Effects of annealing temperatures on the physicochemical properties of nickel-phosphorus deposits

被引:41
作者
Bai, A [1 ]
Hu, CC [1 ]
机构
[1] Natl Chung Cheng Univ, Dept Chem Engn, Chiayi 621, Taiwan
关键词
nickel-phosphorus deposits; P content; annealing; physicochemical properties;
D O I
10.1016/S0254-0584(02)00455-8
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The dependence of physicochemical properties, including microhardness, magnetism, morphology, crystalline information, roughness factor and hydrogen evolution ability, on the phosphorus content, varying from 0 to 28 atomic percentage (at.%), of Ni-P deposits with annealing in air at eight temperatures (i.e., 100, 200, 300, 400, 500, 600, 700 and 800'Q were systematically compared. The microhardness reached a maximum at 400degreesC due to the crystallization of Ni and Ni3P at 400 degreesC and the significant diffusion of Cu into the Ni-P deposit at temperatures greater than or equal to500degreesC, confirmed by the depth profiles of Ni, P, Cu and 0 elements. The paramagnetism of Ni-P deposit was gradually transformed into ferromagnetism at 400 degreesC, attributable to the phase separation of Ni and Ni3P. The roughness factor, R-a, of the deposits with P contents less than or equal to12 at.% were increased with increasing the annealing temperature at temperatures <400 degreesC but R-a of the deposits with 17-28 at.% of P is approximately independent of the annealing temperature. The rate of hydrogen evolution decreased with increasing the annealing temperature because the specific activity (ilR(a)) of the Ni-P deposits was decreased with increasing the annealing temperature. (C) 2002 Elsevier Science B.V. All rights reserved.
引用
收藏
页码:49 / 57
页数:9
相关论文
共 18 条
  • [1] BAKONYI I, 1986, Z METALLKD, V77, P425
  • [2] AN INSITU TEM STUDY OF THE THERMAL-STABILITY OF NANOCRYSTALLINE NI-P
    BOYLAN, K
    OSTRANDER, D
    ERB, U
    PALUMBO, G
    AUST, KT
    [J]. SCRIPTA METALLURGICA ET MATERIALIA, 1991, 25 (12): : 2711 - 2716
  • [3] Relationships among crystallographic structure, mechanical properties and tribological behaviour of electroless Ni-P(9%)/B4C films
    Bozzini, B
    Martini, C
    Cavallotti, PL
    Lanzoni, E
    [J]. WEAR, 1999, 225 : 806 - 813
  • [4] Evidence of clustering in X-ray amorphous Ni-P prepared by autocatalytic chemical deposition
    Bozzini, B
    Cavallotti, PL
    [J]. SCRIPTA MATERIALIA, 1997, 36 (11) : 1245 - 1248
  • [5] BOZZINI B, 1992, P INT 92 SAO PAUL BR, P156
  • [6] The deposition and crystallization behaviors of electroless Ni-Cu-P deposits
    Chen, CJ
    Lin, KL
    [J]. JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1999, 146 (01) : 137 - 140
  • [7] Conway B., 1999, ELECTROCHEMICAL SUPE, P67
  • [8] CULLITY BD, 1972, INTRO MAGNETIC MAT, P92
  • [9] DIETZ G, 1990, J PHYS, V2, P2196
  • [10] Influences of the phosphorus content on physicochemical properties of nickel-phosphorus deposits
    Hu, CC
    Bai, A
    [J]. MATERIALS CHEMISTRY AND PHYSICS, 2003, 77 (01) : 215 - 225