X-ray CT analysis of the influence of process on defect in Ti-6Al-4V parts produced with Selective Laser Melting technology

被引:28
作者
Zhou, Xin [1 ]
Dai, Ning [1 ]
Chu, Mingqiang [2 ]
Wang, Lei [3 ]
Li, Dawei [1 ]
Zhou, Lei [1 ]
Cheng, Xiaosheng [1 ]
机构
[1] Nanjing Univ Aeronaut & Astronaut, Coll Mech & Elect Engn, Nanjing 210016, Jiangsu, Peoples R China
[2] Ctr Excellence Adv Mat, Dongguan 523808, Peoples R China
[3] Shanghai Aircraft Mfg Co Ltd, Inst Aeronaut Mfg Technol, Shanghai 201324, Peoples R China
基金
中国国家自然科学基金;
关键词
Selective Laser Melting; X-ray computed tomography; Defect; Process parameter; BEHAVIOR; POROSITY; DENSITY;
D O I
10.1007/s00170-019-04347-0
中图分类号
TP [自动化技术、计算机技术];
学科分类号
0812 ;
摘要
Selective Laser Melting (SLM) technology is a potential Additive Manufacturing (AM) process. It has the ability to manufacture metal parts with complex construction. However, there are always defects in SLM products due to the raw materials, manufacturing parameters, and post-treatment. To investigate the relationship between manufacturing process parameters and defects in SLM products, laser power and scan speed are selected as variable parameters to fabricate cube samples. The 3D information of each specimen are collected by X-ray computed tomography, including the size, morphology, and spatial distribution of defects. The mathematical model of laser power and scanning speed with defect volume fraction was established. The result shows that when the scanning speed is less than 1200 mm/s, the defect volume rate increases slowly, but when the scanning speed is faster than 1200 mm/s, the volume rate of defects increases rapidly. As the laser power increases, the volume rate of defect decreased initially and then followed by an increase. It can be concluded that there are many defects in the part manufactured by low laser power and high scanning speed parameter, and the same result by high laser power and high scanning speed parameter. Additionally, the defects are larger and some of them distribute along the scanning path in the latter. Besides, the process window for SLM Ti-6Al-4V is created for exposing the relationship between process parameters and defects, and volume-spherical scatters are used to characterize different process zones.
引用
收藏
页码:3 / 14
页数:12
相关论文
共 50 条
[31]   Evolution of molten pool during selective laser melting of Ti-6Al-4V [J].
Zhang, Tao ;
Li, Hui ;
Liu, Sheng ;
Shen, Shengnan ;
Xie, Huimin ;
Shi, Wenxiong ;
Zhang, Guoqing ;
Shen, Bingnan ;
Chen, Liwei ;
Xiao, Bo ;
Wei, Miaomiao .
JOURNAL OF PHYSICS D-APPLIED PHYSICS, 2019, 52 (05)
[32]   Influence of substructures on the selective laser melted Ti-6Al-4V alloy as a function of laser re-melting [J].
Karimi, J. ;
Xie, M. S. ;
Wang, Z. ;
Prashanth, K. G. .
JOURNAL OF MANUFACTURING PROCESSES, 2021, 68 :1387-1394
[33]   Mechanical Properties of Porous Ti-6Al-4V Titanium Alloys Fabricated by Selective Laser Melting [J].
Qing, Li ;
Zhao Guorui ;
Yan Xingchen ;
Ma Wenyou ;
Yu Hongya ;
Min, Liu .
LASER & OPTOELECTRONICS PROGRESS, 2019, 56 (01)
[34]   Ductility improvement due to martensite α′ decomposition in porous Ti-6Al-4V parts produced by selective laser melting for orthopedic implants [J].
Sallica-Leva, E. ;
Caram, R. ;
Jardini, A. L. ;
Fogagnolo, J. B. .
JOURNAL OF THE MECHANICAL BEHAVIOR OF BIOMEDICAL MATERIALS, 2016, 54 :149-158
[35]   XCT analysis of the influence of melt strategies on defect population in Ti-6Al-4V components manufactured by Selective Electron Beam Melting [J].
Tammas-Williams, S. ;
Zhao, H. ;
Leonard, F. ;
Derguti, F. ;
Todd, I. ;
Prangnell, P. B. .
MATERIALS CHARACTERIZATION, 2015, 102 :47-61
[36]   Fatigue strength of blunt V-notched specimens produced by selective laser melting of Ti-6Al-4V [J].
Razavi, N. ;
Ferro, P. ;
Berto, F. ;
Torgersen, J. .
THEORETICAL AND APPLIED FRACTURE MECHANICS, 2018, 97 :376-384
[37]   Melting and solidification behavior of Ti-6Al-4V powder during selective laser melting [J].
Shunya Yamamoto ;
Hisashi Azuma ;
Shinsuke Suzuki ;
Satoshi Kajino ;
Naoko Sato ;
Toshimitsu Okane ;
Shizuka Nakano ;
Toru Shimizu .
The International Journal of Advanced Manufacturing Technology, 2019, 103 :4433-4442
[38]   Optimisation of single contour strategy in selective laser melting of Ti-6Al-4V lattices [J].
Cao, Xue ;
Carter, Luke Nelson ;
Villapun, Victor Manuel ;
Cantaboni, Francesco ;
De Sio, Giulia ;
Lowther, Morgan ;
Louth, Sophie Elizabeth Thompson ;
Grover, Liam ;
Ginestra, Paola ;
Cox, Sophie Constance .
RAPID PROTOTYPING JOURNAL, 2022, 28 (05) :907-915
[39]   Ti-6Al-4V Additively Manufactured by Selective Laser Melting with Superior Mechanical Properties [J].
Xu, W. ;
Sun, S. ;
Elambasseril, J. ;
Liu, Q. ;
Brandt, M. ;
Qian, M. .
JOM, 2015, 67 (03) :668-673
[40]   Melting and solidification behavior of Ti-6Al-4V powder during selective laser melting [J].
Yamamoto, Shunya ;
Azuma, Hisashi ;
Suzuki, Shinsuke ;
Kajino, Satoshi ;
Sato, Naoko ;
Okane, Toshimitsu ;
Nakano, Shizuka ;
Shimizu, Toru .
INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2019, 103 (9-12) :4433-4442