Joining of Cf/SiC composites and Si3N4 ceramic with Y2O3-Al2O3-SiO2 glass filler for high-temperature applications

被引:13
|
作者
Sun, Liangbo [1 ]
Shi, Xiaosong [1 ,2 ]
Liu, Xinyu [1 ]
Fang, Jian [1 ]
Liu, Chunfeng [1 ,3 ]
Zhang, Jie [1 ,3 ]
机构
[1] Harbin Inst Technol, Sch Mat Sci & Engn, Harbin 150001, Peoples R China
[2] China Petr Pipeline Res Inst CO LTD, Langfang 065000, Peoples R China
[3] Harbin Inst Technol, Ctr Anal & Measurement, Harbin 150001, Peoples R China
基金
中国国家自然科学基金;
关键词
Cf; SiC composites; Joining; Thermal shock resistance; Glass; THERMAL-SHOCK RESISTANCE; SILICON-NITRIDE; CARBON/CARBON COMPOSITES; MECHANICAL-PROPERTIES; STRUCTURAL EVOLUTION; C/SIC COMPOSITES; BOND STRENGTH; MICROSTRUCTURE; JOINTS; ADHESIVE;
D O I
10.1016/j.ceramint.2021.02.132
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Cf/SiC composites and Si3N4 ceramics are candidate materials for applications in thermal protection system. This paper investigated the joining of Cf/SiC and Si3N4 using Y2O3?Al2O3?SiO2 glass. The reliability of joints was evaluated by thermal shock tests. In this present work, the typical joint structure was Cf/SiC-glass-Si3N4. The results demonstrate that Direct bonding has been identified as the interfacial bonding mechanism at the SiC/glass and glass/Si3N4 interfaces. The maximum shear strength of the Cf/SiC?Si3N4 joint was -34 MPa, which delivered an effective method to achieve strong, reliable bonding between the dissimilar materials. In addition, after thermal shock for 10 cycles, the residual strength remained -13 MPa. Bubbles instead of microcracks formed in the glass filler, which was the main factor causing the degradation of the joint performance. It is suggested that improving the high temperature resistance of joining materials is the key to realize the application of this joint structure.
引用
收藏
页码:15622 / 15630
页数:9
相关论文
共 50 条
  • [31] DEPENDENCE OF GLASS-FORMING ABILITY ON STARTING COMPOSITIONS IN Y2O3-Al2O3-SiO2 SYSTEM
    Wu, Liang
    Liu, Guanghua
    Li, Jiangtao
    He, Bin
    Yang, Zengchao
    Chen, Yixiang
    CERAMICS-SILIKATY, 2011, 55 (03) : 228 - 231
  • [32] Adhesion of Y2O3-Al2O3-SiO2 coatings to typical aerospace substrates
    Marraco-Borderas, Cinta
    Nistal, Andres
    Garcia, Eugenio
    Antonia Sainz, Maria
    Martin de la Escalera, Federico
    Essa, Yasser
    Miranzo, Pilar
    BOLETIN DE LA SOCIEDAD ESPANOLA DE CERAMICA Y VIDRIO, 2016, 55 (04): : 127 - 135
  • [33] High-temperature ablation performance of Si3N4-Si2N2O-BN composites prepared using selective laser sintering
    Wang, Kejie
    Yang, Guanjun
    Liu, Rongzhen
    CORROSION SCIENCE, 2022, 204
  • [34] Crystallization, thermal expansion and hardness of Y2O3-Al2O3-SiO2 glasses
    Wang, Mitang
    Zheng, Qingshuang
    Chen, Aiying
    Li, Ying
    Zhang, Xiaowei
    Zhang, Dongliang
    Jin, Siqingaowa
    Xiong, Dehua
    Deng, Wei
    CERAMICS INTERNATIONAL, 2021, 47 (17) : 25059 - 25066
  • [35] The decisive role played by graphene nanoplatelets on improving the tribological performance of Y2O3-Al2O3-SiO2 glass coatings
    Gomez-Gomez, Alberto
    Nistal, Andres
    Garcia, Eugenio
    Isabel Osendi, M.
    Belmonte, Manuel
    Miranzo, Pilar
    MATERIALS & DESIGN, 2016, 112 : 449 - 455
  • [36] FABRICATION AND PROPERTIES OF Si3N4/BN COMPOSITE CERAMICS BY PRESSURELESS SINTERING WITH Yb2O3-Al2O3-Y2O3 AS SINTERING ADDITIVES
    Li, Yongfeng
    Liu, Ping
    Qiao, Guanjun
    Yang, Jianfeng
    Jin, Haiyun
    Wang, Xiangdong
    Zhang, Guojun
    CERAMIC MATERIALS AND COMPONENTS FOR ENERGY AND ENVIRONMENTAL APPLICATIONS, 2010, 210 : 291 - +
  • [37] Fabrication and Properties of Pressureless Sintered Si3N4/BN Composite Ceramics with La2O3-Al2O3-Y2O3 as Sintering Additives
    Li, Yongfeng
    Liu, Ping
    Qiao, Guanjun
    Yang, Jianfeng
    Jin, Haiyun
    Wang, Xiangdong
    ECO-MATERIALS PROCESSING AND DESIGN X, 2009, 620-622 : 761 - +
  • [38] CaO-SiO2-Al2O3-Y2O3 glasses as model grain boundary phases for Si3N4 ceramics
    Lichvar, Peter
    Sajgalik, Pavol
    Liska, Marek
    Galusek, Dusan
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2007, 27 (01) : 429 - 436
  • [39] Investigation on Crystallization Behavior of Y2O3-Al2O3-SiO2 Glass Prepared by High-gravity Combustion Synthesis
    Yang Zeng-Chao
    Liu Guang-Hua
    Xu Li-Hua
    Li Jiang-Tao
    Guo Shi-Bin
    JOURNAL OF INORGANIC MATERIALS, 2013, 28 (07) : 780 - 784
  • [40] Si3N4/BN Composite Ceramics with Nd2O3-Al2O3-Y2O3 Ternary Additives by Pressureless Sintering
    Liu, Ping
    Li, Yongfeng
    Wang, Xiangdong
    Jin, Haiyun
    Qiao, Guanjun
    HIGH-PERFORMANCE CERAMICS VI, 2010, 434-435 : 106 - +