Structure failure of the sealing in the assembly process for proton exchange membrane fuel cells

被引:69
作者
Liang, Peng [1 ]
Qiu, Diankai [1 ]
Peng, Linfa [1 ]
Yi, Peiyun [1 ]
Lai, Xinmin [1 ,2 ]
Ni, Jun [3 ]
机构
[1] Shanghai Jiao Tong Univ, State Key Lab Mech Syst & Vibrat, Shanghai 200240, Peoples R China
[2] Shanghai Jiao Tong Univ, Shanghai Key Lab Digital Manufacture Thin Walled, Shanghai 200240, Peoples R China
[3] Univ Michigan, Dept Mech Engn, Ann Arbor, MI 48109 USA
基金
中国国家自然科学基金;
关键词
Proton exchange membrane fuel cell; Sealing structure failure; Slippage angle; Slippage distance; Stack assembly; GAS-DIFFUSION LAYER; CONTACT PRESSURE DISTRIBUTION; PIN-FIN ARRAYS; BIPOLAR PLATE; END-PLATES; MICRO-REACTOR; PERFORMANCE; RESISTANCE; PEMFC; COMPRESSION;
D O I
10.1016/j.ijhydene.2017.01.026
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Sealing stability in proton exchange membrane fuel cell (PEMFC) is critical to the performance and safety of stacks. However, sealing structure failure (SSF), which leads to the leakage of reactant gases, often occurs in the assembly process or start-up operation for PEMFCs. This study aims to investigate the effects of geometrical structure and material parameters of sealing components on the sealing structure failure. Slippage angle and slippage distance are adopted to evaluate the risk of SSF. Finite element (FE) simulations are conducted with consideration of the assembly process and start-up operation. Experiments are carried out to validate the accuracy of the FE model. Influences of parameters of gasket, membrane electrode assembly (MEA) frame, sealing groove shape of bipolar plate (BPP), and gas pressure are discussed in detail. Meanwhile, the risks of SSF for the stack by using metallic and graphite BPPs are compared. It is demonstrated that material properties and geometrical parameters of sealing components in PEMFC have great effects on SSF. The methodology developed is beneficial to the understanding of the SSF, and it can also be applied to guide the design of PEMFC stack assembly process to keep a good sealing reliability. (C) 2017 Hydrogen Energy Publications LLC. Published by Elsevier Ltd. All rights reserved.
引用
收藏
页码:10217 / 10227
页数:11
相关论文
共 52 条
  • [1] Aissaoui H, 2012, GLOB J RES ENG, V12
  • [2] Ali A, 2010, J SCI IND RES INDIA, V69, P495
  • [3] Investigation of contact pressure distribution over the active area of PEM fuel cell stack
    Alizadeh, E.
    Barzegari, M. M.
    Momenifar, M.
    Ghadimi, M.
    Saadat, S. H. M.
    [J]. INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2016, 41 (04) : 3062 - 3071
  • [4] Bagotsky VS, 2015, PROTON EXCHANGE MEMB, P151
  • [5] Local measurements of hydrogen crossover rate in polymer electrolyte membrane fuel cells
    Baik, Kyung Don
    Kong, Im Mo
    Hong, Bo Ki
    Kim, Sae Hoon
    Kim, Min Soo
    [J]. APPLIED ENERGY, 2013, 101 : 560 - 566
  • [6] Banan R, 2012, PROCEEDINGS OF THE ASME 10TH FUEL CELL SCIENCE, ENGINEERING, AND TECHNOLOGY CONFERENCE, 2012, P229
  • [7] Contact mechanics approach to determine contact surface area between bipolar plates and current collector in proton exchange membrane fuel cells
    Barber, M.
    Sun, T. S.
    Petrach, E.
    Wang, X.
    Zou, Q.
    [J]. JOURNAL OF POWER SOURCES, 2008, 185 (02) : 1252 - 1256
  • [8] An investigation of temperature effect on performance of dead-end cascade H2/O2 PEMFC stack with integrated humidifier and separator
    Barzegari, Mohammad M.
    Dardel, Morteza
    Ramiar, Abas
    Alizadeh, Ebrahim
    [J]. INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2016, 41 (04) : 3136 - 3146
  • [9] Performance of individual cells in polymer electrolyte membrane fuel cell stack under-load cycling conditions
    Bose, A.
    Babburi, P.
    Kumar, R.
    Myers, D.
    Mawdsley, J.
    Milhuff, J.
    [J]. JOURNAL OF POWER SOURCES, 2013, 243 : 964 - 972
  • [10] Rubber modeling using uniaxial test data
    Bradley, GL
    Chang, PC
    McKenna, GB
    [J]. JOURNAL OF APPLIED POLYMER SCIENCE, 2001, 81 (04) : 837 - 848