Fabrication of WC-8 wt.%Co hard materials by two rapid sintering processes

被引:45
|
作者
Kim, Hwan Cheol
Jeong, In Kyoon
Shon, In Jin [1 ]
Ko, In Yong
Doh, Jung Mann
机构
[1] Chonbuk Natl Univ, Inst Engn Res, Res Ctr Adv Mat Dev, Dept Adv Mat Engn, Jeonju 560756, Jeonbuk, South Korea
[2] Korea Inst Sci & Technol, Met Proc Res Ctr, Seoul 136791, South Korea
来源
INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS | 2007年 / 25卷 / 04期
关键词
rapid sintering; WC-Co composites; microstructures; hardness; fracture toughness;
D O I
10.1016/j.ijrmhm.2006.09.001
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Two methods, high-frequency induction-heated sintering (HFIHS) and pulsed current activated sintering (PCAS), were utilized to consolidate WC-8 wt.%Co hard materials. The demonstrated advantages of these processes are rapid densification to near theoretical density in a relatively short time and without significant change in grain size. The effect of initial particle size of WC powder on the sintering behavior and mechanical properties were investigated. The hardness, fracture toughness and the relative density of the WC-8Co composites consolidated by HFIHS and PCAS were investigated. (c) 2006 Elsevier Ltd. All rights reserved.
引用
收藏
页码:336 / 340
页数:5
相关论文
共 50 条
  • [1] Densification and alloying of microwave sintering WC-8 wt.%Co composites
    Bao, Rui
    Yi, Jianhong
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2014, 43 : 269 - 275
  • [2] Vacuum sintering of WC-8 wt.% Co hardmetals from WC powders with different dispersity
    Kurlov, A. S.
    Gusev, A. I.
    Rempel, A. A.
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2011, 29 (02): : 221 - 231
  • [3] Skin effect of WC-8 wt% Co alloy by microwave sintering
    Rui Bao
    Jian-Hong Yi
    Yuan-Dong Peng
    Feng-Xian Li
    Shang Li
    Shao-Yu Li
    Rare Metals, 2022, 41 (04) : 1364 - 1368
  • [4] Skin effect of WC-8 wt% Co alloy by microwave sintering
    Bao, Rui
    Yi, Jian-Hong
    Peng, Yuan-Dong
    Li, Feng-Xian
    Li, Shang
    Li, Shao-Yu
    RARE METALS, 2022, 41 (04) : 1364 - 1368
  • [5] Effect of WC nanoparticle size on the sintering temperature, density, and microhardness of WC-8 wt % Co alloys
    Kurlov, A. S.
    Rempel, A. A.
    INORGANIC MATERIALS, 2009, 45 (04) : 380 - 385
  • [6] Effect of WC nanoparticle size on the sintering temperature, density, and microhardness of WC-8 wt % Co alloys
    A. S. Kurlov
    A. A. Rempel
    Inorganic Materials, 2009, 45 : 380 - 385
  • [7] Effect of sintering temperature on the phase composition and microhardness of WC-8 wt % Co cemented carbide
    A. S. Kurlov
    A. A. Rempel’
    Inorganic Materials, 2007, 43 : 602 - 607
  • [8] Effect of sintering temperature on the phase composition and microhardness of WC-8 wt % co cemented carbide
    Kurlov, A. S.
    Rempel, A. A.
    INORGANIC MATERIALS, 2007, 43 (06) : 602 - 607
  • [9] The Structure and Mechanical Properties of WC-8 wt.% Co Hardmetal Produced by Cold and Hot Isostatic Pressing
    Akimov, G. Ya
    Andreev, I., V
    Sheremet, V., I
    Trosnikova, I. Yu
    Loboda, P., I
    Kosenchuk, T. O.
    POWDER METALLURGY AND METAL CERAMICS, 2022, 61 (1-2) : 9 - 17
  • [10] Consolidation and mechanical properties of ultra fine WC-5 wt.% carbides hard materials by a rapid sintering method
    Shon, In-Jin
    Oh, Ik-Hyun
    Ryu, Jung-Han
    Jang, Jun-Ho
    Youn, Hee-Jun
    Park, Hyun-Kuk
    JOURNAL OF CERAMIC PROCESSING RESEARCH, 2013, 14 (05): : 641 - 647