Joining of Cf/SiC composites and Si3N4 ceramic with Y2O3-Al2O3-SiO2 glass filler for high-temperature applications

被引:13
|
作者
Sun, Liangbo [1 ]
Shi, Xiaosong [1 ,2 ]
Liu, Xinyu [1 ]
Fang, Jian [1 ]
Liu, Chunfeng [1 ,3 ]
Zhang, Jie [1 ,3 ]
机构
[1] Harbin Inst Technol, Sch Mat Sci & Engn, Harbin 150001, Peoples R China
[2] China Petr Pipeline Res Inst CO LTD, Langfang 065000, Peoples R China
[3] Harbin Inst Technol, Ctr Anal & Measurement, Harbin 150001, Peoples R China
基金
中国国家自然科学基金;
关键词
Cf; SiC composites; Joining; Thermal shock resistance; Glass; THERMAL-SHOCK RESISTANCE; SILICON-NITRIDE; CARBON/CARBON COMPOSITES; MECHANICAL-PROPERTIES; STRUCTURAL EVOLUTION; C/SIC COMPOSITES; BOND STRENGTH; MICROSTRUCTURE; JOINTS; ADHESIVE;
D O I
10.1016/j.ceramint.2021.02.132
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Cf/SiC composites and Si3N4 ceramics are candidate materials for applications in thermal protection system. This paper investigated the joining of Cf/SiC and Si3N4 using Y2O3?Al2O3?SiO2 glass. The reliability of joints was evaluated by thermal shock tests. In this present work, the typical joint structure was Cf/SiC-glass-Si3N4. The results demonstrate that Direct bonding has been identified as the interfacial bonding mechanism at the SiC/glass and glass/Si3N4 interfaces. The maximum shear strength of the Cf/SiC?Si3N4 joint was -34 MPa, which delivered an effective method to achieve strong, reliable bonding between the dissimilar materials. In addition, after thermal shock for 10 cycles, the residual strength remained -13 MPa. Bubbles instead of microcracks formed in the glass filler, which was the main factor causing the degradation of the joint performance. It is suggested that improving the high temperature resistance of joining materials is the key to realize the application of this joint structure.
引用
收藏
页码:15622 / 15630
页数:9
相关论文
共 50 条
  • [21] Joining of SiC by tape-cast SiC-Al2O3-Y2O3 interlayer
    Tian, Wu-Bian
    Kita, Hideki
    Hyuga, Hideki
    Kondo, Naoki
    ADVANCED ENGINEERING CERAMICS AND COMPOSITES, 2011, 484 : 26 - 31
  • [22] Preparation of P+-implanted Y2O3-Al2O3-SiO2 glass for radiotherapy of cancer
    Kawashita, M
    Miyaji, F
    Kokubo, T
    Takaoka, GH
    Yamada, I
    Suzuki, Y
    Inoue, M
    BIOCERAMICS, VOL 10, 1997, : 531 - 534
  • [23] Crystallization behavior and thermal properties of B2O3-containing MgO-Al2O3-SiO2-Li2O glass-ceramic and its wettability on Si3N4 ceramic
    Sun, Liangbo
    Liu, Chunfeng
    Fang, Jian
    Zhang, Jie
    Lu, Chengjie
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2019, 39 (04) : 1532 - 1539
  • [24] Experiments and transient finite element simulation of γ-Y2Si2O7/B2O3Al2O3-SiO2 glass coating on porous Si3N4 substrate under thermal shock
    Fan, Xingyu
    Wang, Hongjie
    Niu, Min
    Zhang, Dahai
    Zhou, Jun
    Fan, Jinpeng
    CERAMICS INTERNATIONAL, 2018, 44 (04) : 4072 - 4079
  • [25] Effect of CaO doping on the properties and crystallization behavior of Y2O3-Al2O3-SiO2 glass
    Yang, Shaobo
    Ma, Yujie
    Li, Jiali
    Kou, Sijie
    Chen, Bo
    Liu, Chidong
    Deng, Juanli
    Fan, Shangwu
    CERAMICS INTERNATIONAL, 2023, 49 (20) : 33188 - 33196
  • [26] Joining of textured PLS-SiC ceramic with CaO-Al2O3-MgO-TiO2-SiO2 glass filler
    Zhan, Chuang-Tian
    Wu, Jin-Yuan
    Huang, Kun-Heng
    Li, Yun
    Wu, Li-Xiang
    He, Sheng-Jin
    Liu, Yang-Qing
    Zhang, Ze-Xi
    Guo, Wei-Ming
    Xue, Jia-Xiang
    Lin, Hua-Tay
    CERAMICS INTERNATIONAL, 2024, 50 (01) : 495 - 502
  • [27] Preparation of Y2O3-Al2O3-SiO2 glasses by combustion synthesis melt-casting under high gravity
    He, Bin
    Liu, Guanghua
    Li, Jiangtao
    Wu, Liang
    Yang, Zengchao
    Guo, Shibin
    Chen, Yixiang
    MATERIALS RESEARCH BULLETIN, 2011, 46 (07) : 1035 - 1038
  • [28] Novel design of a Si3N4/BaO-Al2O3-SiO2 coating with a heterogeneous- layer structure on porous Si3N4 ceramic
    Liu, Zhengdao
    Tong, Zongwei
    Yue, Sheng
    Li, Xiaolei
    Ji, Huiming
    CERAMICS INTERNATIONAL, 2021, 47 (01) : 1456 - 1461
  • [29] Si3N4 ceramics joined with Si3N4-Li2O-Y2O3 by spark plasma sintering
    Zhu, Lin-Lin
    Tan, Xing-Hao
    Chen, Jia-Hao
    Chen, Xu-Hui
    Dong, Chen-Hao
    Liu, Hong-Lan
    Jian, Yu-Jian
    Zhang, Guang-Xiang
    Lin, Hua-Tay
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2025, 45 (01)
  • [30] Effect of Sm2O3 on microstructure and high-temperature stability of MgAl2O4-Si3N4 ceramic for solar thermal absorber
    Zhang, Yaxiang
    Wu, Jianfeng
    Xu, Xiaohong
    Zhou, Yang
    Zhang, Qiankun
    Song, Jia
    JOURNAL OF ALLOYS AND COMPOUNDS, 2017, 711 : 365 - 373