Time-resolved X-ray scattering and calorimetric studies on the crystallization behaviors of poly(ethylene terephthalate) (PET) and its copolymers containing isophthalate units

被引:64
作者
Lee, B
Shin, TJ
Lee, SW
Yoon, J
Kim, J
Youn, HS
Ree, M
机构
[1] Pohang Univ Sci & Technol, Dept Chem, Funct Polymer Thin Grp BK21, Ctr Integrated Mol Syst,Nam Gu, Pohang 790784, South Korea
[2] Pohang Univ Sci & Technol, Div Mol & Life Sci, Nam Gu, Pohang 790784, South Korea
[3] Pohang Univ Sci & Technol, Pohang Accelerator Lab, Nam Gu, Pohang 790784, South Korea
关键词
X-ray scattering; calorimetry; crystallization of PET and copolyesters;
D O I
10.1016/S0032-3861(03)00130-7
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
Time-resolved small-angle X-ray scattering (SAXS) measurements were carried out for PET and its copolymers undergoing isothermal crystallization. Wide-angle X-ray diffraction and differential scanning calorimetric measurements were also performed. Our data analysis of the SAXS results for PET and the copolymers clearly demonstrate that the one layer thickness l(1) (derived directly from the correlation functions of the measured SAXS profiles) is the lamellar crystal thickness d(c), not the amorphous layer thickness d(a). The observed d(c) values are found to be always smaller than d(a), regardless of polymer composition. d(c) is highly dependent on the crystallization temperature, showing that the degree of supercooling is the major factor determining the thickness of lamellar crystals. No thickening, however, occurs in isothermal crystallizations. The kinked isophthalate units in the copolymer are found to be mostly excluded from the lamellar crystals during the crystallization process, leading to an increase of the amorphous layer thickness. Moreover, the kinked, rigid nature of the isophthalate unit was found to restrict crystal growth along the chain axis of the copolymers and also to lower their crystallinity. Unlike d(c), d(a) decreases with crystallization time, causing a reduction of the long period in the lamellar stack. This drop in d(a) is interpreted in this paper by taking into account several factors that could influence crystallization behavior: the d(a) distribution in the lamellar stacks and its variation with time, the number of lamellae in the lamellar stacks and their effect on the SAXS profile, and the relaxation of polymer chains in the amorphous layers. (C) 2003 Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:2509 / 2518
页数:10
相关论文
共 50 条
[31]  
2-C
[32]   A KINETIC-ANALYSIS OF THE GAUCHE-TRANS ISOMERIZATION IN SEMICRYSTALLINE POLY(ETHYLENE-TEREPHTHALATE) [J].
LIN, SB ;
KOENIG, JL .
JOURNAL OF POLYMER SCIENCE PART B-POLYMER PHYSICS, 1983, 21 (11) :2365-2378
[33]   Influence of structural and topological constraints on the crystallization and melting behavior of polymers. 2. Poly(arylene ether ether ketone) [J].
Marand, H ;
Alizadeh, A ;
Farmer, R ;
Desai, R ;
Velikov, V .
MACROMOLECULES, 2000, 33 (09) :3392-3403
[34]   Melting behavior of high-temperature polymers [J].
MedellinRodriguez, FJ ;
Phillips, PJ ;
Lin, JS .
MACROMOLECULES, 1996, 29 (23) :7491-7501
[35]   PLS BENDING MAGNET X-RAY BEAMLINE 3C2 [J].
PARK, BJ ;
RAH, SY ;
PARK, YJ ;
LEE, KB .
REVIEW OF SCIENTIFIC INSTRUMENTS, 1995, 66 (02) :1722-1724
[37]  
Scherrer P., 1918, Phys, V2, P98
[38]   EFFECT OF DIETHYLENE GLYCOL CONTENT AND ANNEALING TEMPERATURE ON THE STRUCTURE AND PROPERTIES OF POLY(ETHYLENE-TEREPHTHALATE) [J].
SEGANOV, I ;
SCHULTZ, JM ;
FAKIROV, S .
JOURNAL OF APPLIED POLYMER SCIENCE, 1986, 32 (02) :3371-3392
[39]   RATE OF RECRYSTALLIZATION OF POLYETHYLENE SINGLE CRYSTALS [J].
STATTON, WO .
JOURNAL OF APPLIED PHYSICS, 1961, 32 (11) :2332-&
[40]   DIRECT EVALUATION OF THE ELECTRON-DENSITY CORRELATION-FUNCTION OF PARTIALLY CRYSTALLINE POLYMERS [J].
STROBL, GR ;
SCHNEIDER, M .
JOURNAL OF POLYMER SCIENCE PART B-POLYMER PHYSICS, 1980, 18 (06) :1343-1359