Mechanical Properties of Glass Bead- and Wollastonite-Filled Isotactic-Polypropylene Composites Modified With Thermoplastic Elastomers

被引:42
作者
Balkan, Onur [1 ]
Demirer, Halil [2 ]
机构
[1] Marmara Univ, Dept Mat, Inst Pure & Appl Sci, TR-34722 Istanbul, Turkey
[2] Marmara Univ, Dept Mat, Tech Educ Fac, TR-34722 Kadikoy, Turkey
关键词
FUNCTIONALIZED BLOCK COPOLYMERS; WOOD FLOUR COMPOSITES; RUBBER PARTICLE-SIZE; G-MA ELASTOMERS; PP SEBS BLENDS; TERNARY COMPOSITES; TENSILE PROPERTIES; PHASE-STRUCTURE; HYBRID COMPOSITES; FRACTURE-TOUGHNESS;
D O I
10.1002/pc.20953
中图分类号
TB33 [复合材料];
学科分类号
摘要
Mechanical properties of the isotactic-polypropylene/glass bead (iPP/GB) and iPP/wollastonite (iPP/W) composites modified with thermoplastic elastomers, the poly(styrene-b-ethylene-co-butylene-b-styrene) copolymer (SEBS) and corresponding block copolymer grafted with maleic anhydride (SEBS-g-MA), were investigated. An increase in toughness of iPP with the elastomers was associated with a decrease in rigidity and strength. Mechanical performance of iPP increased more with acicular W than with spherical GB due to reinforcing effect of W. Comparing the (iPP/GB)/SEBS and (iPP/W)/SEBS composites having the separate microstructure, strength and toughness values of the iPP/GB and iPP/W composites increased more with SEBS-g-MA at the expense of rigidity due to the core-shell microstructure with strong interfacial adhesion. Moreover, the iPP/W composite exhibited superior mechanical performance with 2.5 and 5 vol% of SEBS-g-MA because of a positive synergy between the core-shell microstructure and reinforcing effect of acicular W. The extended models revealed that the elastomer and filler particles in the (iPP/GB)/SEBS and (iPP/W)/ SEBS composites acted individually due to the separate microstructure. However, the rigid GB and W particles encapsulated with the thick elastomer interlayer (R(0)/R(1) = 0.91) in the (iPP/GB)/SEBS-g-MA and (iPP/W)/ SEBS-g-MA composites acted like neither big elastomer particles nor like individual rigid particles, inferring more complicated failure mechanisms in the core-shell composites. POLYM. COMPOS., 31:1285-1308, 2010. (C) 2010 Society of Plastics Engineers
引用
收藏
页码:1285 / 1308
页数:24
相关论文
共 132 条
[61]  
MATONIS VA, 1967, THESIS U CONNECTICUT
[62]   The effect of the volume fraction of dispersed phase on toughness of injection molded polypropylene blended with SEBS, SEPS, and SEP [J].
Matsuda, Y ;
Hara, M ;
Mano, T ;
Okamoto, K ;
Ishikawa, M .
POLYMER ENGINEERING AND SCIENCE, 2005, 45 (12) :1630-1638
[63]   Fracture behaviour of polypropylene/glass bead elastomer composites by using the essential work-of-fracture method [J].
Mouzakis, DE ;
Stricker, F ;
Mülhaupt, R ;
Karger-Kocsis, J .
JOURNAL OF MATERIALS SCIENCE, 1998, 33 (10) :2551-2562
[64]   Fracture resistance of polyblends and polyblend matrix composites .1. Unreinforced and fibre-reinforced nylon 6,6/ABS polyblends [J].
Nair, SV ;
Wong, SC ;
Goettler, LA .
JOURNAL OF MATERIALS SCIENCE, 1997, 32 (20) :5335-5346
[65]   STRENGTH OF PARTICULATE COMPOSITE [J].
NICOLAIS, L ;
NICODEMO, L .
POLYMER ENGINEERING AND SCIENCE, 1973, 13 (06) :469-469
[66]   SIMPLE THEORY OF STRESS-STRAIN PROPERTIES OF FILLED POLYMERS [J].
NIELSEN, LE .
JOURNAL OF APPLIED POLYMER SCIENCE, 1966, 10 (01) :97-&
[67]  
Nielsen LE., 1978, Predicting the properties of mixtures
[68]  
Nitz H, 2000, MACROMOL MATER ENG, V276, P51, DOI 10.1002/(SICI)1439-2054(20000301)276:1<51::AID-MAME51>3.0.CO
[69]  
2-Z
[70]  
Oksman K, 1998, J APPL POLYM SCI, V67, P1503, DOI 10.1002/(SICI)1097-4628(19980228)67:9<1503::AID-APP1>3.0.CO