Joining of zirconia to metal with Cu-Ga-Ti and Cu-Sn-Pb-Ti fillers

被引:38
作者
Durov, AV [1 ]
Kostjuk, BD [1 ]
Shevchenko, AV [1 ]
Naidich, YV [1 ]
机构
[1] Natl Acad Sci, Inst Mat Sci Problems, UA-03142 Kiev, Ukraine
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2000年 / 290卷 / 1-2期
关键词
ceramic to metal joint; zirconia; brazing;
D O I
10.1016/S0921-5093(00)00916-3
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The method of brazing by capillary impregnation of Cu-Ca melt through a titanium powder layer situated between brazed details is elaborated. Samples of ZrO2 ceramic/metal brazed joints using Cu-Ga-Ti filler and Cu-Su-Pb-Ti filler were fabricated. The joints' shear strength was 277 +/- 37 MPa for the Cu-Ga-Ti and 156 +/- 25 MPa for the Cu-Sn-Pb-Ti. (C) 2000 Elsevier Science S.A. All rights reserved.
引用
收藏
页码:186 / 189
页数:4
相关论文
共 7 条
[1]  
COLIN C, 1991, VIDE COUCHES MINCE S, V47, P146
[2]  
LASCAR G, 1991, SOUDAGE TECHN CONNEX, V45, P11
[3]  
NAIDICH YV, 1992, ADHEZIYA RASPLAVOV P, V27, P53
[4]   Brazing of Si3N4 by active Cu-Ga-Ti filler alloys [J].
Prokopenko, AA ;
Zhuravlev, VS ;
Naidich, YV .
JOURNAL OF MATERIALS SCIENCE LETTERS, 1998, 17 (24) :2121-2123
[5]   JOINING OF YTTRIA TETRAGONAL ZIRCONIA POLYCRYSTAL WITH AN ALUMINUM ZIRCONIUM ALLOY [J].
RATHNER, RC ;
GREEN, DJ .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1990, 73 (04) :1103-1105
[6]  
SUHMAN AL, 1974, T I HIM UNC AN SSSR, V29, P56
[7]  
UEKI M, 1998, J MATER SCI, V23, P2983