Critical design parameters of the electrode for liquid metal embrittlement cracking in resistance spot welding

被引:39
作者
Murugan, Siva Prasad [1 ]
Mahmud, Kaisar [1 ]
Ji, Changwook [2 ]
Jo, Ilguk [1 ]
Park, Yeong-Do [1 ]
机构
[1] Dong Eui Univ, Dept Adv Mat Engn, 176 Eomgwangno, Busan 614714, South Korea
[2] Korea Inst Ind Technol, Adv Forming Proc R&D Grp, Ulsan 44413, South Korea
关键词
Liquid metal embrittlement; Resistance spot welding; Welding electrode; Dome type; Radius type; Current density; GEOMETRY;
D O I
10.1007/s40194-019-00797-y
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The present work studied the influence of the geometric design of the electrode on Zn-assisted liquid metal embrittlement (LME) cracking during resistance spot welding (RSW). LME cracking of the galvannealed transformation-induced plasticity (TRIP) steel welds, induced by two types of electrodes, a radius type with different radius of curvature (R), and a dome type with variable tip diameter (d), was studied both experimentally and by simulation. The current density decreased and the contact area at the electrode/sheet (E/S) interface increased with the increasing R, resulting in low temperatures and thermal stress, which subsequently led to decreased LME tendency. On the contrary, the current density decreased but the initial contact area at the E/S interface remained unchanged with increasing d, causing only a minor reduction in the temperature and hence less influence on LME cracking. These results suggested that R is the most critical design parameter of the electrode that controls LME cracking. Moreover, the radius type electrode displayed lower LME sensitivity as compared with the dome type electrode. This is attributed to the fact that the radius type electrode provides the benefits of increase in both R and d.
引用
收藏
页码:1613 / 1632
页数:20
相关论文
共 35 条
[1]  
Aa EMVanDer, 2017, STEELS CARS TRUCK C
[2]  
American Welding Society, 2012, AWS D8.9M:2012
[3]  
[Anonymous], 2003, RES WELD MAN
[4]   Liquid metal embrittlement-free welds of Zn-coated twinning induced plasticity steels [J].
Ashiri, Rouholah ;
Shamanian, Morteza ;
Salimijazi, Hamid Reza ;
Haque, Md Anwarul ;
Bae, Jin-Hee ;
Ji, Chang-Wook ;
Chin, Kwang-Geun ;
Park, Yeong-Do .
SCRIPTA MATERIALIA, 2016, 114 :41-47
[5]   Supercritical area and critical nugget diameter for liquid metal embrittlement of Zn-coated twining induced plasticity steels [J].
Ashiri, Rouholah ;
Hague, Md Anwarul ;
Ji, Chang-Wook ;
Shamanian, Morteza ;
Salimijazi, Hamid Reza ;
Park, Yeong-Do .
SCRIPTA MATERIALIA, 2015, 109 :6-10
[6]   Liquid Metal Embrittlement in Resistance Spot Welding and Hot Tensile Tests of Surface-refined TWIP Steels [J].
Barthelmie, J. ;
Schram, A. ;
Wesling, V. .
18TH CHEMNITZ SEMINAR ON MATERIALS ENGINEERING, 2016, 118
[7]   Liquid metal embrittlement during resistance spot welding of Zn-coated high-strength steels [J].
Bhattacharya, Diptak .
MATERIALS SCIENCE AND TECHNOLOGY, 2018, 34 (15) :1809-1829
[8]  
BOWERS RJ, 1990, WELD J, V69, pS45
[9]   Experimental and Numerical Analysis of Liquid Metal Embrittlement Crack Location [J].
DiGiovanni, C. ;
Han, X. ;
Powell, A. ;
Biro, E. ;
Zhou, N. Y. .
JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2019, 28 (04) :2045-2052
[10]   Impact of liquid metal embrittlement cracks on resistance spot weld static strength [J].
DiGiovanni, Christopher ;
Biro, Elliot ;
Zhou, Norman Y. .
SCIENCE AND TECHNOLOGY OF WELDING AND JOINING, 2019, 24 (03) :218-224