Brazing of Inconel 600 by active filler metal

被引:2
作者
Zaharinie, T. [1 ,2 ]
Yusof, F. [1 ,2 ]
Hamdi, M. [1 ,2 ]
Ariga, T. [3 ]
机构
[1] Univ Malaya, Dept Mech Engn, Kuala Lumpur, Malaysia
[2] Univ Malaya, AMMP Ctr, Kuala Lumpur, Malaysia
[3] Tokai Univ, Sch Engn, Dept Mat Sci, Hiratsuka, Kanagawa 25912, Japan
关键词
Brazing; Inconel; 600; Active filler metal; Ag-Cu-Ti; Reaction layer; Shear strength; STAINLESS-STEEL; MECHANICAL-PROPERTIES; TEMPERATURE; ALLOY; MICROSTRUCTURE;
D O I
10.1179/1432891714Z.000000000968
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Inconel 600 alloy was brazed at three different brazing temperatures 830, 865 and 900 degrees C for 30 minutes. An active filler metal, Ag-Cu-Ti, was utilised to study its effects on bonding strength by the diffusion of some elements with Inconel 600 during brazing. The experiment was carried out in a high vacuum chamber at 1 x 10(-4) Pa. Scanning electron microscope-energy dispersive spectroscopy and electron probe microanalysis was conducted for element identification and a shear test served to evaluate the bonding strength. The results show that good bonding was achieved and two continuous reaction layers were formed in the brazed area. The reaction layers were crossing in the middle in most areas at 865 degrees C compared to 830 and 900 degrees C. It was revealed that a stronger Ti-Ni interaction than Ti-Cu influenced the formation behaviour of reaction layers and the highest shear strength identified was at 865 degrees C.
引用
收藏
页码:260 / 263
页数:4
相关论文
共 16 条
[1]   Details on the formation of Ti2Cu3 in the Ag-Cu-Ti system in the temperature range 790 to 860°C [J].
Andrieux, J. ;
Dezellus, O. ;
Bosselet, F. ;
Sacerdote-Peronnet, M. ;
Sigala, C. ;
Chiriac, R. ;
Viala, J. C. .
JOURNAL OF PHASE EQUILIBRIA AND DIFFUSION, 2008, 29 (02) :156-162
[2]   Transient liquid phase bonding of Inconel 718 and Inconel 625 with BNi-2: Modeling and experimental investigations [J].
Arafin, M. A. ;
Medraj, M. ;
Turner, D. P. ;
Bocher, P. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2007, 447 (1-2) :125-133
[3]  
Belohlav A., STRENGTH DATA BAG 1
[4]   Brazing silicon nitride to an iron-based intermetallic using a copper interlayer [J].
Brochu, M ;
Pugh, MD ;
Drew, RAL .
CERAMICS INTERNATIONAL, 2004, 30 (06) :901-910
[5]   THE METALLURGICAL BEHAVIOR DURING BRAZING OF NI-BASE ALLOY INCONEL-600 TO SI3N4 WITH AG71CU27TI2 FILLER METAL [J].
CHEN, JH ;
WANG, GZ ;
NOGI, K ;
KAMAI, M ;
SATO, N ;
IWAMOTO, N .
JOURNAL OF MATERIALS SCIENCE, 1993, 28 (11) :2933-2942
[6]   Joining of superalloy Inconel 600 by diffusion induced isothermal solidification of a liquated insert metal [J].
Egbewande, A. T. ;
Chukwukaeme, C. ;
Ojo, O. A. .
MATERIALS CHARACTERIZATION, 2008, 59 (08) :1051-1058
[7]   Correlation between microstructure, mechanical properties, and brazing temperature of steel to titanium joint [J].
Elrefaey, Ahmed ;
Tillmann, Wolfgang .
JOURNAL OF ALLOYS AND COMPOUNDS, 2009, 487 (1-2) :639-645
[8]   Comparison of Inconel 625 and Inconel 600 in resistance to cavitation erosion and jet impingement erosion [J].
Hu, H. X. ;
Zheng, Y. G. ;
Qin, C. P. .
NUCLEAR ENGINEERING AND DESIGN, 2010, 240 (10) :2721-2730
[9]  
Huda Z., 2011, INT J PHYS SCI, V30, P7073, DOI 10.5897/UPS11.245
[10]   Evaluation of surface integrity in micro drilling process for nickel-based superalloy [J].
Imran, Muhammad ;
Mativenga, Paul T. ;
Gholinia, Ali ;
Withers, Philip J. .
INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2011, 55 (5-8) :465-476