Corrosion of SS310 and Alloy 740 in high temperature supercritical CO2 with impurities H2O and O2

被引:34
|
作者
Li, Kaiyang [1 ]
Zeng, Yimin [2 ]
Luo, Jing-Li [1 ]
机构
[1] Univ Alberta, Dept Chem & Mat Engn, Edmonton, AB T6G 1H9, Canada
[2] Nat Resources Canada, CanmetMATERIALS, Hamilton, ON L8P 0AS, Canada
基金
加拿大自然科学与工程研究理事会;
关键词
Alloy; TEM; XRD; Oxidation; Carburization; High temperature corrosion;
D O I
10.1016/j.corsci.2021.109350
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
This study investigated corrosion performance of SS310 and Alloy 740 in supercritical CO2 with the impurity of 100 ppm H2O or O2 at 600 ?C and 30 MPa for up to 1000 h. The addition of 100 ppm H2O remarkably enhanced general and localized oxidations while the presence of O2 led to the opposite tendency. Alloy 740 exhibited better resistance to carburization compared to SS310, possibly due to the higher solubility of carbides in Ni-based alloys than those in Fe-based alloys. Both alloys exhibit near parabolic oxidation behavior and acceptable corrosion resistance in the supercritical CO2 environments.
引用
收藏
页数:13
相关论文
共 50 条
  • [1] Advancing the mechanistic understanding of corrosion in supercritical CO2 with H2O and O2 impurities
    Li, Kaiyang
    Zeng, Yimin
    CORROSION SCIENCE, 2023, 213
  • [2] Effects of CO and O2 Impurities on Supercritical CO2 Corrosion of Alloy 625
    Mahaffey, Jacob
    Schroeder, Anthony
    Adam, David
    Brittan, Andrew
    Anderson, Mark
    Couet, Adrien
    Sridharan, Kumar
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2018, 49A (08): : 3703 - 3714
  • [3] Effects of CO and O2 Impurities on Supercritical CO2 Corrosion of Alloy 625
    Jacob Mahaffey
    Anthony Schroeder
    David Adam
    Andrew Brittan
    Mark Anderson
    Adrien Couet
    Kumar Sridharan
    Metallurgical and Materials Transactions A, 2018, 49 : 3703 - 3714
  • [4] Corrosion Behavior of Austenitic Stainless Steel in Supercritical CO2 containing O2 and H2O
    Teeter, L.
    Huerta, N.
    Dogan, O.
    Ziomek-Moroz, M.
    Oleksak, R.
    Oryshchyn, D.
    Disenhof, C.
    Baltrus, J.
    Tucker, J.
    CORROSION GENERAL SESSION, 2016, 72 (17): : 137 - 148
  • [5] The Effect of Impurities (H2O, O2, SO2, NO, and NO2) on Supercritical CO2 Structures in Relation to CO2 Pipeline Transport
    Xie, Minjunshi
    Liu, Minkang
    Jin, Zhehui
    Zeng, Yimin
    ENERGY & FUELS, 2024, 38 (24) : 23576 - 23584
  • [6] Revealing the effect of O2, SO2 and H2O in supercritical CO2 on the corrosion behavior of 316 L steel at elevated temperature
    Yu, Chunjiang
    Liu, Yafei
    Chen, Jiayang
    Wang, Zheng
    Guo, Qinghe
    Wu, Yi
    Wen, Zhangquan
    Chen, Dan
    Gong, Kaigang
    Xiao, Gang
    SURFACES AND INTERFACES, 2024, 49
  • [7] CALCULATED TABULATIONS OF H2O LINE BROADENING BY H2O,N2,O2, AND CO2 AT HIGH-TEMPERATURE
    DELAYE, C
    HARTMANN, JM
    TAINE, J
    APPLIED OPTICS, 1989, 28 (23): : 5080 - 5087
  • [8] Technical Note: Characterization of Corrosion Films Formed on Austenitic Stainless Steel in Supercritical CO2 Containing H2O and O2
    Oleksak, Richard P.
    Baltrus, John P.
    Teeter, Lucas
    Ziomek-Moroz, Margaret
    Dogan, Omer N.
    CORROSION, 2018, 74 (10) : 1047 - 1053
  • [9] Corrosion Behavior of High Temperature and O2 Content on Gas Pipelines in CO2/H2S/O2 System
    He G.-X.
    Tang X.
    Leng J.-H.
    Liao K.-X.
    Zhou Q.
    Tian Z.-Y.
    Surface Technology, 2023, 52 (04): : 285 - 294
  • [10] Preheating and combustion characteristics of anthracite under O2/N2, O2/CO2 and O2/CO2/H2O atmospheres
    Zhang, Xiaoyu
    Zhu, Shujun
    Zhu, Jianguo
    Liu, Yuhua
    Zhang, Jiahang
    Hui, Jicheng
    Ding, Hongliang
    Cao, Xiaoyang
    Lyu, Qinggang
    ENERGY, 2023, 274