共 21 条
[1]
INTERNAL-FRICTION ASSOCIATED WITH THE ALLOTROPIC TRANSFORMATION OF COBALT
[J].
JOURNAL DE PHYSIQUE,
1985, 46 (C-10)
:601-604
[3]
Transformation sequence in severely cold-rolled and annealed Ti50Ni50 alloy
[J].
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING,
2006, 438 (SPEC. ISS.)
:509-512
[4]
Damping characteristics of cold-rolled and annealed equiatomic TiNi shape memory alloy
[J].
HIGH DAMPING MATERIALS II,
2006, 319
:9-15
[8]
FACTORS AFFECTING INTERNAL-FRICTION PEAK DUE TO THERMOELASTIC MARTENSITIC-TRANSFORMATION
[J].
SCRIPTA METALLURGICA,
1976, 10 (12)
:1125-1128
[9]
DELORME JF, 1971, J PHYSIQUE, V32, P101
[10]
Duering T.W, 1990, ENG ASPECTS SHAPE ME, P3