Hydrogen diffusivity and tensile-ductility loss of solution-treated austenitic stainless steels with external and internal hydrogen

被引:106
作者
Yamabe, Junichiro [1 ,2 ,3 ]
Takakuwa, Osamu [2 ]
Matsunaga, Hisao [2 ,3 ,4 ]
Itoga, Hisatake [2 ,5 ]
Matsuoka, Saburo [2 ]
机构
[1] Kyushu Univ, Int Res Ctr Hydrogen Energy, Nishi Ku, 744 Moto Oka, Fukuoka, Fukuoka 8190395, Japan
[2] Kyushu Univ, Res Ctr Hydrogen Ind Use & Storage HYDROGENIUS, Nishi Ku, 744 Moto Oka, Fukuoka, Fukuoka 8190395, Japan
[3] Kyushu Univ, Int Inst Carbon Neutral Energy Res WPI I2CNER, Nishi Ku, 744 Moto Oka, Fukuoka, Fukuoka 8190395, Japan
[4] Kyushu Univ, Dept Mech Engn, Nishi Ku, 744 Moto Oka, Fukuoka, Fukuoka 8190395, Japan
[5] Hydrogen Energy Test & Res Ctr HyTReC, 915-1 Tomi, Itoshima, Fukuoka 8191133, Japan
关键词
Hydrogen embrittlement; Slow-strain-rate tensile test; Austenitic stainless steel; Nickel equivalent; Additive element; ENVIRONMENT EMBRITTLEMENT; FRACTURE; COMPATIBILITY; TRANSPORT; BEHAVIOR;
D O I
10.1016/j.ijhydene.2017.04.055
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The effects of external and internal hydrogen on the slow-strain-rate tensile (SSRT) properties at room temperature were studied for ten types of solution-treated austenitic stainless steels containing a small amount of additive elements. The hydrogen diffusivity and solubility of the steels were measured with high-pressure hydrogen gas. The remarkable tensile-ductility loss observed in the SSRT tests was attributed to hydrogen induced successive crack growth (HISCG) and was successfully quantified according to the nickel-equivalent content (Ni-eq), which represents the stability of the austenitic phase. The relative reduction in area (RRA) of the steels with a larger Ni-eq was influenced by the hydrogen distribution, whereas that of the steels with a smaller Ni-eq was not. This unique trend was interpreted with regard to the hydrogen distribution and fracture morphology (HISCG or microvoid coalescence). (C) 2017 Hydrogen Energy Publications LLC. Published by Elsevier Ltd. All rights reserved.
引用
收藏
页码:13289 / 13299
页数:11
相关论文
共 37 条
  • [1] [Anonymous], 1997, 174016 NASA NSS
  • [2] [Anonymous], 2011, G14298 ASTM INT
  • [3] [Anonymous], 2011, G14897 ASTM INT
  • [4] Chandler WT, 1975, P HYDROGEN EC MIAMI, P1057
  • [5] INVESTIGATION OF PLASTIC FRACTURE OF ALSL-4340 AND 18 NICKEL-200 GRAE MARAGING STEELS
    COX, TB
    LOW, JR
    [J]. METALLURGICAL TRANSACTIONS, 1974, 5 (06): : 1457 - 1470
  • [6] DIFFUSION OF HYDROGEN IN MILD STEEL
    DEMAREZ, A
    HOCK, AG
    MEUNIER, FA
    [J]. ACTA METALLURGICA, 1954, 2 (02): : 214 - 223
  • [7] Effect of temperature on hydrogen environment embrittlement of type 316 series austenitic stainless seels at low temperatures
    Fukuyama, S
    Sun, DS
    Zhang, L
    Wen, M
    Yokogawa, K
    [J]. JOURNAL OF THE JAPAN INSTITUTE OF METALS, 2003, 67 (09) : 456 - 459
  • [8] Effect of strain-induced martensite on hydrogen environment embrittlement of sensitized austenitic stainless steels at low temperatures
    Han, G
    He, J
    Fukuyama, S
    Yokogawa, K
    [J]. ACTA MATERIALIA, 1998, 46 (13) : 4559 - 4570
  • [9] Hirayama T., 1970, J. Jpn. Inst. Met., V34, P507, DOI [10.2320/jinstmet1952.34.5_507, DOI 10.2320/JINSTMET1952.34.5_507]
  • [10] Itoga H, 2014, P PVP 2014 ASME PRES