Wear resistance properties of austempered ductile iron

被引:35
作者
Lerner, YS [1 ]
Kingsbury, GR [1 ]
机构
[1] Univ No Iowa, Cedar Falls, IA 50614 USA
关键词
abrasion wear test; abrasive medium; austempered ductile iron; austenite; coefficient of friction; countersurface material; martensite; rotating dry sliding test; stress-affected phase transformation; wear behavior;
D O I
10.1361/105994998770348034
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
A detailed review of wear resistance properties of austempered ductile iron (ADI) was undertaken to examine the potential applications of this material for wear parts, as an alternative to steels, alloyed and white irons, bronzes, and other competitive materials. Two modes of wear were studied: adhesive (frictional) dry sliding and abrasive wear, In the rotating dry sliding tests, wear behavior of the base material (a stationary block) was considered in relationship to countersurface (steel shaft) wear, In this wear mode, the wear rate of ADI was only one-fourth that of pearlitic ductile iron (DI) grade 100-70-03; the wear rates of aluminum bronze and leaded-tin bronze, respectively, were 3.7 and 3.3 times greater than that of ADI, Only quenched DI with a fully martensitic matrix slightly outperformed ADI, No significant difference was observed in the wear of steel shafts running against ADI and quenched DI, The excellent wear performance of ADI and its countersurface, combined with their relatively low friction coefficient, indicate potential for dry sliding wear applications, In the abrasive wear mode, the wear rate of ADI was comparable to that of alloyed hardened AISI 4340 steel, and approximately one-half that of hardened medium-carbon AISI 1050 steel and of white and alloyed cast irons, The excellent wear resistance of ADI may be attributed to the strain-affected transformation of high-carbon austenite to martensite that takes place in the surface layer during the wear tests.
引用
收藏
页码:48 / 52
页数:5
相关论文
共 15 条
[1]  
American Foundrymens Society, 1992, DUCT IR HDB
[2]  
ASM International, 1992, ASM HDB, V18
[3]  
Gundlach R., 1986, P 2 INT C AUST DUCT, P23
[4]  
HAYRYNEN KL, 1995, MODERN CASTING AUG, P35
[5]  
JONES MH, 1983, IND TRIBOLOGY
[6]  
KEOUGH JR, 1995, FOUNDRY MANAGE T OCT, P28
[7]  
KEOUGH JR, 1995, FOUNDRY MANAGE T NOV, P27
[8]  
Kovacs BV, 1990, MOD CAST, V80, P38
[9]  
LAUB JR, 1994, ADV MAT PROCESS, V145, P12
[10]  
LERNER YS, 1995, J MAT ENG PERFORM, V3, P1