Effect of Li addition on the plastic deformation behaviour of AZ31 magnesium alloy

被引:9
作者
Bajargan, Govind [1 ,2 ]
Singh, Gaurav [2 ]
Ramamurty, U. [2 ,3 ]
机构
[1] Vikram Sarabhai Space Ctr, Foundry Technol Div, Trivandrum 695022, Kerala, India
[2] Indian Inst Sci, Dept Mat, Bangalore 560012, Karnataka, India
[3] King Abdulaziz Univ, Ctr Excellence Adv Mat Res, Jeddah 21589, Saudi Arabia
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2016年 / 662卷
关键词
Mg alloys; Li addition; Twinning; Dynamic recrystallization; Dynamic recovery; Slip system; Work hardening; HIGH-TEMPERATURE DEFORMATION; DYNAMIC RECRYSTALLIZATION; NONBASAL SLIP; HEXAGONAL SYMMETRY; TENSILE PROPERTIES; TEXTURE EVOLUTION; PRISMATIC GLIDE; GRAIN-SIZE; CROSS-SLIP; IN-SITU;
D O I
10.1016/j.msea.2016.03.087
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The enhancement in the workability, if any, of a dilute Mg alloy, AZ31, with the Li addition is investigated by examining the hot deformation behaviour of AZ31 alloyed with 1, 3 and 5 wt% Li. Compression tests were conducted in the temperature, T, range of 150-400 degrees C and strain rates, (epsilon) over dot, ranging from 10(-3) to 10(+2) s(-1). Experimental results show that the deformation behaviour can be divided into three T regimes. In the low T regime (150-200 degrees C), an increase in the Li content in AZ31 decreases the twin density with a concomitant enhancement in the non-basal or cross-slip activity. While high Li alloys exhibit low flow stress at low (epsilon) over dot in this regime, an increase in (epsilon) over dot increases strain hardening rate and twinning activity. Flow localization and shear band formation were observed in most of the alloys in this regime. Deformation in the intermediate T regime (250-300 degrees C) leads to dynamic recovery (DRY) at low (epsilon) over dot and dynamic re-crystallization (DRX) at high (epsilon) over dot, which are the softening mechanisms in Li containing alloys. In high T regime (350-400 degrees C), these alloys exhibit softening mechanisms similar to intermediate T regime but high Li alloys surprisingly exhibit higher flow stresses, which is attributed to the higher amount of Li in the solid solution, a result of the dissolution of Li containing precipitates. Non-basal slip and twinning at high (epsilon) over dot occur uniformly with homogeneous DRX. A low activation energy for deformation of high Li alloys indicates that the Friedel-Escaig (F-E) mechanism as the rate controlling deformation mechanism. The onset of twinning was examined by the appearance of first local maxima before peak strain in (d(2)sigma/d epsilon(2)) vs. epsilon curves. Mechanisms responsible for the dependence of critical stress for the onset of DRX on T and (epsilon) over dot are also discussed. (C) 2016 Elsevier B.V. All rights reserved.
引用
收藏
页码:492 / 505
页数:14
相关论文
共 62 条
[1]   Plastic anisotropy and the role of non-basal slip in magnesium alloy AZ31B [J].
Agnew, SR ;
Duygulu, Ö .
INTERNATIONAL JOURNAL OF PLASTICITY, 2005, 21 (06) :1161-1193
[2]   Study of slip mechanisms in a magnesium alloy by neutron diffraction and modeling [J].
Agnew, SR ;
Tomé, CN ;
Brown, DW ;
Holden, TM ;
Vogel, SC .
SCRIPTA MATERIALIA, 2003, 48 (08) :1003-1008
[3]   Application of texture simulation to understanding mechanical behavior of Mg and solid solution alloys containing Li or Y [J].
Agnew, SR ;
Yoo, MH ;
Tomé, CN .
ACTA MATERIALIA, 2001, 49 (20) :4277-4289
[4]  
Agnew SR, 2002, METALL MATER TRANS A, V33, P851, DOI 10.1007/s11661-002-1017-1
[5]  
Ahmadieh A., 1965, T MET SOC AIME, V233
[6]   SOLID SOLUTION STRENGTHENING OF MAGNESIUM SINGLE CRYSTALS .2. EFFECT OF SOLUTE ON EASE OF PRISMATIC SLIP [J].
AKHTAR, A ;
TEGHTSOONIAN, E .
ACTA METALLURGICA, 1969, 17 (11) :1351-+
[7]   Comparative study of the deformation behavior of hexagonal magnesium-lithium alloys and a conventional magnesium AZ31 alloy [J].
Al-Samman, T. .
ACTA MATERIALIA, 2009, 57 (07) :2229-2242
[8]  
Aldinger F, 1979, BERYLLIUM SCI TECHNO, V1, P7
[9]   Non-basal slip in magnesium-lithium alloy single crystals [J].
Ando, S ;
Tonda, H .
MATERIALS TRANSACTIONS JIM, 2000, 41 (09) :1188-1191
[10]  
Avedesian MM., 1999, ASM Specialty Handbook: Magnesium and Magnesium Alloys