Short shots and industrial case studies: Understanding fluid flow and solidification in high pressure die casting

被引:48
作者
Cleary, Paul W. [1 ]
Ha, Joseph [1 ]
Prakash, Mahesh [1 ]
Nguyen, Thang [2 ]
机构
[1] CSIRO Math & Informat Sci, Clayton, Vic 3169, Australia
[2] CSIRO Mat Sci & Engn, Clayton, Vic 3169, Australia
关键词
High pressure die casting; SPH; Solidification; Short shot; Fluid flow; Casting defects; SMOOTHED PARTICLE HYDRODYNAMICS; SPH; SIMULATION;
D O I
10.1016/j.apm.2009.10.015
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The geometric complexity and high fluid speeds involved in high pressure die casting (HPDC) combine to give strongly three dimensional fluid flow with significant free surface fragmentation and splashing. A simulation method that has proved particularly suited to modelling HPDC is Smoothed Particle Hydrodynamics (SPH). Materials are approximated by particles that are free to move around rather than by fixed grids, enabling more accurate prediction of fluid flows involving complex free surface motion. Three practical industrial case studies of SPH simulated HPDC flows are presented; aluminium casting of a differential cover (automotive), an electronic housing and zinc casting of a door lock plate. These show significant detail in the fragmented fluid free surfaces and allow us to understand the predisposition to create defects such as porosity in the castings. The validation of flow predictions coupled with heat transfer and solidification is an important area for such modelling. One powerful approach is to use short shots, where insufficient metal is used in the casting or the casting shot is halted part way through, to leave the die cavity only partially filled. The frozen partial castings capture significant detail about the order of fill and the flow structures occurring during different stages of filling. Validation can occur by matching experimental and simulated short shots. Here we explore the effect of die temperature, metal super-heat and volume fill on the short shots for the casting of a simple coaster. The bulk features of the final solid castings are found to be in good agreement with the predictions, but the fine details appear to depend on surface behaviour of the solidifying metals. This potentially has significant implications for modelling HPDC. (C) 2009 Elsevier Inc. All rights reserved.
引用
收藏
页码:2018 / 2033
页数:16
相关论文
共 14 条
[1]   3D SPH flow predictions and validation for high pressure die casting of automotive components [J].
Cleary, P. W. ;
Ha, J. ;
Prakash, M. ;
Nguyen, T. .
APPLIED MATHEMATICAL MODELLING, 2006, 30 (11) :1406-1427
[2]   Smooth particle hydrodynamics: status and future potential [J].
Cleary, Paul W. ;
Prakash, Mahesh ;
Ha, Joseph ;
Stokes, Nick ;
Scott, Craig .
PROGRESS IN COMPUTATIONAL FLUID DYNAMICS, 2007, 7 (2-4) :70-90
[3]   Modelling confined multi-material heat and mass flows using SPH [J].
Cleary, PW .
APPLIED MATHEMATICAL MODELLING, 1998, 22 (12) :981-993
[4]   Conduction modelling using smoothed particle hydrodynamics [J].
Cleary, PW ;
Monaghan, JJ .
JOURNAL OF COMPUTATIONAL PHYSICS, 1999, 148 (01) :227-264
[5]   High pressure die casting simulation using smoothed particle hydrodynamics [J].
Cleary, PW ;
Ha, J ;
Ahuja, V .
INTERNATIONAL JOURNAL OF CAST METALS RESEARCH, 2000, 12 (06) :335-355
[6]   Comparison of SPH simulations of high pressure die casting with the experiments and VOF simulations of Schmid and Klein [J].
Ha, J ;
Cleary, PW .
INTERNATIONAL JOURNAL OF CAST METALS RESEARCH, 2000, 12 (06) :409-418
[7]   Simulation of high pressure die filling of a moderately complex industrial object using smoothed particle hydrodynamics [J].
Ha, J ;
Cleary, PW .
INTERNATIONAL JOURNAL OF CAST METALS RESEARCH, 2005, 18 (02) :81-92
[8]  
HA J, 1999, P 2 INT C CFD MIN PR, P423
[9]  
Kokot V., 2006, P 20 MCWASP C FRANC
[10]   Integrated optimization system for high pressure die casting processes [J].
Kong, L. X. ;
She, F. H. ;
Gao, W. M. ;
Nahavandi, S. ;
Hodgson, P. D. .
JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2008, 201 (1-3) :629-634