Iron self-diffusion in nanocrystalline FeZr thin films

被引:9
作者
Gupta, A
Gupta, M
Pietsch, U
Ayachit, S
Rajagopalanl, S
Balamurgan, AK
Tyagi, AK
机构
[1] Interuniv Consortium, DAE Facil, Indore 452017, India
[2] Neutron Scattering Lab, CH-5232 Villigen, Switzerland
[3] Swiss Fed Inst Technol, Paul Scherrer Inst, CH-5232 Villigen, Switzerland
[4] Univ Potsdam, Inst Phys, D-14469 Potsdam, Germany
[5] Indira Gandhi Ctr Atom Res, MSD, Kalpakkam 603102, Tamil Nadu, India
关键词
D O I
10.1016/j.jnoncrysol.2004.07.051
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Thin films of amorphous Fe85Zr15 alloy were deposited by ion-beam sputtering of a composite target. Analogous to the melt-spun amorphous alloys of similar composition, the crystallization of the amorphous film occurs in two steps, however, with a substantially reduced thermal stability. After completion of the first crystallization step which starts at 473 K, the microstructure consists of 12 nm nanocrystals of bcc-Fe embedded in a grain boundary region of the remaining amorphous phase. At 673 K, the remaining amorphous phase transforms into the Fe2Zr alloy. The self-diffusion measurements of iron in the nanocrystalline state and in the parent amorphous state has been carried out using secondary ion mass spectroscopy (SIMS) depth profiling and neutron reflectivity techniques. In contrast to the case of finemet Fe73.5Si13.5B9Nb3Cu1 alloy, where a significant enhancement of diffusivity takes place in the nanocrystalline state, in the present case the diffusivity in the nanocrystalline state is similar to that in the parent amorphous state. It is suggested that in this system the atomic diffusion occurs mainly via the grain boundary regions. The calculated values of the pre-exponential factor and the activation energy for the diffusion are D-0 = 1 x 10(-14+/-1) m(2)/s and E = (0.7 +/- 0.1) eV respectively. (C) 2004 Published by Elsevier B.V.
引用
收藏
页码:39 / 47
页数:9
相关论文
共 42 条
  • [21] KRONMULLER H, 1995, NATO ADV SCI INST SE, V278, P271
  • [22] On the origin of stress-anneal-induced anisotropy in FINEMET-type nanocrystalline magnets
    Lachowicz, HK
    Neuweiler, A
    Poplawski, F
    Dynowska, E
    [J]. JOURNAL OF MAGNETISM AND MAGNETIC MATERIALS, 1997, 173 (03) : 287 - 294
  • [23] AN EXAMINATION OF THE SOURCES OF VARIATION IN THE MEASURED PROPERTIES OF FE80B20 GLASS
    LEAKE, JA
    GREER, AL
    [J]. JOURNAL OF NON-CRYSTALLINE SOLIDS, 1980, 38-9 (MAY-) : 735 - 740
  • [24] A SIMS investigation of tracer diffusivities in an amorphous Ni54Z46 alloy
    Loirat, Y
    Bocquet, JL
    Limoge, Y
    [J]. JOURNAL OF NON-CRYSTALLINE SOLIDS, 2000, 265 (03) : 252 - 264
  • [25] SELF-DIFFUSION IN ALPHA-IRON - THE INFLUENCE OF DISLOCATIONS AND THE EFFECT OF THE MAGNETIC PHASE-TRANSITION
    LUBBEHUSEN, M
    MEHRER, H
    [J]. ACTA METALLURGICA ET MATERIALIA, 1990, 38 (02): : 283 - 292
  • [26] SURFACE STUDIES OF SOLIDS BY TOTAL REFLECTION OF X-RAYS
    PARRATT, LG
    [J]. PHYSICAL REVIEW, 1954, 95 (02): : 359 - 369
  • [27] EFFECT OF HOMOGENEOUS DEFORMATION ON THE CRYSTALLIZATION OF A METALLIC GLASS
    PATTERSON, J
    JONES, DRH
    [J]. SCRIPTA METALLURGICA, 1979, 13 (10): : 947 - 949
  • [28] MODIFICATION OF PD77SI23 METALLIC GLASSES BY PICOSECOND LASER ANNEALING
    RADLINSKI, AP
    CALKA, A
    LUTHERDAVIES, B
    [J]. PHYSICAL REVIEW LETTERS, 1986, 57 (24) : 3081 - 3084
  • [29] RAO PR, 1989, REV SOLID STATE SCI, V3, P311
  • [30] SHEWMON PG, 1963, DIFFUSION SOLIDS, P7