Fracture Control of the 2nd West to East Gas Pipeline in China

被引:5
作者
Feng, Yaorong [1 ]
Huo, Chunyong [1 ]
Zhuang, Chuanjing [1 ]
Ji, Lingkang [1 ]
Li, Yang [1 ]
Li, Helin [1 ]
机构
[1] CNPC Tubular Goods Res Inst, State Key Lab Performance & Struct Safety Petr Tu, Xian 710077, Shaanxi, Peoples R China
来源
FIRST INTERNATIONAL SYMPOSIUM ON RISK ANALYSIS AND SAFETY OF COMPLEX STRUCTURES AND COMPONENTS (IRAS 2019) | 2019年 / 22卷
关键词
fracture control; crack initiation; crack arrest toughness; full-scale burst test; X80 steel pipe; gas pipeline;
D O I
10.1016/j.prostr.2020.01.028
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The 2nd West to East Gas Pipeline ( WEGP) is the first major pipeline project in China importing abroad natural gas and also the longest and largest gas transmission pipeline in the world with gas supply of Middle Asian natural gas and adjusting gas supply of domestic gas from Tarim Basin and Ordos Basin. Its total length is 9 000 kilometers, in which the total length of artery from Khorgos to Guangzhou is 4 900 kilometers. Its design throughput is 30 billion cubic meters per year. Designed maximum operation pressure is 12 MPa, largest diameter of pipe is 1219mm and highest steel grade is X80. To ensure the long-term safety and reliability in operation, fracture control program has been proposed through systematic research, including crack initiation control, brittle fracture control and ductile long -running fracture control. The requirement of arrest toughness of the 2nd WEGP had been studied on the basis of pipe full-scale burst test data base in the world, Battelle Two Curve (BTC) method and GasDecom software. Fullscale burst tests of X80 high-pressure gas pipeline had been successfully performed based on previous research results. The fracture control program was set up based on different fracture criteria and the principle of both safety and economy. The crack arrest ability of X80 spiral submerged arc welded (SSAW) steel pipe was firstly verified and a new correct factor of arrest toughness prediction was obtained. Results presented that the crack arrest ability of SSAW pipe is better than longitudinal submerged arc welded (LSAW) pipe. It lays a solid foundation for the safe operation of the X80 pipeline after construction and completion. 2019 The Authors. Published by Elsevier B.V. This is an open access article under the CC BY-NC-ND license (http:hicreativecommons.orgilicenses/b:,, -ne-nd/4.0/) Peer-review under responsibility of the First International Symposium on Risk and Safety of Complex Structures and Components organizers
引用
收藏
页码:219 / 228
页数:10
相关论文
共 20 条
[1]  
Bonomo F, 1980, PIPELINE ENERGY PLAN, P337
[2]  
Eiber R J, 1974, MECH WORK STEEL PROC, VIII, P353
[3]   FRACTURE CONTROL TESTING AND ACCEPTANCE CRITERIA FOR LINE PIPE [J].
HANSEN, DA .
JOURNAL OF PETROLEUM TECHNOLOGY, 1981, 33 (03) :527-534
[4]   PREDICTION OF LINEPIPE FRACTURE-BEHAVIOR FROM LABORATORY TESTS [J].
HOLMES, B ;
PRIEST, AH ;
WALKER, EF .
INTERNATIONAL JOURNAL OF PRESSURE VESSELS AND PIPING, 1983, 12 (01) :1-27
[5]  
Jones B L, 1984, P CENT C, P282
[6]  
Kanninen M., 1992, JOINT FINAL REPORT D
[7]  
KOCH FO, 1986, OIL GAS J, V84, P110
[8]  
Leis Brian N, INT PIP C, V2, P723
[9]  
Lin Xuemei, 1998, OIL COUNTRY TUBULAR, V6, P27
[10]  
Maxey W A, P 1971 NAT S FRACT 2, P71