The Influence of Crystallographic Texture and Niobium Stabilisation on the Corrosion Resistance of Ferritic Stainless Steel

被引:0
作者
Narvaes Ardila, Miguel Angel [1 ]
Labiapari, Wilian Silva [1 ]
Biasoli de Mello, Jose Daniel [1 ]
机构
[1] Univ Fed Uberlandia, Lab Tribol & Mat, Uberlandia, MG, Brazil
来源
MATERIALS RESEARCH-IBERO-AMERICAN JOURNAL OF MATERIALS | 2017年 / 20卷 / 03期
关键词
Potentiodynamic polarisation; corrosion; crystallographic texture; stabilising elements; ferritic stainless steel; niobium; INTERGRANULAR CORROSION; PITTING CORROSION; GRAIN-SIZE; BEHAVIOR; CR; MICROSTRUCTURE; PRECIPITATION; DEFORMATION; ORIENTATION; ALUMINUM;
D O I
10.1590/1980-5373-MR-2016-0622
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The objective of this work is to investigate the influence of the crystallographic texture on the corrosion resistance of 16% Cr ferritic stainless steel. Samples of ASTM S43000 ferritic stainless steel, both niobium-stabilised and non-stabilised, were used. The samples were subjected to crystallographic characterisation (EBSD) and analysed using an inverse pole figure (IPF) and a crystalline orientation distribution function (CODF). The samples also underwent anodic potentiodynamic polarisation tests (deaeration by high-purity argon gas) in 3.56% NaCl and 1N H2SO4 solutions, and the surface was examined by SEM after the tests. The results showed a clear influence of the crystallographic texture on the corrosion resistance. The niobium decreases the amount of the preferred orientation and thus the influence of the texture on the corrosion resistance, although the corrosion resistance of the stainless steel is increased as niobium carbides are formed.
引用
收藏
页码:576 / 583
页数:8
相关论文
共 38 条
  • [1] Effect of grain size on pitting corrosion of 304L austenitic stainless steel
    Aghuy, A. Abbasi
    Zakeri, M.
    Moayed, M. H.
    Mazinani, M.
    [J]. CORROSION SCIENCE, 2015, 94 : 368 - 376
  • [2] [Anonymous], 2004, G594 ASTM
  • [3] Bakhtiari A, 2015, METALL MATER ENG, V21, P1
  • [4] Chouthai S. S., 1976, British Corrosion Journal, V11, P40, DOI 10.1179/000705976798320278
  • [5] Metastable pitting behavior of aluminum single crystals
    Davis, BW
    Moran, PJ
    Natishan, PM
    [J]. CORROSION SCIENCE, 2000, 42 (12) : 2187 - 2192
  • [6] De Angclis R., 2000, JCPDS-International Centre for Diffraction Data, Advances in X-ray Analysis, V42, P510
  • [7] Grain size distribution effects on the corrosion behaviour of materials
    Gollapudi, Srikant
    [J]. CORROSION SCIENCE, 2012, 62 : 90 - 94
  • [8] Effect of deformation on corrosion behavior of Ti-23Nb-0.7Ta-2Zr-O alloy
    Guo, W. Y.
    Sun, J.
    Wu, J. S.
    [J]. MATERIALS CHARACTERIZATION, 2009, 60 (03) : 173 - 177
  • [9] The corrosion behavior of niobium bearing cold deformed austenitic stainless steels in 3.5% NaCl solution
    Hamdy, Abdel Salam
    El-Shenawy, Eman
    El-Bitar, T.
    [J]. MATERIALS LETTERS, 2007, 61 (13) : 2827 - 2832
  • [10] Effect of Precipitation on Intergranular Corrosion Resistance of 430 Ferritic Stainless Steel
    Huang, Xun-zeng
    Wang, Dan
    Yang, Yi-tao
    [J]. JOURNAL OF IRON AND STEEL RESEARCH INTERNATIONAL, 2015, 22 (11) : 1062 - 1068