Surface passivation of 5556 aluminum alloy in solutions based on cerium nitrate

被引:9
作者
Abrashov, A. A. [1 ]
Grigoryan, N. S. [1 ]
Vagramyan, T. A. [1 ]
Simonova, M. A. [1 ]
Miroshnikov, V. S. [1 ]
Arkhipushkin, I. A. [2 ]
机构
[1] Mendeleev Univ Chem Technol, Miusskaya Sq 9, Moscow 125047, Russia
[2] Russian Acad Sci, AN Frumkin Inst Phys Chem & Electrochem, Leninsky Pr 31, Moscow 119071, Russia
来源
INTERNATIONAL JOURNAL OF CORROSION AND SCALE INHIBITION | 2021年 / 10卷 / 01期
关键词
corrosion protection; conversion coatings; cerium-containing coatings; surface treatment; chromate free passivation; rare earth metals; CHROMATE CONVERSION COATINGS; CORROSION PROTECTION; INHIBITION; XPS;
D O I
10.17675/2305-6894-2021-10-1-8
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
A solution has been developed for applying protective-adhesive cerium-containing coatings to the surface of the 5556 aluminum alloy in order to replace the toxic chromating process in the automotive and other industries. The developed solution contains: 5-10 g/l Ce(NO3)3 center dot 6H(2)O, 30-40 ml/l H2O2 and 0.5-1.5 g/l gallic acid ester. Coatings with the best physicochemical characteristics are formed in a solution with pH=2-3 at a temperature of 18-25 degrees C and a process duration of 10-15 minutes. The optimum drying temperature is 120-160 degrees C. The coatings formed under these conditions consist of cerium oxides CeO2, Ce2O3 and aluminum oxide Al2O3. The addition of a gallic acid ester (in an amount of 0.5-1.5 g/l) to the working solution leads to a change in the chemical composition of the forming coatings, namely, to the exclusion of CeO2 compounds in their composition. This increases the protective ability of coatings. Corrosion tests in a salt-spray chamber have shown that the developed cerium-containing coatings are superior in protective ability to the currently widely used chromate coatings. The developed coatings have good adhesion properties and withstand exposure to high temperatures without degradation of their protective properties. Adhesion after 750 hours of salt-spray corrosion tests decreased by 13.0 and 13.8% for cerium-containing and chromate coatings, respectively. The thickness of cerium-containing coatings is 280-320 mu. The developed solution for the formation of protective adhesive coatings on aluminum is an alternative to toxic chromating solutions.
引用
收藏
页码:132 / 144
页数:13
相关论文
共 31 条
[1]  
[Anonymous], OFF J EUR COMMUNITIE, VL269, P34
[2]  
[Anonymous], 2003, Guidance Document No. 5. Transitional and Coastal Waters-Typology, Reference Conditions and Classification Systems
[3]  
[Anonymous], Directive 2011/65 / EC (RoHS II) of the European Parliament and of the Council of 8 June 2011 on the restriction of the use of certain hazardous substances in electrical and electronic equipment
[4]  
ASTM, 2017, D454117 ASTM
[5]  
Chen SY, 2015, INT J ELECTROCHEM SC, V10, P9073
[6]  
Cumpson PJ, 1997, SURF INTERFACE ANAL, V25, P430, DOI 10.1002/(SICI)1096-9918(199706)25:6<430::AID-SIA254>3.0.CO
[7]  
2-7
[8]   Corrosion resistance of cerium-based chemical conversion coatings on AA5083 aluminium alloy [J].
Dabalà, M ;
Ramous, E ;
Magrini, M .
MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 2004, 55 (05) :381-386
[9]   Chromate conversion coated aluminium as a lightweight and corrosion-resistant current collector for aqueous lithium-ion batteries [J].
Gheytani, Saman ;
Liang, Yanliang ;
Jing, Yan ;
Xu, Jeff Q. ;
Yao, Yan .
JOURNAL OF MATERIALS CHEMISTRY A, 2016, 4 (02) :395-399
[10]   Corrosion protection mechanism of Ce4+/organic inhibitor for AA2024 in 3.5% NaCl [J].
Gobara, Mohamed ;
Baraka, Ahmad ;
Akid, Robert ;
Zorainy, Mahmoud .
RSC ADVANCES, 2020, 10 (04) :2227-2240