Racemization on thermal degradation of poly(L-lactide) with calcium salt end structure

被引:66
作者
Fan, YJ
Nishida, H
Shirai, Y
Endo, T
机构
[1] Kinki Univ, Mol Engn Inst, Iizuka, Fukuoka 8208555, Japan
[2] Kyushu Inst Technol, Grad Sch Life Sci & Syst Engn, Kitakyushu, Fukuoka 8080196, Japan
[3] Yamagata Univ, Fac Engn, Yonezawa, Yamagata 9928510, Japan
关键词
poly(L-lactide); poly(L-lactic acid); PLLA; thermal degradation; pyrolysis; racemization; calcium; end structure;
D O I
10.1016/S0141-3910(03)00033-8
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
Poly(L-lactide) with calcium salt end structure (PLLA-Ca) is a promising material for PLLA recycling because of the ease of lactide recovery through the unzipping depolymerization process. However, the pyrolysis of PLLA-Ca also causes meso-lactide to form. In this article, the racemization in PLLA-Ca pyrolysis was analyzed in detail with Py-MS, Py-GC/MS, and a glass tube oven. The results suggested that at a temperature lower than 250 degreesC, nucleophilic attack by a carboxylate anion end on an asymmetrical methyne carbon in a penultimate lactate unit occurred, resulting in the predominant formation of meso-lactide. On the other hand, also at temperatures over 320 degreesC, by-reactions, such as enolization reactions, caused the meso-lactide to form, but not dominantly. In the temperature range of 250-320 degreesC, L,L-lactide was produced exclusively, because unzipping depolymerization proceeded as the main reaction. This is a very significant result for PLLA recycling, because PLLA-Ca is an easily recyclable material, which depolymerizes based on the 1st-order weight loss process. (C) 2003 Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:503 / 511
页数:9
相关论文
共 29 条
  • [1] AJIOKA M, 1995, J ENVIRON POLYM DEGR, V3, P4
  • [2] Amass W, 1998, POLYM INT, V47, P89, DOI 10.1002/(SICI)1097-0126(1998100)47:2<89::AID-PI86>3.0.CO
  • [3] 2-F
  • [4] Biodegradation and biocompatibility of PLA and PLGA microspheres
    Anderson, JM
    Shive, MS
    [J]. ADVANCED DRUG DELIVERY REVIEWS, 1997, 28 (01) : 5 - 24
  • [5] Thermal degradation of poly[(R)-3-hydroxybutyrate], poly[ε-caprolactone], and poly[(S)-lactide]
    Aoyagi, Y
    Yamashita, K
    Doi, Y
    [J]. POLYMER DEGRADATION AND STABILITY, 2002, 76 (01) : 53 - 59
  • [6] Babanalbandi A, 1999, POLYM INT, V48, P980, DOI 10.1002/(SICI)1097-0126(199910)48:10<980::AID-PI257>3.0.CO
  • [7] 2-B
  • [8] STEREOCOMPLEXATION AND MORPHOLOGY OF POLYLACTIDES
    BROCHU, S
    PRUDHOMME, RE
    BARAKAT, I
    JEROME, R
    [J]. MACROMOLECULES, 1995, 28 (15) : 5230 - 5239
  • [9] Influence of residual monomers and metals on poly (L-lactide) thermal stability
    Cam, D
    Marucci, M
    [J]. POLYMER, 1997, 38 (08) : 1879 - 1884
  • [10] Pyrolysis kinetics of poly(L-lactide) with carboxyl and calcium salt end structures
    Fan, YJ
    Nishida, H
    Hoshihara, S
    Shirai, Y
    Tokiwa, Y
    Endo, T
    [J]. POLYMER DEGRADATION AND STABILITY, 2003, 79 (03) : 547 - 562