Performance of cement-based materials containing calcined coal gangue with different calcination regimes

被引:46
作者
Guo, Zhaoheng [1 ,3 ]
Xu, Jingjing [2 ]
Xu, Zhenhai [1 ,3 ]
Gao, Jianming [1 ,3 ]
Zhu, Xiaoliang [2 ,4 ]
机构
[1] Southeast Univ, Sch Mat Sci & Engn, Nanjing 211189, Peoples R China
[2] China Western Construct Acad Bldg Mat Co Ltd, Chengdu 610221, Peoples R China
[3] Jiangsu Key Lab Construction Mat, Nanjing 211189, Peoples R China
[4] China West Construction Grp Co Ltd, Chengdu 610213, Peoples R China
来源
JOURNAL OF BUILDING ENGINEERING | 2022年 / 56卷
基金
中国国家自然科学基金;
关键词
Coal gangue; Pozzolanic reactivity; Fluidity; Mechanical property; Pore structure; POZZOLANIC ACTIVITY;
D O I
10.1016/j.jobe.2022.104821
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
The storage of coal gangue (CG) takes up a lot of lands and pollutes the environment. Calcined CG has the potential to be used as supplementary cementitious material. In this paper, the CG from Yibin, Sichuan province of China were treated with different calcined temperature, holding times and cooling modes, and the microtopography, phase composition and pozzolanic reactivity of calcined CG were studied. Meanwhile, the fluidity, mechanical properties, hydration products, and pore structure of cement paste and mortar with different calcined CG were analyzed. The apparent color of coal gangue under different treatment methods has also been studied to promote its better application for a wider range in cement-based materials. Results showed that there exists an optimal calcination condition of calcined CG at 800 degrees C and holding time of 2 h. Rapid cooling and slow cooling reduced the activity of calcined CG. Calcined CG powder would reduce the fluidity of cement mortar. However, proper calcination temperature and sufficient holding time could eliminate it to some extent. It was also found that calcination temperature has a greater impact on the early age reactivity of CG when compared to different temperature treated CG powder, C8T2 sample has the best early activity. Compared to rapid cooling, slow cooling and water-cooling mode, room temperature cooling would result in higher reactive CG. CG powder after proper thermal treatment could refine the pore structure of the hardened cement paste in the later age (28 days), reduce the harmful pores content (>100 nm), and increase harmless pores content (<100 nm) in hardened cement paste. It was found that the CG powder of calcined at 800 degrees C for 2 h, cooling in water and room temperature might be more suitable as the supplementary cementing material combined the apparent color, pozzolanic reactivity, and preparation process.
引用
收藏
页数:15
相关论文
共 27 条
  • [1] [Anonymous], 2005, GBT24192005
  • [2] [Anonymous], 2017, 15962017 GBT
  • [3] Effect of calcination condition on the microstructure and pozzolanic activity of calcined coal gangue
    Cao, Zhao
    Cao, Yongdan
    Dong, Hongjuan
    Zhang, Jinshan
    Sun, Chunbao
    [J]. INTERNATIONAL JOURNAL OF MINERAL PROCESSING, 2016, 146 : 23 - 28
  • [4] Effect of coal gangue with different kaolin content son compressive strength and pore
    Chen Yimin
    Zhou Shuangxi
    Zhang Wensheng
    [J]. JOURNAL OF WUHAN UNIVERSITY OF TECHNOLOGY-MATERIALS SCIENCE EDITION, 2008, 23 (01): : 12 - 15
  • [5] Chinese Standard, 1999, Method of testing cementsDetermination of strength
  • [6] Scientific Aspects of Kaolinite Based Coal Mining Wastes in Pozzolan/Ca(OH)2 System
    Frias, M.
    Vigil de la Villa, R.
    Sanchez de Rojas, M. I.
    Medina, C.
    Juan Valdes, A.
    [J]. JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2012, 95 (01) : 386 - 391
  • [7] Giergiczny Z., 2019, CEMENT CONCRETE RES, V124, P1, DOI DOI 10.1016/j.cemconres.2019.105826
  • [8] Early hydration of composite cement with thermal activated coal gangue
    Guo Wei
    Zhu Jianping
    Li Dongxu
    Chen Jianhua
    Yang Nanru
    [J]. JOURNAL OF WUHAN UNIVERSITY OF TECHNOLOGY-MATERIALS SCIENCE EDITION, 2010, 25 (01): : 162 - 166
  • [9] International Energy Agency, 2019, Renewables Information 2019: Overview
  • [10] International Energy Agency Statistics, 2019, CEM MOR EFF NEED