Paucity of Nanolayering in Resin-Dentin Interfaces of MDP-based Adhesives

被引:67
|
作者
Tian, F. [1 ]
Zhou, L. [2 ]
Zhang, Z. [3 ]
Niu, L. [4 ]
Zhang, L. [1 ]
Chen, C. [5 ]
Zhou, J. [1 ]
Yang, H. [2 ]
Wang, X. [1 ,6 ]
Fu, B. [3 ]
Huang, C. [2 ]
Pashley, D. H. [6 ]
Tay, F. R. [6 ]
机构
[1] Peking Univ, Sch & Hosp Stomatol, Dept Cariol & Endodontol, Beijing 100871, Peoples R China
[2] Wuhan Univ, Sch & Hosp Stomatol, Key Lab Oral Biomed, Minist Educ, Wuhan 430072, Peoples R China
[3] Zhejiang Univ, Sch & Hosp Stomatol, Dept Prosthodont, Hangzhou 310027, Zhejiang, Peoples R China
[4] Fourth Mil Hosp, Sch Stomatol, State Key Lab Mil Stomatol, Xian, Shaanxi, Peoples R China
[5] Nanjing Med Univ, Affiliated Hosp Stomatol, Dept Operat Dent & Endodont, Nanjing, Jiangsu, Peoples R China
[6] Augusta Univ, Dent Coll Georgia, Augusta, GA 30912 USA
基金
国家高技术研究发展计划(863计划);
关键词
10-MDP; transmission electron microscopy; x-ray diffraction; functional monomer; methacryloyloxydecyl dihydrogen phosphate; dental bonding; PHOSPHORIC-ACID ESTER; X-RAY-DIFFRACTION; AMPHIPHILES; SURFACTANT; MONOMER; TISSUE; ENAMEL;
D O I
10.1177/0022034515623741
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Self-assembled nanolayering structures have been reported in resin-dentin interfaces created by adhesives that contain 10-methacryloyloxydecyl dihydrogen phosphate (10-MDP). These structures have been hypothesized to contribute to bond durability. The objective of the present study was to determine the extent of nanolayering in resin-dentin interfaces after application of commercialized 10-MDP-containing self-etch and universal adhesives to human dentin. Seven commercialized adhesives were examined: Adhese Universal (Ivoclar-Vivadent), All-Bond Universal (Bisco, Inc.), Clearfil SE Bond 2, Clearfil S3 Bond Plus, Clearfil Universal Bond (all from Kuraray Noritake Dental Inc.), G-Premio Bond (GC Corp.), and Scotchbond Universal (3M ESPE). Each adhesive was applied in the self-etch mode on midcoronal dentin according to the respective manufacturer's instructions. Bonded specimens (n = 6) were covered with flowable resin composite, processed for transmission electron microscopy, and examined at 30 random sites without staining. Thin-film glancing angle X-ray diffraction (XRD) was used to detect the characteristic peaks exhibited by nanolayering (n = 4). The control consisted of 15%wt, 10%wt, and 5%wt 10-MDP (DM Healthcare Products, Inc.) dissolved in a mixed solvent (ethanol and water weight ratio 9:8, with photoinitiators). Experimental primers were applied to dentin for 20 s, covered with hydrophobic resin layer, and examined in the same manner. Profuse nanolayering with highly ordered periodicity (similar to 3.7 nm wide) was observed adjacent to partially dissolved apatite crystallites in dentin treated with the 15% 10-MDP primer. Three peaks in the 2 range of 2.40 degrees (3.68 nm), 4.78 degrees (1.85 nm), and 7.18 degrees (1.23 nm) were identified from thin-film XRD. Reduction in the extent of nanolayering was observed in the 10% and 5% 10-MDP experimental primer-dentin interface along with lower intensity XRD peaks. Nanolayering and characteristic XRD peaks were rarely observed in specimens prepared from the commercialized adhesives. The sparsity of nanolayering in resin-dentin interfaces created by commercialized adhesives challenges its clinical effectiveness as a mechanism for improving bond longevity in dentin bonding.
引用
收藏
页码:380 / 387
页数:8
相关论文
共 50 条
  • [21] Moist vs over-dried etched dentin: FE-SEM/TEM and bond strength evaluation of resin-dentin interfaces produced by universal adhesives
    Kumagai, Rose Y.
    Hirata, Ronaldo
    Pereira, Patricia N. R.
    Reis, Andre F.
    JOURNAL OF ESTHETIC AND RESTORATIVE DENTISTRY, 2020, 32 (03) : 325 - 332
  • [22] Influence of Ozone Gas and Ozonated Water Application to Dentin and Bonded Interfaces on Resin-Dentin Bond Strength
    Garcia, Eugenio Jose
    Mena Serrano, Alexandra Patricia
    Urruchi, Wilfredo Irrazabal
    Deboni, Maria Cristina
    Reis, Alessandra
    Miranda Grande, Rosa Helena
    Loguercio, Alessandro Dourado
    JOURNAL OF ADHESIVE DENTISTRY, 2012, 14 (04): : 363 - 370
  • [23] Effect of the demineralisation efficacy of MDP utilized on the bonding performance of MDP-based all-in-one adhesives
    Fujita , Kou
    Nikaido, Toru
    Burrow, Michael Francis
    Iwasaki, Taro
    Tanimoto, Yasuhiro
    Hirayama, Satoshi
    Nishiyama, Norihiro
    JOURNAL OF DENTISTRY, 2018, 77 : 59 - 65
  • [24] Matrix metalloproteinase inhibitor modulates esterase-catalyzed degradation of resin-dentin interfaces
    Serkies, Kyle B.
    Garcha, Reena
    Tam, Laura E.
    De Souza, Grace M.
    Finer, Yoav
    DENTAL MATERIALS, 2016, 32 (12) : 1513 - 1523
  • [25] Four-year effects of copper-nanoparticles on durability of resin-dentin interfaces
    Naupari-Villasante, Romina
    Gutierrez, Mario F.
    Matos, Thalita de Paris
    Nunez, Alejandra
    Fernandez, Eduardo
    Reis, Alessandra
    Loguercio, Alessandro D.
    INTERNATIONAL JOURNAL OF ADHESION AND ADHESIVES, 2022, 119
  • [26] Effects of agitation of self-etching primers/adhesives on resin-dentin bond strength.
    Chan, KM
    Tay, FR
    King, NM
    Imazato, S
    Pashley, DH
    JOURNAL OF DENTAL RESEARCH, 2002, 81 : A222 - A222
  • [27] In vitro degradation of resin-dentin bonds with one-bottle self-etching adhesives
    Hashimoto, Masanori
    Fujita, Shinichi
    Endo, Kazuhiko
    Ohno, Hiroki
    EUROPEAN JOURNAL OF ORAL SCIENCES, 2009, 117 (05) : 611 - 617
  • [28] Measurement of microstrains across loaded resin-dentin interfaces using microscopic moire interferometry
    Wood, Judy D.
    Sobolewski, Paul
    Thakur, Varun
    Arola, Dwayne
    Nazari, Ahmed
    Tay, Franklin R.
    Pashley, David H.
    DENTAL MATERIALS, 2008, 24 (07) : 859 - 866
  • [29] Investigation of the effect of Tideglusib on the hydroxyapatite formation, crystallinity and elasticity of conditioned resin-dentin interfaces
    Toledano, Manuel
    Fernandez-Romero, Enrique
    Osorio, Maria T.
    Osorio, Estrella
    Aguilera, Fatima S.
    Toledano, Raquel
    Osorio, Raquel
    JOURNAL OF DENTISTRY, 2024, 150
  • [30] Effect of nanolayering of calcium salts of phosphoric acid ester monomers on the durability of resin-dentin bonds (vol 38, pg 190, 2016)
    Tian, Fu-cong
    Wang, Xiao-yan
    Huang, Qi
    Niu, Li-na
    Mitchell, Jan
    Zhang, Zheng-yi
    Prananik, Chandrani
    Zhang, Lu
    Chen, Ji-hua
    Breschi, Lorenzo
    Pashley, David H.
    Tay, Franklin R.
    ACTA BIOMATERIALIA, 2017, 49 : 605 - 605