Wear protection for titanium components

被引:0
作者
Bobzin, K. [1 ]
Ernst, F. [1 ]
Roesing, J. [1 ]
Rojas, Y. [1 ]
机构
[1] Rhein Westfal TH Aachen, Inst Oberflachentech, D-52070 Aachen, Germany
关键词
wear resistance; wear protection; brazing; titanium; tribology;
D O I
10.1002/mawe.200600106
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The use of titanium and its alloys in the last decades keeps on increasing due to its material-specific characteristics like high firmness, good corrosion characteristics and very high thermal maximum stress. However nowadays, the use of titanium components in systems where wear resistance is important is limited by titanium's relatively low wear resistance. Surface wear is in principle a characteristic, conditioned by chemical and physical effects of the elements involved as well as collective stress. The necessity for new systems where good wear resistance and excellent mechanical properties are combined keeps on showing up. Due to titanium's tendency to react with surrounding media, titanium alloys are difficult to be welded. Embrittlement by admission of hydrogen and oxygen can occur at high temperature processes or even changes on titanium's microstructure may appear. Brazing techniques, which are actually applied to steel, have been modified and adapted for using them to titanium materials. Here, commercially available braze pastes and hard materials where combined and applied on titanium.
引用
收藏
页码:160 / 163
页数:4
相关论文
共 50 条
[21]   Surface Nitriding and Improvement of Wear Resistance of Titanium Using Laser Irradiation [J].
Yamaguchi, Tomiko ;
Yonesho, Yutaka ;
Nishio, Kazumasa .
JOURNAL OF THE JAPAN INSTITUTE OF METALS, 2011, 75 (12) :697-704
[22]   TOPOGRAPHY, HARDNESS, ELASTIC MODULUS AND WEAR RESISTANCE OF NITRIDE COATINGS ON TITANIUM [J].
Pohrelyuk, I. M. ;
Padgurskas, J. ;
Lavrys, S. M. ;
Luk'yanenko, A. G. ;
Trush, V. S. ;
Kreivaitis, R. .
PROCEEDINGS OF IX INTERNATIONAL SCIENTIFIC CONFERENCE (BALTTRIB 2017), 2018, :41-46
[23]   Friction and wear properties of titanium and oxidised titanium in dry sliding against hardened C45 steel [J].
Król, S ;
Ptacek, L ;
Zalisz, Z ;
Hepner, M .
JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2004, 157 :364-369
[24]   Improving Wear Resistance of Highly Porous Titanium by Surface Engineering Methods [J].
Lavrys, Serhii ;
Pohrelyuk, Iryna ;
Padgurskas, Juozas ;
Shliakhetka, Khrystyna .
COATINGS, 2023, 13 (10)
[25]   Influence of Porosity on Wear Resistance of Sintered Titanium under Boundary Lubrication [J].
I. M. Pohreluyk ;
S. M. Lavrys ;
O. H. Lukyanenko .
Journal of Friction and Wear, 2021, 42 :461-465
[26]   Influence of Porosity on Wear Resistance of Sintered Titanium under Boundary Lubrication [J].
Pohreluyk, I. M. ;
Lavrys, S. M. ;
Lukyanenko, O. H. .
JOURNAL OF FRICTION AND WEAR, 2021, 42 (06) :461-465
[27]   Microstructure and wear resistance of red mud iron alloy with chromium and titanium [J].
Zhou, Jiachang ;
Kang, Heyi ;
Wei, Haiping ;
Tang, Hongqun ;
Ou, Xingcheng ;
Luo, Chaoqin .
COMPOSITES AND ADVANCED MATERIALS, 2021, 30
[28]   Friction and wear behavior of titanium matrix (TiB plus TiC) composites [J].
Kim, I. Y. ;
Choi, B. J. ;
Kim, Y. J. ;
Lee, Y. Z. .
WEAR, 2011, 271 (9-10) :1962-1965
[29]   Designer surfaces for titanium components [J].
Dong, HS ;
Bell, T .
INDUSTRIAL LUBRICATION AND TRIBOLOGY, 1998, 50 (06) :282-+
[30]   Designer surfaces for titanium components [J].
Dong, HS ;
Bell, T .
ANTI-CORROSION METHODS AND MATERIALS, 1999, 46 (05) :338-345