITE STRUCTURES, 2016, 146 : 34 - 49
  • [23] In-situ observation and finite element analysis of fretting fatigue crack propagation behavior in 1045 steel
    Han, Qinan
    Lei, Xusheng
    Su, Yue
    Rui, Shaoshi
    Ma, Xianfeng
    Cui, Haitao
    Shi, Huiji
    CHINESE JOURNAL OF AERONAUTICS, 2021, 34 (11) : 131 - 139
  • [24] Effect of microstructure on slip-induced crack initiation and early propagation of martensitic steel during high cycle fatigue
    Dai, Yajun
    Wang, Shijian
    He, Qiyuan
    Liu, Chang
    Wang, Xianyu
    Li, Xue
    Li, Lang
    Liu, Yongjie
    He, Chao
    Wang, Qingyuan
    INTERNATIONAL JOURNAL OF FATIGUE, 2023, 167
  • [25] Crack initiation mechanism of M50 bearing steel under high cycle fatigue
    Guo, Jun
    Zhao, Aimin
    Yang, Maosheng
    INTERNATIONAL JOURNAL OF FATIGUE, 2023, 174
  • [26] The influence of stress levels on crack initiation and propagation behaviors of an Al-Li alloy under high cycle fatigue
    Yang, Xusheng
    Xiao, Wenya
    Huang, Weijiu
    Zhu, Xianghui
    Liu, Mofang
    Qian, Yuanzhi
    INTERNATIONAL JOURNAL OF FATIGUE, 2025, 197
  • [27] The propagation of a circumferential fatigue crack in medium-carbon steel bars under combined torsional and axial loadings
    Tanaka, K
    Akinawa, Y
    Yu, HC
    MIXED-MODE CRACK BEHAVIOR, 1999, 1359 : 295 - 311
  • [29] Effects of Vanadium Addition on Strain Distribution, Crack Initiation and Propagation during Low-cycle Fatigue Test in Ferrite and Martensite Dual-phase Steel
    Koga, Norimitsu
    Kaseya, Akihiro
    Umezawa, Osamu
    Nakata, Hiroshi
    Toyoda, Shunsuke
    ISIJ INTERNATIONAL, 2022, 62 (10) : 2132 - 2134
  • [30] Low-cycle fatigue crack initiation and propagation from controlled surface imperfections in nuclear steels
    Cussac, Paul
    Gardin, Catherine
    Pelosin, Veronique
    Henaff, Gilbert
    de Baglion, Laurent
    Ancelet, Olivier
    Courtin, Stephan
    INTERNATIONAL JOURNAL OF FATIGUE, 2020, 139