Separation of Iron Phase and P-Bearing Slag Phase from Gaseous-Reduced, High-Phosphorous Oolitic Iron Ore at 1473 K (1200 °C) by Super Gravity

被引:25
作者
Gao, Jintao [1 ]
Zhong, Yiwei [1 ]
Guo, Lei [1 ]
Guo, Zhancheng [1 ]
机构
[1] Univ Sci & Technol Beijing, State Key Lab Adv Met, Beijing 100083, Peoples R China
来源
METALLURGICAL AND MATERIALS TRANSACTIONS B-PROCESS METALLURGY AND MATERIALS PROCESSING SCIENCE | 2016年 / 47卷 / 02期
基金
中国国家自然科学基金;
关键词
DEPHOSPHORIZATION TREATMENT; PRE-REDUCTION; REMOVAL; MICROWAVE; HEMATITE; CAO; MECHANISM; SYSTEM; HEAT;
D O I
10.1007/s11663-015-0575-8
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In situ observation on the morphology evolution and phosphorous migration of gaseous-reduced, high-phosphorous oolitic iron ore during the melting process was carried out with a high-temperature confocal scanning laser microscope. The results showed that 1473 K (1200 degrees C) was a critical temperature at which the gangue minerals started to form into the slag phase while the iron grains remained in a solid state; in addition, the phosphorus remained in the slag phase. Since the separation of iron grains and P-bearing slag was not achieved at the low temperature under the conventional conditions, separate experiments of the iron phase and the P-bearing slag phase from gaseous-reduced, high-phosphorous oolitic iron ore at 1473 K (1200 degrees C) by super gravity were carried out in this study. Based on the iron-slag separation by super gravity, phosphorus was removed effectively from the iron phase at the temperature below the melting point of iron. Iron grains moved along the super-gravity direction, joined, and concentrated as the iron phase on the filter, whereas the slag phase containing apatite crystals broke through the barriers of the iron grains and went through the filter. Consequently, increasing the gravity coefficient was definitely beneficial for the separation of the P-bearing slag phase from the iron phase. With the gravity coefficient of G = 1200, the mass fractions of separated slag and iron phases were close to their respective theoretical values, and the mass fraction of MFe in the separated iron phase was up to 98.09 wt pct and that of P was decreased to 0.083 wt pct. The recovery of MFe in the iron phase and that of P in the slag phase were up to 99.19 and 95.83 pct, respectively. (C) The Minerals, Metals & Materials Society and ASM International 2016
引用
收藏
页码:1080 / 1092
页数:13
相关论文
共 43 条
  • [1] Catalyzing Carbothermic Reduction of Siderite Ore with High Content of Phosphorus by Adding Sodium Carbonate
    Bai, Shaojun
    Wen, Shuming
    Liu, Dianwen
    Zhang, Wenbin
    Xian, Yongjun
    [J]. ISIJ INTERNATIONAL, 2011, 51 (10) : 1601 - 1607
  • [2] Bacterial solubilization of phosphorus from phosphate rock containing sulfur-mud
    Bhatti, Tariq M.
    Yawar, Wasim
    [J]. HYDROMETALLURGY, 2010, 103 (1-4) : 54 - 59
  • [3] Dephosphorisation of Western Australian iron ore by hydrometallurgical process
    Cheng, CY
    Misra, VN
    Clough, J
    Mun, R
    [J]. MINERALS ENGINEERING, 1999, 12 (09) : 1083 - 1092
  • [4] Diversity and activity of phosphate bioleaching bacteria from a high-phosphorus iron ore
    Delvasto, P.
    Valverde, A.
    Ballester, A.
    Munoz, J. A.
    Gonzalez, F.
    Blazquez, M. L.
    Igual, J. M.
    Garcia-Balboa, C.
    [J]. HYDROMETALLURGY, 2008, 92 (3-4) : 124 - 129
  • [5] Mobilization of phosphorus from iron ore by the bacterium Burkholderia caribensis FeGL03
    Delvasto, P.
    Ballester, A.
    Munoz, J. A.
    Gonzalez, F.
    Blazquez, M. L.
    Igual, J. M.
    Valverde, A.
    Garcia-Balboa, C.
    [J]. MINERALS ENGINEERING, 2009, 22 (01) : 1 - 9
  • [6] Heat and Acid Leach Treatments to Lower Phosphorus Levels in Goethitic Iron Ores
    Fisher-White, Michael John
    Lovel, Roy Randall
    Sparrow, Graham Jeffrey
    [J]. ISIJ INTERNATIONAL, 2012, 52 (10) : 1794 - 1800
  • [7] Phosphorus Removal from Goethitic Iron Ore with a Low Temperature Heat Treatment and a Caustic Leach
    Fisher-White, Michael John
    Lovel, Roy Randall
    Sparrow, Graham Jeffrey
    [J]. ISIJ INTERNATIONAL, 2012, 52 (05) : 797 - 803
  • [8] Formation reaction of phosphate compound in multi phase flux at 1573 K
    Fukagai, Shinya
    Hamano, Tasuku
    Tsukihashi, Furnitaka
    [J]. ISIJ INTERNATIONAL, 2007, 47 (01) : 187 - 189
  • [9] Separation of P Phase and Fe Phase in High Phosphorus Oolitic Iron Ore by Ultrafine Grinding and Gaseous Reduction in a Rotary Furnace
    Gao, Jintao
    Guo, Lei
    Guo, Zhancheng
    [J]. METALLURGICAL AND MATERIALS TRANSACTIONS B-PROCESS METALLURGY AND MATERIALS PROCESSING SCIENCE, 2015, 46 (05): : 2180 - 2189
  • [10] Reagents in igneous phosphate ores flotation
    Guimaraes, RC
    Araujo, AC
    Peres, AEC
    [J]. MINERALS ENGINEERING, 2005, 18 (02) : 199 - 204