Vitrification of chromium electroplating sludge

被引:90
作者
Li, Chun-Teh
Lee, Wen-Jhy
Huang, Kuo-Lin [1 ]
Fu, Sheng-Feng
Lai, Yi-Chieh
机构
[1] Natl Cheng Kung Univ, Dept Environm Engn, Tainan 70101, Taiwan
[2] Natl Pingtung Univ Sci & Technol, Dept Environm Engn & Sci, Neipu 91201, Pingtung, Taiwan
[3] Natl Cheng Kung Univ, Sustainable Environm Res Ctr, Tainan 70101, Taiwan
关键词
FLY-ASH; MUNICIPAL; INDUSTRIAL; RECOVERY; METAL;
D O I
10.1021/es062803d
中图分类号
X [环境科学、安全科学];
学科分类号
08 ; 0830 ;
摘要
This work investigated the vitrification of hazardous electroplating sludge containing 140 mg/g Cr with/without bottom ash or cullet conditioning to lower specimens' basicities to 0.97-1.17 or 0.18-0.23, respectively. The conditioning was found to enhance the smooth/glassy appearance of slags but no ingot was obtained. Cr was > 98% retained in the vitrified slags. Cr2O3 dominated in crystalline structure for the slag vitrified from the sludge, but this domination gradually shifted to Fe2SiO4/Fe3O4/SiO2 or SiO2 crystalline with increasing addition of bottom ash or cullet into the sludge, respectively. Compared to the raw sludge, the sludge-vitrified slag displayed lower leaching concentrations for most metals (particularly Cr (2.54 mg/ L)), and smaller leaching ratios for Ag, Cr, and Cu (1.35, 0.02, and < 0.01%, respectively) but greater ones for Cd, Pb, and Zn (3.83, 2.46, and 0.36%, respectively). The Cr leaching ratios were similar to 0.01% for the slags vitrified from the conditioned sludge. Independent of the slag basicity and crystalline structure, metal leaching quantity increased but leaching ratio decreased with increasing slag metal content. The slag compressive strengths were improved to > 14.7 MPa at the mixing ratios >= 2/1 and 1/1 for bottom ash/sludge and cullet/sludge, respectively. Fulfilling the criteria of Toxicity Characteristic Leaching Procedure (TCLP), all the slags were recyclable.
引用
收藏
页码:2950 / 2956
页数:7
相关论文
共 21 条
[1]  
[Anonymous], 1992, USEPA. "Environmental regulations and technology: Control of pathogens and vector attraction in sewage sludge." (1992).
[2]   Solidification of electroplating sludge using alkali-activated pulverized fuel ash as cementitious binder [J].
Asavapisit, S ;
Chotklang, D .
CEMENT AND CONCRETE RESEARCH, 2004, 34 (02) :349-353
[3]   Alkaline and alkaline-earth silicate glasses and glass-ceramics from municipal and industrial wastes [J].
Barbieri, L ;
Bonamartini, AC ;
Lancellotti, I .
JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2000, 20 (14-15) :2477-2483
[4]   Chloride influence on the incorporation of Cr2O3 and NiO in clinker:: a laboratory evaluation [J].
Barros, AM ;
Tenório, JAS ;
Espinosa, DCR .
JOURNAL OF HAZARDOUS MATERIALS, 2002, 93 (02) :221-232
[5]  
*CNS, 619R3013 CNS
[6]   Effect of electric arc vitrification of bottom ash on the mobility and fate of metals [J].
Ecke, H ;
Sakanakura, H ;
Matsuto, T ;
Tanaka, N ;
Lagerkvist, A .
ENVIRONMENTAL SCIENCE & TECHNOLOGY, 2001, 35 (07) :1531-1536
[7]   Thermal behavior of chromium electroplating sludge [J].
Espinosa, DCR ;
Tenório, JAS .
WASTE MANAGEMENT, 2001, 21 (04) :405-410
[8]   Laboratory study of galvanic sludge's influence on the clinkerization process [J].
Espinosa, DCR ;
Tenório, JAS .
RESOURCES CONSERVATION AND RECYCLING, 2000, 31 (01) :71-82
[9]   Environmental properties of vitrified fly ash from hazardous and municipal waste incineration [J].
Haugsten, KE ;
Gustavson, B .
WASTE MANAGEMENT, 2000, 20 (2-3) :167-176
[10]   ASME/US Bureau of Mines investigative program on vitrification of combustion ash residue: Findings and conclusions [J].
Hollander, HI ;
Plumley, AL ;
DeCesare, RS .
JOURNAL OF HAZARDOUS MATERIALS, 1996, 47 (1-3) :369-381