Additive Friction Stir-Enabled Solid-State Additive Manufacturing for the Repair of 7075 Aluminum Alloy

被引:108
作者
Griffiths, R. Joey [1 ]
Petersen, Dylan T. [1 ]
Garcia, David [1 ]
Yu, Hang Z. [1 ]
机构
[1] Virginia Tech, Dept Mat Sci & Engn, 460 Old Turner St, Blacksburg, VA 24061 USA
来源
APPLIED SCIENCES-BASEL | 2019年 / 9卷 / 17期
关键词
solid-state additive manufacturing; repair; high-strength Al alloys; friction stir; severe plastic deformation; interface; CORROSION BEHAVIOR; DYNAMIC RECRYSTALLIZATION; WELDING PROCESS; WELDED-JOINTS; MICROSTRUCTURE; KEYHOLE;
D O I
10.3390/app9173486
中图分类号
O6 [化学];
学科分类号
0703 ;
摘要
The repair of high strength, high performance 7075 aluminum alloy is essential for a broad range of aerospace and defense applications. However, it is challenging to implement it using traditional fusion welding-based approaches, owing to hot cracking and void formation during solidification. Here, the use of an emerging solid-state additive manufacturing technology, additive friction stir deposition, is explored for the repair of volume damages such as through-holes and grooves in 7075 aluminum alloy. Three repair experiments have been conducted: double through-hole filling, single through-hole filling, and long, wide-groove filling. In all experiments, additive friction stir deposition proves to be effective at filling the entire volume. Additionally, sufficient mixing between the deposited material and the side wall of the feature is always observed in the upper portions of the repair. Poor mixing and inadequate repair quality have been observed in deeper portions of the filling in some scenarios. Based on these observations, the advantages and disadvantages of using additive friction stir deposition for repairing volume damages are discussed. High quality and highly flexible repairs are expected with systematic optimization work on process control and repair strategy development in the future.
引用
收藏
页数:15
相关论文
共 38 条
[1]   Recent Developments in Friction Stir Welding of Al-alloys [J].
Cam, Gurel ;
Mistikoglu, Selcuk .
JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2014, 23 (06) :1936-1953
[2]   Characteristics of friction plug welding to 10 mm thick AA2219-T87 sheet: Weld formation, microstructure and mechanical property [J].
Du, Bo ;
Sun, Zhuanping ;
Yang, Xinqi ;
Cui, Lei ;
Song, Jianling ;
Zhang, Zhongping .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2016, 654 :21-29
[3]   A Perspective on Solid-State Additive Manufacturing of Aluminum Matrix Composites Using MELD [J].
Griffiths, R. Joey ;
Perry, Mackenzie E. J. ;
Sietins, Jennifer M. ;
Zhu, Yunhui ;
Hardwick, Nanci ;
Cox, Chase D. ;
Rauch, Hunter A. ;
Yu, Hang Z. .
JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2019, 28 (02) :648-656
[4]  
Grushko O., 2017, ALUMINUM LITHIUM ALL, V8, P1
[5]   AA7075 bit for repairing AA2219 keyhole by filling friction stir welding [J].
Han, Bing ;
Huang, Yongxian ;
Lv, Shixiong ;
Wan, Long ;
Feng, Jicai ;
Fu, Guansheng .
MATERIALS & DESIGN, 2013, 51 :25-33
[6]  
Hashimoto S., 1986, HOT WORKING ALUMINUM, P91
[7]  
Hashmi S, 2014, COMPREHENSIVE MATERIALS PROCESSING, VOL 1: ASSESSING PROPERTIES OF CONVENTIONAL AND SPECIALIZED MATERIALS, P1
[8]   A review of dynamic recrystallization phenomena in metallic materials [J].
Huang, K. ;
Loge, R. E. .
MATERIALS & DESIGN, 2016, 111 :548-574
[9]   New technique of filling friction stir welding [J].
Huang, Y. X. ;
Han, B. ;
Tian, Y. ;
Liu, H. J. ;
Lv, S. X. ;
Feng, J. C. ;
Leng, J. S. ;
Li, Y. .
SCIENCE AND TECHNOLOGY OF WELDING AND JOINING, 2011, 16 (06) :497-501
[10]   Retrogression and Reaging Applied to Warm Forming of High-Strength Aluminum Alloy AA7075-T6 Sheet [J].
Ivanoff, Thomas A. ;
Carter, Jon T. ;
Hector, Louis G., Jr. ;
Taleff, Eric M. .
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2019, 50A (03) :1545-1561