The effects of lithiation process on the performance of all-solid-state electrochromic devices

被引:16
|
作者
Coskun, Ozlem Duyar [1 ]
Atak, Gamze [1 ]
机构
[1] Hacettepe Univ, Dept Engn Phys, Thin Film Preparat & Characterizat Lab, TR-06800 Ankara, Turkey
关键词
All-solid-state electrochromic device; Lithiation; Optical modulation; Magnetron sputtering; NICKEL-OXIDE; THIN-FILMS; WO3; ELECTROLYTE;
D O I
10.1016/j.tsf.2018.07.019
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
All solid-state electrochromic devices were fabricated using radio-frequency magnetron sputtering. The electrochromic layers employed in the all solid-state device were subjected to lithiation insertion to improve performance of the device. Two structures, one with dry, and one with both wet and dry lithiation processes were used for intercalation of lithium atoms into the electrochromic layers. The main device configuration was as follows: indium fin oxide (ITO)/NiO/Ta2O5/dry lithiated WO3/ITO/glass. Dry lithiation was performed by exposing the WO3 layer in vacuum to Li vapor atoms obtained by radio-frequency (RF) magnetron sputtering of LiNbO3 at room temperature. An additional, wet lithiation, step was performed on one structure by electrochemical cycling in a solution containing lithium ions, leading to Li+ insertion into the Ta2O5 layer used as an ion-conducting layer. The optical modulation of the device containing only dry lithiated WO3 was found to be 34.8% at 550 nm for applied potentials of +/- 4 V. With wet lithiation additionally applied to the ion-conducting layer (Ta2O5), the optical modulation of the device increased to 71.7% at 550 nm for applied potentials of +/- 4 V.
引用
收藏
页码:13 / 20
页数:8
相关论文
共 50 条
  • [1] All-solid-state electrochromic devices: Fabrication process and technology
    Huang, S.Y.
    Qu, F.Q.
    Miao, Y.
    Meng, Z.K.
    Zhenkong Kexue yu Jishu Xuebao/Vacuum Science and Technology, 2001, 21 (02): : 170 - 172
  • [2] Study on the WO3 dry lithiation for all-solid-state electrochromic devices
    Ye, YH
    Zhang, JY
    Gu, PF
    Tang, JF
    SOLAR ENERGY MATERIALS AND SOLAR CELLS, 1997, 46 (04) : 349 - 355
  • [3] Lithiation of WO3 films by evaporation method for all-solid-state electrochromic devices
    Li, Wenjie
    Zhang, Xiang
    Chen, Xi
    Zhao, Yingming
    Wang, Lebin
    Chen, Mingjun
    Li, Zitong
    Zhao, Jiupeng
    Li, Yao
    ELECTROCHIMICA ACTA, 2020, 355
  • [4] Optical properties of electrochromic all-solid-state devices
    Larsson, AL
    Niklasson, GA
    SOLAR ENERGY MATERIALS AND SOLAR CELLS, 2004, 84 (1-4) : 351 - 360
  • [5] Strong coloration of nanoporous tungsten oxides by in-vacuo lithiation for all-solid-state electrochromic devices
    Bouvard, Olivia
    Lagier, Maxime
    Burnier, Luc
    Krammer, Anna
    Schueler, Andreas
    THIN SOLID FILMS, 2021, 730
  • [6] Annealing effects of NiO thin films for all-solid-state electrochromic devices
    Atak, Gamze
    Coskun, Ozlem Duyar
    SOLID STATE IONICS, 2017, 305 : 43 - 51
  • [7] All-solid-state electrochromic devices on glass and flexible substrate
    Nah, YC
    Ahn, KS
    Park, JY
    Shim, HS
    Park, NH
    Sung, YE
    ELECTROCHROMIC MATERIALS AND APPLICATIONS, 2003, 2003 (17): : 243 - 253
  • [8] Advances in Inorganic All-solid-state Electrochromic Materials and Devices
    Jia Hanxiang
    Cao Xun
    Jin Pingshi
    JOURNAL OF INORGANIC MATERIALS, 2020, 35 (05) : 511 - 524
  • [9] Long life all-solid-state electrochromic devices by annealing
    Li, Wenjie
    Zhang, Xiang
    Chen, Xi
    Zhao, Yingming
    Sun, Wenhai
    Xiao, Yingjun
    Li, Senran
    Zhao, Jiupeng
    Li, Yao
    SOLAR ENERGY MATERIALS AND SOLAR CELLS, 2021, 224
  • [10] Extraordinarily fast response all-solid-state electrochromic devices
    Song, Kunrun
    Cao, Zhenhu
    Weng, Shichen
    Chen, Wentao
    Jiang, Ran
    Rogachev, Alexandr Alexandrovich
    Yarmolenko, Maxim Anatolievich
    Zhou, Jumei
    Zhang, Hongliang
    SOLAR ENERGY MATERIALS AND SOLAR CELLS, 2024, 278