Application of Carbon Composite Bricks for Blast Furnace Hearth

被引:0
|
作者
Zuo, Haibin [1 ,2 ]
Wang, Cong [1 ,2 ]
Zhang, Jianliang [1 ,2 ]
Zhao, Yongan [3 ]
Jiao, Kexin [1 ,2 ]
机构
[1] Univ Sci & Technol Beijing, State Key Lab Adv Met, 30 Xueyuan Rd, Beijing 100083, Peoples R China
[2] Univ Sci & Technol Beijing, Sch Met & Ecol Engn, Beijing 100083, Peoples R China
[3] Henan Winna Ind Grp Co Ltd, Beishankou Town 451250, Henan, Peoples R China
关键词
Blast furnace; Long service life; Carbon composite brick; SLAG; LIFE;
D O I
暂无
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Traditional refractory materials for blast furnace hearth lining are mainly composed of carbon bricks and the ceramic cup. However, these materials can't meet the demands for long service life design of blast furnaces. In this paper, a new refractory called carbon composite brick (CCB) was introduced, which combined the advantages of carbon bricks and the ceramic cup. In this case, the resistance of the CCB against corrosion was equal to the ceramic cup and the thermal conductivity of the CCB was equal to carbon bricks. From the results of more than 20 blast furnaces, the CCB could be well used in small blast furnaces and large blast furnaces. In the bad condition of low grade burden and high smelting intensity, the CCB gave full play to the role of cooling system, and effectively resisted the erosion of hot metal to improve the service life of blast furnaces.
引用
收藏
页码:595 / 602
页数:8
相关论文
共 50 条
  • [31] Influence of the Residual Iron on the Erosion of Carbon Bricks in a 4000 m3 Blast Furnace Hearth: From the Measured Properties to the Proposed Mechanisms
    Wang, Gang
    Liao, Zhehan
    Hu, Zhaowen
    Wang, Dongdong
    Bai, Hao
    Zou, Zhongping
    Xu, Jian
    METALLURGICAL AND MATERIALS TRANSACTIONS B-PROCESS METALLURGY AND MATERIALS PROCESSING SCIENCE, 2022, 53 (02): : 931 - 937
  • [32] Influence of the Residual Iron on the Erosion of Carbon Bricks in a 4000 m3 Blast Furnace Hearth: From the Measured Properties to the Proposed Mechanisms
    Gang Wang
    Zhehan Liao
    Zhaowen Hu
    Dongdong Wang
    Hao Bai
    Zhongping Zou
    Jian Xu
    Metallurgical and Materials Transactions B, 2022, 53 : 931 - 937
  • [33] THERMAL-STRESS FATIGUE OF CARBON BLOCK IN BLAST-FURNACE HEARTH
    NUMATA, N
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1987, 73 (04): : S74 - S74
  • [34] Analysis of erosion morphology characteristics and mechanism of carbon brick in blast furnace hearth
    Cao, Jian
    Jiao, Kexin
    Zhang, Jianliang
    Wang, Cui
    Lei, Ming
    Shi, Huangyu
    ENGINEERING FAILURE ANALYSIS, 2025, 173
  • [35] Reactivity of Coke Ash on Alumina-Carbon Blast Furnace Hearth Refractories
    Drain, Phillip Brian
    Monaghan, Brian Joseph
    Chapman, Michael Wallace
    Nightingale, Robert John
    ISIJ INTERNATIONAL, 2015, 55 (09) : 1849 - 1858
  • [36] Blast furnace hearth lining and cooling concepts
    Hebel, Rudolf
    Hille, Volker
    STAHL UND EISEN, 2008, 128 (02): : 31 - +
  • [37] Long life technology for blast furnace hearth
    Zhang, Dianyou
    Kang T'ieh/Iron and Steel (Peking), 1995, 30 (04): : 6 - 9
  • [38] Determination of the liquid level in the hearth of the blast furnace
    Peters, M
    Rüther, P
    Schmöle, P
    Thiemann, T
    Rödl, S
    60TH IRONMAKING CONFERENCE PROCEEDINGS, 2001, 60 : 283 - 295
  • [39] COMPUTATION OF THE EROSION IN THE HEARTH OF A BLAST-FURNACE
    PREUER, A
    WINTER, J
    HIEBLER, H
    STEEL RESEARCH, 1992, 63 (04): : 147 - 151
  • [40] CONTROL OF HEARTH HEAT IN IRON BLAST FURNACE
    HODGE, AL
    BABCOCK, RS
    JOURNAL OF METALS, 1965, 17 (11): : 1215 - &