Compressive behaviour of open cell Al-Al2O3 composite foams fabricated by sintering and dissolution process

被引:12
|
作者
Yang, Y. J. [1 ]
Han, F. S. [1 ]
Yang, D. K. [1 ]
Zheng, K. [1 ]
机构
[1] Chinese Acad Sci, Inst Solid State Phys, Key Lab Mat Phys, Hefei 230031, Anhui, Peoples R China
关键词
Al foam; Al-Al2O3; composite; mechanical properties; sintering;
D O I
10.1179/174328407X161114
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The sintering and dissolution process (SDP) was used to produce the fine open cell Al-Al2O3 composite and pure Al foams with the relative density of 0.25-0-40 and the pore size of 112-400 mu m. The composite foam exhibited much higher yield strength and Young's modulus than the pure Al foam, and thus had an elevated plateau stress. Moreover, the composite foam showed a unique dependence of the compression stress on the pore size, i.e. it increased with increasing pore size, which was quite different from that for the common metal foams.